# US 6,731,386 B2 · Measurement technique for ultra-thin oxides

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,731,386 B2
- Document ID: US6731386B2
- Status: Granted
- Kind: B2
- Application number: 09/754,611
- Filed: 2001-01-04
- Published: 2002-07-04
- Granted: 2004-05-04
- Earliest claimed: 2001-01-04
- Assignees: Agere Systems Inc.
- Inventors: Mindaugas Fernand Dautartas; George John Przybylek
- Web page: https://patentgrep.com/patent/US6731386B2

## CPC

- G01B 11/065: {using one or more discrete wavelengths}
- G01B: MEASURING LENGTH, THICKNESS OR SIMILAR LINEAR DIMENSIONS; MEASURING ANGLES; MEASURING AREAS; MEASURING IRREGULARITIES OF SURFACES OR CONTOURS

## Abstract

A method of measuring the thickness of ultra-thin (e.g., <200 Å) oxide formed on a semiconductor device uses a reference sample (i.e., another silicon wafer) which has been pre-processed to include a relatively thick oxide surface layer. The thickness of the reference oxide (t) is measured using any conventional technique (such as an ellipsometer). An ultra-thin oxide is then simultaneously formed on both the reference sample and semiconductor device. The total oxide thickness (T) of the dual-layer structure on the reference sample is then measured (again, using any conventional technique), and the difference between the two measured values (T−t=δ) is defined as the thickness of the ultra-thin oxide layer.

## Claims

### Claim 1

A method of measuring the thickness (δ) of an ultra-thin oxide grown on a surface of a semiconductor device, the method comprising the steps of:
a) providing a reference sample device including a top major surface;
b) forming a relatively thick reference oxide on the top major surface of said reference sample device;
c) measuring the thickness (t) of said relatively thick reference oxide;
d) providing a semiconductor device;
e) simultaneously forming, on both said semiconductor device and said reference sample, an ultra-thin oxide layer, using identical formation conditions;
f) measuring the total thickness (T) of both said relatively thick reference oxide and the ultra-thin oxide layers on said reference sample; and
g) subtracting the initial thickness (t) of said relatively thick reference oxide from said total thickness (T) to determine the thickness (δ) of the ultra-thin oxide layer formed on the semiconductor device.

### Claim 2 (depends on 1)

The method as defined in claim 1 wherein in performing steps c) and f) an ellipsometer is used to measure the oxide layer thicknesses on the reference sample.

### Claim 3 (depends on 2)

The method as defined in claim 2 wherein a HeNe ellipsometer source is used to measure the oxide layer thicknesses.

### Claim 4 (depends on 1)

The method as defined in claim 1 wherein in performing step a) a silicon wafer is provided as the reference sample.

### Claim 5 (depends on 1)

The method as defined in claim 1 wherein in performing step b) an oxide having a thickness in the range of 1000-1400 Å is formed.

### Claim 6 (depends on 1)

The method as defined in claim 1 wherein in performing step e), an ultra-thin oxide having a thickness of at most 200 Å is formed.