Process for removing aluminum species from alkali metal halide brine solutions
AssigneeKvaerner Canada, Inc.
InventorsFelix Mok, R. Ganapathy Subramanian
Life of this patent
Estimating the term…
Abstract
A method for the reduction of soluble aluminum species in an evaporated salt alkali metal halide brine containing up to 500 ppb aluminum species to provide a brine feedstock suitable for use in a chlor-alkali membrane cell process, said method comprising treating said brine with a magnesium salt in an amount to provide a Mg to Al molar ratio selected from 5-20 to 1 at a Mg concentration selected from 0.5-10 ppm, and sufficient alkali metal hydroxide to provide an excess alkalinity concentration of between 0.1-0.5 g/L alkali metal hydroxide to effect precipitation of a magnesium aluminum hydroxide complex; and removing said complex to provide said brine feedstock.
Claims9
A method for the reduction of soluble aluminum species in an evaporated salt alkali metal halide brine containing up to 500 ppb aluminum species to provide a brine feedstock suitable for use in a chlor-alkali membrane cell process, said method comprising:
- (a) treating said brine with a magnesium salt in an amount to provide a Mg to Al molar ratio selected from 5-20 to 1 and at a Mg concentration of from 0.5 to 5 ppm, and sufficient alkali metal hydroxide to provide an excess alkalinity concentration of between 0.1-0.3 g/L alkali metal hydroxide to effect precipitation of a magnesium aluminum hydroxide complex;
- and
- (b) removing said complex to provide said brine feedstock.