# US 6,731,352 B2 · Method for fabricating liquid crystal display

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,731,352 B2
- Document ID: US6731352B2
- Status: Granted
- Kind: B2
- Application number: 10/161,301
- Filed: 2002-06-03
- Published: 2003-09-11
- Granted: 2004-05-04
- Earliest claimed: 2002-03-07
- Assignees: Toppoly Optoelectronics Corp.
- Inventors: Chu-Jung Shih; Gwo-Long Lin; I-Min Lu; I-Wei Wu
- Web page: https://patentgrep.com/patent/US6731352B2

## CPC

- G02F 1/136227: {Through-hole connection of the pixel electrode to the active element through an insulation layer}
- G02F 2202/104: poly-Si
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS

## Abstract

A six mask-steps method for fabricating liquid crystal display is described. A driving area and a pixel area are defined by a first mask step. Gates on the driving/pixel area and upper electrodes of capacitors on the pixel area are defined by a second mask step. Then, using the gates and the upper electrodes as a mask, a source/drain, channel region and lower electrode are formed in the driving/pixel area by an ion-doping process. A second insulation layer is formed and covers the insulation substrate. A plurality of first openings is formed by the third mask step and the gate and the source/drain are exposed. A second conductive layer is formed and covers the second insulation layer and the first opening is filled. Then, the second conductive layer is patterned, and a source/drain line is formed and contacts electrically with the source/drain by the fourth mask step. A dielectric layer is formed and covers the second insulation layer and the second conductive layer; the dielectric layer has a planar surface. A second opening is formed by the fifth mask step and the drain line on the pixel area is exposed. Finally, a pixel electrode is defined by the sixth mask step and contacts electrically with the drain line.

## Claims

### Claim 1

A method for fabricating liquid crystal display, comprising:
providing an insulation substrate;
forming a buffer layer on the insulation substrate;
forming an amorphous silicon layer on the buffer layer;
transforming the amorphous silicon layer into a polysilicon layer by laser low temperature annealing;
forming a first active area and a second active area by defining the polysilicon layer, wherein the first active area is a driving area and the second active area is a pixel area;
forming a first insulation layer covering the polysilicon layer;
forming a patterned conductive layer on the driving area and the pixel layer, wherein the patterned conductive layer serves as gates and upper electrodes of capacitors;
using the patterned conductive layer as a mask, forming a source/drain, channel region and lower electrode in the polysilicon layer by an ion-doping process;
forming a second insulation layer covering the insulation substrate;
forming a plurality of first openings and exposing the gate and the source/drain;
forming a second conductive layer to cover the second insulation layer and fill the first opening;
patterning the second conductive layer to form a source/drain line contacting electrically with the source/drain;
forming a dielectric layer covering the second insulation layer and the second conductive layer, wherein the dielectric layer has a planar surface;
forming a second opening, wherein the drain line on the pixel area is exposed; and
forming a pixel electrode connecting electrically with the drain line.

### Claim 2 (depends on 1)

The method of claim 1, wherein the ion-doping process is a P-type ion implantation.

### Claim 3 (depends on 2)

The method of claim 2, wherein an ion concentration formed by the P-type ion implantation is about between about 10E19 and 10E21 ions/cm3.

### Claim 4 (depends on 1)

The method of claim 1, wherein the buffer layer sequentially comprises a nitride layer and an oxide layer.

### Claim 5 (depends on 1)

The method of claim 1, wherein the pixel electrode is made from ITO glass.

### Claim 6 (depends on 1)

The method of claim 1, wherein a bottom electrode is defined by the ion-doping process.

### Claim 7

A method for fabricating liquid crystal display, the method being adapted for fabrication on an insulation substrate, the method comprising:
forming a polysilicon layer on the insulation substrate;
forming a first active area and a second active area by defining the polysilicon layer;
forming a first insulation layer covering the polysilicon layer;
forming a patterned conductive layer on the first insulation layer, wherein the patterned conductive layer serves as gates and upper electrodes of capacitors;
using the patterned conductive layer as a mask, forming a source/drain and channel region in the polysilicon layer by a P-type ion-doping process;
forming a second insulation layer covering the insulation substrate;
forming a plurality of first openings and exposing the gate and the source/drain;
forming a source line and a drain line, wherein the source line contacts electrically with the source and the drain line contacts electrically with the drain;
forming a dielectric layer covering the second insulation layer and the source/drain lines, wherein the dielectric layer has a planar surface;
forming a second opening, wherein a drain line on the second active area is exposed; and
forming a pixel electrode contacting electrically with the drain line on the second active area.

### Claim 8 (depends on 7)

The method of claim 7, wherein the first active area is a driving area and the second active area is a pixel area.

### Claim 9 (depends on 7)

The method of claim 7, further comprising a buffer layer formed before the polysilicon layer formed.

### Claim 10 (depends on 7)

The method of claim 7, wherein a method for forming the polysilicon layer comprises:
forming an amorphous poly layer on the buffer layer; and
transforming the amorphous poly layer into the polysilicon layer by laser low temperature annealing.

### Claim 11 (depends on 7)

The method of claim 7, wherein an ion concentration formed by the P-type ion implantation is about between about 10E19 and 10E21 ions/cm3.

### Claim 12 (depends on 7)

The method of claim 7, wherein a bottom electrode is defined by the ion-doping process.

### Claim 13 (depends on 7)

The method of claim 7, wherein the buffer layer sequentially comprises a nitride layer and an oxide layer.

### Claim 14 (depends on 7)

The method of claim 7, wherein the pixel electrode is made from ITO glass.