# US 6,731,006 B1 · Doped copper interconnects using laser thermal annealing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,731,006 B1
- Document ID: US6731006B1
- Status: Granted
- Kind: B1
- Application number: 10/323,941
- Filed: 2002-12-20
- Granted: 2004-05-04
- Earliest claimed: 2002-12-20
- Assignees: Advanced Micro Devices, Inc.
- Inventors: Arvind Halliyal; Minh Van Ngo
- Web page: https://patentgrep.com/patent/US6731006B1

## CPC

- H10W 20/081: {by forming openings in the dielectric parts}
- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- H10W 20/064: {by modifying the conductivity of conductive parts, e.g. by alloying}
- H10W 20/082: {the openings being tapered via holes}
- H10W 20/084: {for dual-damascene structures}
- H10W 20/42: Vias, e.g. via plugs
- H10W 20/4424: {Copper alloys}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A semiconductor device and method of making the same includes a first metallization level, a first etch stop layer, a dielectric layer and an opening extending through the dielectric layer and the first etch stop layer. The first etch stop layer is disposed over the first metallization level. Metal within the opening forms a second metal feature, and the metal can comprise copper or a copper alloy. Dopants are introduced into the metal and are activated by laser thermal annealing. A concentration of the dopants within the metal in a lower portion of the second metal feature proximate the first metal feature is greater than a concentration of dopants in a central portion of the second metal feature, and a concentration of the dopants within the metal in an upper portion of the second metal feature is greater than a concentration of dopants in the central portion of the second metal feature.

## Claims

### Claim 1

A semiconductor device, comprising:
a first metallization level, said first metallization level including a first metal feature;
a dielectric layer disposed over said metallization level;
an opening extending through said dielectric layer to said first metal feature; and
metal within said opening forming a second metal feature,
wherein said metal includes dopants, and a concentration of said dopants within said metal in a lower portion of said second metal feature proximate said first metal feature is greater than a concentration of dopants in a central portion of said second metal feature.

### Claim 2 (depends on 1)

The semiconductor device according to claim 1, wherein said opening is a via opening, a trench, or a dual damascene opening comprising a lower via opening in communication with an upper trench; and wherein said second metal feature comprises a via, a line, or a combination of a lower via in contact with an upper line, respectively.

### Claim 3 (depends on 1)

The semiconductor device according to claim 1, wherein said metal and said first metallization level comprise copper (Cu) or a Cu alloy.

### Claim 4 (depends on 1)

The semiconductor device according to claim 1, wherein said dopants are activated by laser thermal annealing.

### Claim 5 (depends on 1)

The semiconductor device according to claim 1, wherein a concentration of said dopants within said metal in an upper portion of said second metal feature is greater than a concentration of dopants in the central portion of said second metal feature.

### Claim 6 (depends on 5)

The semiconductor device according to claim 5, wherein said upper portion has a depth equal to about 5% to about 15% of a depth of said second feature.

### Claim 7 (depends on 1)

The semiconductor device according to claim 1, wherein said central portion has a depth equal to about 70% to about 90% of a depth of said second feature.

### Claim 8 (depends on 1)

The semiconductor device according to claim 1, wherein said lower portion has a depth equal to about 5% to about 15% of a depth of said second feature.

### Claim 9 (depends on 1)

The semiconductor device according to claim 1, wherein the dopants are electromigration reducing dopants.

### Claim 10 (depends on 9)

The semiconductor device according to claim 9, wherein the dopants are selected from the group consisting of palladium, nickel, tantalum, aluminum, chromium, titanium, magnesium, boron, tin, zirconium, carbon, and combinations thereof.

### Claim 11

A method of manufacturing a semiconductor device, comprising the steps of:
forming a first metallization level including a first metal feature;
forming a dielectric layer over the first metallization layer;
forming an opening through the dielectric layer to the first metal feature;
filling the opening with a metal to form a second metal feature;
introducing dopants into the metal of the second metal feature; and
laser thermal annealing the metal of the second metal feature.

### Claim 12 (depends on 11)

The method of manufacturing a semiconductor device according to claim 11, wherein the opening is a via opening, a trench, or a dual damascene opening comprising a lower via opening in communication with an upper trench; and wherein the second metal feature comprises a via, a line, or a combination of a lower via in contact with an upper line, respectively.

### Claim 13 (depends on 11)

The method of manufacturing a semiconductor device according to claim 11, wherein a concentration of said dopants within said metal in a lower portion of said second metal feature proximate said first metal feature is greater than a concentration of dopants in a central portion of said second metal feature.

### Claim 14 (depends on 12)

The method of manufacturing a semiconductor device according to claim 12, wherein the lower portion is laser thermal annealed before filling the opening to form the central portion.

### Claim 15 (depends on 11)

The method of manufacturing semiconductor device according to claim 11, wherein a concentration of said dopants within said metal in an upper portion of said second metal feature is greater than a concentration of dopants in the central portion of said second metal feature.

### Claim 16 (depends on 15)

The method of manufacturing a semiconductor device according to claim 15, wherein a concentration of said dopants within said metal in a lower portion of said second metal feature proximate said first metal feature is greater than a concentration of dopants in the central portion of said second metal feature.

### Claim 17 (depends on 14)

The method of manufacturing a semiconductor device according to claim 14, wherein the lower portion is laser thermal annealed before filling the opening to form the central portion.

### Claim 18 (depends on 11)

The method of manufacturing a semiconductor device according to claim 11, wherein the dopants are electromigration reducing dopants.

### Claim 19 (depends on 18)

The method of manufacturing a semiconductor device according to claim 18, wherein the dopants are selected from the group consisting of palladium, nickel, tantalum, aluminum, chromium, titanium, magnesium, boron, tin, zirconium, carbon, and combinations thereof.

### Claim 20

A method of manufacturing a semiconductor device, comprising the steps of:
forming a metal feature;
introducing dopants into the metal feature; and
laser thermal annealing the metal feature, wherein at least one portion of the metal feature is not doped during the step of introducing dopants.