Low density paper and paperboard articles
AssigneeInternational Paper Company
InventorsKosaraju Krishna Mohan, Alexander A. Koukoulas
Life of this patent
Estimating the term…
Loading patent…
AssigneeInternational Paper Company
InventorsKosaraju Krishna Mohan, Alexander A. Koukoulas
Estimating the term…
The invention provides a low density paperboard material and associated method for use in producing an insulated container, and is especially well-suited for making cups. The paperboard material comprises a paperboard web including wood fibers and expanded microspheres, and has a relatively low density ranging from about 6 to about 10 lb/3MSF/mil, a relatively high caliper ranging from about 24 to about 35 mil, and an internal bond strength of at least about 80×10−3 ft-lbf., preferably at least 100×10−3 lft-lbf. For applications such as cups the material is also coated on one or both sides with a barrier coating, preferably low density polyethylene, to limit liquid penetration into the web. The low density paperboard material of the invention is convertible for manufacture of containers, particularly cups, and exhibits insulative properties comparable to higher cost materials conventionally used to make cups. Also, the surface of the low density board may have a Sheffield smoothness of 300 SU or greater compared with the surface smoothness of 160 to 200 SU for conventional cupstock, the latter having been thought necessary for adequate print quality. However, it has been found that the low density board exhibits good printability on flexo printing machines despite its relatively rough surface, which is surprising and bonus effect realized along with the insulative and other properties of the board.
A method for making an insulated paperboard-based cup having a sidewall and a bottom which comprises providing a paperboard material comprising a paperboard web including from about 0.25 to about 10% by weight dry basis of expanded polymeric microspheres, a caliper of from about 24 to about 35 mils, an apparent density of from about 6.5 to about 10 lb/3MSF/mil, an internal bond of at least about 80×10−3 ft-lbf, and a Sheffield smoothness of at least about 300 SU, and a barrier coating on at least one surface of the web having a thickness of from about 0.5 to about 3.5 mil, forming at least the sidewall of the cup from the web with a surface of the web containing the barrier coating facing interiorly of the cup and the other surface of the web facing exteriorly of the cup, and sealably joining the sidewall to the bottom.
Dependencies are inferred from the claim text.