Modified polypropylene and process for producing same
AssigneeTonen Chemical Corporation
InventorsHideaki Wakabayashi, Hiroyuki Ozaki, Kunihiko Imanishi, Takeshi Ishihara, Masatoshi Horii, Satoshi Ueki
Life of this patent
Estimating the term…
Loading patent…
AssigneeTonen Chemical Corporation
InventorsHideaki Wakabayashi, Hiroyuki Ozaki, Kunihiko Imanishi, Takeshi Ishihara, Masatoshi Horii, Satoshi Ueki
Estimating the term…
A modified polypropylene which is a polypropylene having a value of racemic diad fraction [r] in a specific range and modified with a specific compound, e.g., (meth)acrylic acids, and their derivatives or styrene derivatives to have well-balanced properties of affinity for polypropylene-based materials, thermal stability, and high solubility in organic solvents; and a process for producing same. More particularly, the modified polypropylene which is a polypropylene having a value of racemic diad fraction [r] of 0.51 to 0.88, determined by 13C-NMR analysis, and chemically modified with a compound serving as a modifier, e.g., (meth)acrylic acids, and their derivatives or styrene derivatives; and the process for producing the modified polypropylene, wherein the polypropylene having a value of racemic diad fraction [r] in the above range is reacted with at least one type of the compound serving as the modifier in the presence of a radical initiator.
A modified polypropylene which is a polypropylene having a value of racemic diad fraction [r] of 0.51 to 0.88, determined by 13C-NMR analysis, and weight-average molecular weight (Mw) of 5,000 to 400,000, and grafted with units represented by the general formula (1):
A modified polypropylene which is a polypropylene having a value of racemic diad fraction [r] of 0.51 to 0.88, determined by 13C-NMR analysis, and weight-average molecular weight (Mw) of 5,000 to 400,000, and grafted with units represented by the general formula (2):