# US 6,913,790 B2 · Process for reducing the resistivity of an electrically conductive layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,913,790 B2
- Document ID: US6913790B2
- Status: Granted
- Kind: B2
- Application number: 10/228,887
- Filed: 2002-08-27
- Published: 2003-01-16
- Granted: 2005-07-05
- Earliest claimed: 2000-12-27
- Assignees: Plansee SE
- Inventors: Arno Schintlmeister; Peter Wilhartitz
- Web page: https://patentgrep.com/patent/US6913790B2

## CPC

- H10P 14/6314: {of a metallic layer}
- H10P 14/6939: {characterised by the metal}
- H10W 20/065: {by making at least a portion of the conductive part non-conductive, e.g. by oxidation}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

The resistivity of an electrically conductive layer of molybdenum or a molybdenum alloy is reduced. For that purpose, a MoO2 layer is formed on the surface of the electrically conductive layer. The sheet resistivity can thereby be reduced in the order of magnitude of 10% to 15%.

## Claims

### Claim 1

A method of reducing a resistivity of an electrically conductive layer, which comprises:
providing on electrically conductive layer of a material selected from the group consisting at molybdenum and molybdenum alloy; and
oxidizing the conductive layer to thereby form a MoO2 layer on a surface of the electrically conductive layer.

### Claim 2 (depends on 1)

The method according to claim 1, which comprises forming the MoO2 layer with a layer thickness of between 5 nm and 50 nm.

### Claim 3 (depends on 1)

The method according to claim 1, which comprises forming the MoO2 layer with a layer thickness of between 20 nm and 30 nm.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the oxidizing step is a two-step process comprising, in a first step, converting a surface zone of the electrically conductive layer into a MoO3 layer by an oxidation treatment process, and, in a second step, converting the MoO3 layer into a MoO2 layer by a reduction treatment process.

### Claim 5 (depends on 4)

The method according to claim 4, which comprises performing the oxidation treatment process for a period of 5 to 20 minutes at a temperature of between 250° C. and 325° C. with flowing, pure oxygen, an performing the reduction treatment process for a period of 5 to 20 min at a temperature of between 375° C. and 450° C. with flowing hydrogen.

### Claim 6

A method of reducing a resistivity of an electrically conductive layer, which comprises:
providing an electrically conductive layer of a material selected from the group consisting of molybdenum and molybdenum alloy; and
depositing a layer of MoO2 on a surface of the electrically conductive layer with a coating process.

### Claim 7 (depends on 6)

The method according to claim 6, which comprises sputtering the MoO2 layer onto the surface of the electrically conductive layer.

### Claim 8 (depends on 6)

The method according to claim 6, which comprises forming the MoO2 layer with a layer thickness of between 5 nm and 50 nm.

### Claim 9 (depends on 6)

The method according to claim 6, which comprises forming the MoO2 layer with a layer thickness of between 20 nm and 30 nm.