# US 6,875,467 B2 · Crack resistant sol-gel wafer coatings for integrated optics

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,875,467 B2
- Document ID: US6875467B2
- Status: Granted
- Kind: B2
- Application number: 10/320,313
- Filed: 2002-12-15
- Published: 2004-06-17
- Granted: 2005-04-05
- Earliest claimed: 2002-12-15
- Assignees: Optinetrics, Inc.
- Inventors: Fernando A. Sigoli; Lothar U. Kempen; Edgar A. Mendoza
- Web page: https://patentgrep.com/patent/US6875467B2

## CPC

- C03C 1/008: {for the production of films or coatings}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

A method of preparing a multi-layer, crack resistant sol-gel glass derived coating on a substrate by removing the outer periphery of each layer before curing the layer and depositing any succeeding layer.

## Claims

### Claim 1

A method of preparing a multi-layer, crack resistant sol-gel glass derived coating on a substrate by the steps of
spin coating a first sol-gel layer on said substrate;
removing an outer peripheral portion of said spin-coated layer;
curing said spin coated layer;
depositing at least one additional spin-coated layer;
removing from each said additional spin-coated layer an additional outer peripheral portion beyond the edge of said first removed outer peripheral portion; and
curing each said additional deposited layer.

### Claim 2 (depends on 1)

A method according to claim 1 wherein a layer of sol-gel is formed of a viscous mixture of methyl trimethoxysilane and tetraethyl orthosilicate in the presence of diluted hydrochloric acid.

### Claim 3

A method of making a crack resistant sol-gel film in layers sufficiently thick to be useful for forming optical waveguide structures, comprising the steps of:
a. spin-coating a substrate selected from the group consisting of glass and silicon to deposit a buffer layer of sol-gel;
b. removing the outer periphery of said buffer layer of spin-coated sol-gel from said substrate;
c. curing said buffer layer;
d. spin-coating a core layer of sol-gel on top of said buffer layer;
e. removing more of the outer periphery of core layer than has been removed from said buffer layer;
f. curing said core layer;
g. spin-coating a cladding layer of sol-gel on top of said core layer;
h. removing more of the outer periphery of said cladding layer than has been removed from said buffer and core layers; and
i. curing said cladding layer.

### Claim 4 (depends on 3)

A method according to claim 3 wherein the spin-coated sol-gel substrate is cured by baking.

### Claim 5 (depends on 3)

A method according to claim 3 wherein said outer periphery of said sol-gel is removed by spraying a solvent at said outer periphery.

### Claim 6 (depends on 3)

A method according to claim 3 wherein a layer of sol-gel is formed of a viscous mixture of methyl trimethoxysilane and tetraethyl orthosilicate in the presence of diluted hydrochloric acid.