Thermoset volatile monomer molding compositions and method for molding
AssigneeE. I. Du Pont de Nemours and Company
InventorsRolf Thomas Weberg, Lawrence J. Simmons, Richard Reid Gleason
Life of this patent
Estimating the term…
Abstract
A molding composition including reactive high-volatility monomeric groups, such as acrylics, at least one primary thermal initiator and at least one secondary thermal initiator is described. Molding process using molding compositions including reactive high-volatility monomeric groups are also described.
Claims25
A method for making a molded article comprising the steps:
- (1) providing at least one mold charge unit having a molding composition comprising (a) from about 10 to about 25% by weight of a liquid polymerizable material including at least one volatile monomer reactive material, (b) at least one primary thermal initiator having a primary thermal initiator ten-hour half-life temperature, (c) at least one secondary thermal initiator having a secondary thermal initiator ten-hour half-life temperature of at least about 5° C. greater than the primary thermal initiator ten-hour half-life temperature;
- (2) placing the at least one mold charge unit in a mold cavity of a mold, the mold cavity having a preheated mold temperature sufficient to cause the secondary thermal initiator to pass through from about three to about ten half lives within about ten minutes or less;
- (3) applying pressure to the mold to a molding pressure sufficient to maintain an internal geometric integrity and a surface geometric integrity of the molded article;
- (4) maintaining the preheated mold temperature and the molding pressure for a time sufficient to ensure that the secondary thermal initiator has passed through from about three to about ten half lives.
A method for making a molded article comprising the steps:
- (1) providing at least one mold charge unit comprising (a) a most volatile component, (b) at least one primary thermal initiator having a primary thermal initiator ten-hour half-life temperature;
- and (c) at least one secondary thermal initiator, wherein the ten-hour half-life temperature of the secondary thermal initiator is at most about 5° C. greater than the primary thermal initiator ten-hour half-life temperature;
- (2) placing the at least one mold charge unit in a mold cavity of a mold having an initial mold temperature that is at most about 10° C. less than the boiling point of the most volatile component;
- (3) applying pressure to the mold to a molding pressure sufficient to maintain an internal geometric integrity and a surface geometric integrity of the molded article;
- (4) heating the mold to a final mold temperature sufficient to cause the secondary thermal initiator to cycle through from about three to about ten half lives within about ten minutes or less;
- (5) maintaining the final mold temperature and the molding pressure for a time sufficient to ensure that the secondary thermal initiator has passed through from about three to about ten half lives.
A method for making a molded article comprising the steps:
- (1) providing at least one mold charge unit comprising (a) at least one primary thermal initiator having a primary thermal initiator ten-hour half-life temperature, and (b) at least one secondary thermal initiator having a secondary thermal initiator ten-hour half-life temperature that is at least about 5° C. greater than the primary thermal initiator ten-hour half-life temperature;
- (2) placing the at least one mold charge unit in a mold cavity of a mold, the mold having a flash gap and a preheated mold temperature sufficient to cause the secondary thermal initiator to cycle through from about three to about ten half lives within about ten minutes or less;
- (3) applying an initial molding pressure sufficient to fill the mold with the at least one mold charge unit;
- (4) maintaining time initial molding pressure for a time sufficient to seal the flash gap;
- (5) applying a selected molding pressure sufficient to maintain an internal geometric integrity and a surface geometric integrity of the molded article;
- and
- (6) maintaining the mold temperature and a final molding pressure for a time sufficient to ensure that time secondary thermal initiator has passed through from about three to about ten half lives.
A method for making a molded article comprising the steps:
- (1) providing at least one mold charge unit comprising (a) a most volatile component, (b) at least one primary thermal initiator having a primary thermal initiator ten-hour half-life;
- and (c) at least one secondary thermal initiator having a secondary initiator ten-hour half-life temperature that is at least 5° C. greater than the primary thermal initiator ten-hour half-life temperature;
- (2) placing the at least one mold charge unit in a mold cavity of a mold, the mold having a flash gap and an initial mold temperature that is at most about 10° C. less than the boiling point or the most volatile component;
- (3) applying an initial molding pressure sufficient to fill the mold with the at least one mold charge unit
- (4) maintaining the initial molding pressure for a time sufficient to seal the flash gap;
- (5) heating to a final mold temperature sufficient to cause the secondary thermal initiator to cycle through from about three to about ten half lives within about ten minutes or less;
- (6) applying a selected molding pressure to maintain an internal geometric integrity and surface geometric integrity of the molded article;
- and
- (7) maintaining the final mold temperature and a final molding pressure for a time sufficient to ensure that the secondary thermal initiator has passed through from about three to about ten half lives.
A method for making a molded article having at least one intricate design detail thereon comprising the steps:
- (1) providing at least one mold charge unit having a molding composition comprising (a) at least one primary thermal initiator having a primary thermal initiator ten-hour half-life temperature. (b) at least one secondary thermal initiator having a secondary thermal initiator ten-hour half-life temperature of at least about 5° C. greater than the primary thermal initiator ten-hour half-life temperature;
- (2) placing the at least one mold charge unit in a mold cavity of a mold, the mold cavity having a preheated mold temperature sufficient to cause the secondary thermal initiator to pass through from about three to about ten half lives within about ten minutes or less;
- (3) applying pressure to the mold to a molding pressure sufficient to maintain an internal geometric integrity and a surface geometric integrity of the molded article;
- (4) maintaining the preheated mold temperature and molding pressure for a time sufficient to ensure that the secondary thermal initiator has passed through from about three to about ten half lives.
A method for making a molded article including at least one core encapsulated therein comprising the steps of:
- (1) providing at least two preformed charge units to form a shape corresponding to a portion of the molded article, the preformed charge units having an interior side and a opposite exterior side, wherein the preformed charge units having a molding composition comprising (a) at least one primary thermal initiator having a primary thermal initiator ten-hour half-life temperature, (b) at least one secondary thermal initiator having a secondary thermal initiator ten-hour half-life temperature of at least about 5° C. greater than the primary thermal initiator ten-hour half-life temperature;
- (2) providing a composite charge by placing the at least one core adjacent to the interior side of the preformed charge units;
- (3) placing the composite charge in a mold cavity of a mold, the mold cavity having a preheated mold temperature sufficient to cause the secondary thermal initiator to pass through from about three to about ten half lives within about ten minutes or less;
- (4) applying pressure to the mold to a molding pressure sufficient to maintain an internal geometric integrity and a surface geometric integrity of the molded article;
- (5) maintaining the preheated mold temperature and the molding pressure for a time sufficient to ensure that the secondary thermal initiator has passed through from about three to about ten half lives.
A method for making a molded article including at least one core encapsulated therein comprising the steps of:
- (1) providing at least two preformed charge units forming a shape corresponding to a portion of the molded article, the preformed charge units having an interior side and a opposite exterior side, wherein the preformed charge units having a molding composition comprising (a) a most volatile component, (b) at least one primary temperature initiator having a primary thermal initiator ten-hour half-life temperature;
- and (c) at least one secondary thermal initiator having a secondary thermal initiator ten-hour half-life temperature of at least 5° C. greater than the primary thermal initiator ten-hour half-life temperature:
- (2) providing a composite charge by placing the at least one core adjacent to the interior side of the preformed charge units;
- (3) placing the composite charge in a mold cavity of a mold having an initial mold temperature that is at most about 10° C. less than the boiling point of the most volatile component;
- (4) applying pressure to the mold to a molding pressure sufficient to maintain an internal geometric integrity and a surface geometric integrity of the molded article;
- (5) heating the mold to a final mold temperature sufficient to cause the secondary thermal initiator to cycle through from about three to about ten half lives within about ten minutes or less;
- (6) maintaining the final mold temperature and the molding pressure for a time sufficient to ensure that the secondary thermal initiator has passed through from about three to about ten half lives.
A method for making a molding article including at least one core encapsulated therein comprising the steps of:
- (1) providing the at least one core in a mold cavity of a mold, the mold having a flash gap;
- (2) providing at least one mold charge unit having a molding composition comprising (a) at least one primary thermal initiator having a primary thermal initiator ten-hour half-life temperature;
- and (b) at least one secondary thermal initiator, wherein the ten-hour half-life temperature of the secondary thermal initiator is at least about 5° C. greater than the primary thermal initiator ten-hour half-life temperature;
- (3) heating the mold to a mold temperature sufficient to cause the secondary thermal initiator to cycle through from about three to about ten half lives within about ten minutes or less;
- (4) placing the at least one mold charge unit into the mold cavity, wherein the at least one mold charge unit encompasses the at least one core in the mold cavity;
- (5) applying an initial molding pressure sufficient to fill the mold with the at least one mold charge unit;
- (6) maintaining the initial molding pressure for a time sufficient to seal the flash gap;
- (7) applying a selected molding pressure sufficient to maintain an internal geometric integrity and a surface geometric integrity of the molded article;
- and
- (8) maintaining the mold temperature and a final molding pressure for a time sufficient to ensure that the secondary thermal initiator has passed through from about three to about ten half lives.
A method for making a molded article including at least one core encapsulated therein comprising the steps of:
- (1) providing the at least one core in a mold cavity of a mold, the mold having a flash gap and an initial mold temperature that is at most about 10° C. less than the boiling point of the most volatile component;
- (2) providing at least one mold charge unit into the mold cavity, wherein the at least one mold charge unit encompasses the at least one core in the mold cavity, the at least one mold charge unit having a molding composition comprising (a) a most volatile component, (b) at least one primary thermal initiator having a primary thermal initiator ten-hour half-life temperature;
- and (c) at least one secondary thermal initiator having a secondary thermal initiator ten-hour half-life temperature of at least 50° C. greater than the primary thermal initiator ten-hour half-life temperature;
- (3) applying an initial molding pressure sufficient to fill the mold with the at least one mold charge unit;
- (4) maintaining the initial molding pressure for a time sufficient to seal the flash gap;
- (5) heating to a final mold temperature sufficient to cause the secondary thermal initiator to cycle through from about three to about ten half lives within about ten minutes or less;
- (6) applying a selected molding pressure to maintain an internal geometric integrity and surface geometric integrity of the molded article;
- and
- (7) maintaining the final mold temperature and a final molding pressure for a time sufficient to ensure that the secondary thermal initiator has cycled through from about three to about ten half lives.
Dependencies are inferred from the claim text.