# US 6,731,130 B1 · Method of determining gate oxide thickness of an operational MOSFET

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,731,130 B1
- Document ID: US6731130B1
- Status: Granted
- Kind: B1
- Application number: 10/017,832
- Filed: 2001-12-12
- Granted: 2004-05-04
- Earliest claimed: 2001-12-12
- Assignees: Advanced Micro Devices, Inc.
- Inventors: Nian Yang; Zhigang Wang; Tien-Chun Yang
- Web page: https://patentgrep.com/patent/US6731130B1

## CPC

- H10P 74/23: {characterised by multiple measurements, corrections, marking or sorting processes}
- H10P 74/203: {Structural properties, e.g. testing or measuring thicknesses, line widths, warpage, bond strengths or physical defects}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A non-destructive and non-intrusive, user friendly, easy to setup and efficient system and method of determining the gate oxide thickness of an operational MOSFET used in real circuit applications is provided. Additionally, the present invention determines the gate oxide thickness when the operational MOSFET is operating in the inversion mode.

## Claims

### Claim 1

A method of determining a gate oxide thickness of an operational MOSFET (metal oxide semiconductor field effect transistor) fabricated with a gate oxide formation process, comprising:
a) providing said operational MOSFET fabricated with said gate oxide formation process;
b) coupling a drain node and a source node of said operational MOSFET to a ground;
c) applying a range of voltages at a gate node of said operational MOSFET and measuring at said gate node a gate direct tunneling current for each applied voltage to generate a plurality of measured data;
d) providing a gate direct tunneling current model; and
e) determining said gate oxide thickness by fitting said gate direct tunneling current model to said measured data and using a gate oxide thickness variable as a fitting parameter.

### Claim 2 (depends on 1)

A method as recited in claim 1 wherein said gate oxide thickness is no less than approximately 3 nanometers.

### Claim 3 (depends on 1)

A method as recited in claim 1 wherein said gate oxide thickness is no greater than approximately 3 nanometers.

### Claim 4 (depends on 1)

A method as recited in claim 1 wherein a channel length of said operational MOSFET is no less than approximately 0.5 micrometers.

### Claim 5 (depends on 1)

A method as recited in claim 1 wherein a channel length of said operational MOSFET is no greater than approximately 0.5 micrometers.

### Claim 6 (depends on 1)

A method as recited in claim 1 wherein a channel width of said operational MOSFET is no less than approximately 5 micrometers.

### Claim 7 (depends on 1)

A method as recited in claim 1 wherein a channel width of said operational MOSFET is no greater than approximately 5 micrometers.

### Claim 8 (depends on 1)

A method as recited in claim 1 wherein in said step c) said operational MOSFET is operated in an inversion mode by application of a particular range of voltages at said gate node.

### Claim 9 (depends on 1)

A method as recited in claim 1 wherein said gate direct tunneling current model includes a value representing reflectivity of an electron from an inversion layer due to a gate oxide energy barrier.