Replenishing developer and developing method
AssigneeCanon Kabushiki Kaisha
InventorsKenji Okado, Yushi Mikuriya, Kazumi Yoshizaki, Naotaka Ikeda
Life of this patent
Estimating the term…
Abstract
An electrostatic latent image on an image-bearing member is developed with a two-component developer comprising a toner and a carrier stored in a developer vessel while supplying as required a replenishing developer to the developer vessel. The replenishing developer comprises 1 wt. part of a carrier and 2-50 wt. parts of a toner, wherein the carrier is a magnetic fine particle-dispersed resin carrier comprising at least inorganic compound particles and a carrier binder resin, and the toner has a weight-average particle size of 3 to 10 μm and contains 1 to 40 wt. % of solid wax.
Claims43
A replenishing developer, comprising:
- 1 wt. part of a carrier and 2-50 wt. parts of a toner,
- wherein the carrier is a magnetic fine particle-dispersed resin carrier comprising at least inorganic compound particles and a carrier binder resin, the toner has a weight-average particle size of 3 to 10 μm and contains 1 to 40 wt. % of solid wax,
- wherein the carrier binder resin comprises a thermosetting resin,
- wherein the inorganic compound particles comprise magnetite particles containing at least one additive element selected from the group consisting of magnesium, silicon, manganese and phosphorous, and
- wherein the magnetite particles contain said at least one additive element in a total amount of 0.03-5.0 wt. % based on Fe.
A developing method, comprising:
- developing an electrostatic latent image on an image-bearing member with a two-component developer comprising a toner and a carrier stored in a developer vessel, while periodically supplying a replenishing developer to the developer vessel,
- wherein the replenishing developer comprises 1 wt. part of a carrier and 2-50 wt parts of a toner, wherein the carrier is a magnetic fine particle-dispersed resin carrier comprising at least inorganic compound particles and a carrier binder resin, the toner has a weight-average particle size of 3 to 10 μm and contains 1 to 40 wt. % of solid wax,
- wherein the carrier binder resin comprises a thermosetting resin,
- wherein the inorganic compound particles comprise magnetite particles containing at least one additive element selected from the group consisting of magnesium, silicon, manganese and phosphorous, and
- wherein the magnetite particles contain said at least one additive element in a total amount of 0.03-5.0 wt. % based on Fe.
A replenishing developer, comprising:
- 1 wt. part of a carrier and 2-50 wt. parts of a toner,
- wherein the carrier is a magnetic fine particle-dispersed resin carrier comprising at least inorganic compound particles and a carrier binder resin, the toner has a weight-average particle size of 3 to 10 μm and contains 1 to 40 wt. % of solid wax,
- wherein the carrier has a magnetization (δ1000) as measured at a magnetic field of 1000/4π kA/m of 15-65 Am2/kg (emu/g), and a residual magnetization (δr) of 0.1-20 Am2/kg,
- wherein the inorganic compound particles comprise magnetite particles containing at least one additive element selected from the group consisting of magnesium, silicon, manganese and phosphorous, and
- wherein the magnetite particles contain said at least one additive element in a total amount of 0.03-5.0 wt. % based on Fe.
A developing method, comprising:
- developing an electrostatic latent image on an image-bearing member with a two-component developer comprising a toner and a carrier stored in a developer vessel, while periodically supplying a replenishing developer to the developer vessel,
- wherein the replenishing developer comprises 1 wt. part of a carrier and 2-50 wt parts of a toner, wherein the carrier is a magnetic fine particle-dispersed resin carrier comprising at least inorganic compound particles and a carrier binder resin, the toner has a weight-average particle size of 3 to 10 μm and contains 1 to 40 wt. % of solid wax,
- wherein the carrier has a magnetization (δ1000) as measured at a magnetic field of 1000/4π kA/m of 15-65 Am2/kg (emu/g), and a residual magnetization (δr) of 0.1-20 Am2/kg,
- wherein the inorganic compound particles comprise magnetite particles containing at least one additive element selected from the group consisting of magnesium, silicon, manganese and phosphorous, and
- wherein the magnetite particles contain said at least one additive element in a total amount of 0.03-5.0 wt. % based on Fe.
Dependencies are inferred from the claim text.