# US 6,730,943 B2 · Thin semiconductor GaInN layer, method for preparing same, light-emitting diode comprising said layer and illumination device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,943 B2
- Document ID: US6730943B2
- Status: Granted
- Kind: B2
- Application number: 10/257,515
- Filed: 2002-10-11
- Published: 2003-05-15
- Granted: 2004-05-04
- Earliest claimed: 2000-04-12
- Assignees: Centre National De La Recherche Scientifique
- Inventors: Jean Claude Massies; Nicolas Pierre Grandjean; Benjamin Gérard Pierre Damilano
- Web page: https://patentgrep.com/patent/US6730943B2

## CPC

- H10H 20/813: having a plurality of light-emitting regions, e.g. multi-junction LEDs or light-emitting devices having photoluminescent regions within the bodies
- B82Y 20/00: Nanooptics, e.g. quantum optics or photonic crystals
- H10H 20/0137: {the light-emitting regions comprising nitride materials}
- H10H 20/812: within the light-emitting regions, e.g. having quantum confinement structures
- H10H 20/825: containing nitrogen, e.g. GaN
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES

## Abstract

Thin, single semi conducting layer of GaInN, possibly containing a small percentage of arsenic, phosphorus or antimony, the said layer emitting at least two visible lights with determined colors which can be combined, particularly to obtain white light. Method for preparing this layer. Light emitting diode (LED), particularly a LED emitting white light comprising such a thin layer in its active zone, and lighting device comprising such a diode.

## Claims

### Claim 1

A thin layer comprising:
a single, thin, semi conducting layer of GaInN; and
a small percentage of arsenic, phosphorus or antimony,
wherein the layer emits at least two visible lights with determined colors.

### Claim 2 (depends on 1)

The thin layer according to claim 1, further comprising at least two deposits of GaInN adjacent to each other or superposing them, each deposit emitting a visible light with a determined colour.

### Claim 3 (depends on 2)

The thin layer according to claim 2, in which there are three of said deposits and they emit blue, green and red light respectively.

### Claim 4 (depends on 2)

The thin layer according to claim 2, in which there are two of said deposits and they emit blue and yellow light respectively.

### Claim 5 (depends on 1)

The thin layer according to claim 1, in which the combination of said visible lights with at least two determined colors produces white light.

### Claim 6 (depends on 1)

The thin layer according to claim 1, wherein the thickness of which is less than or equal to 100 Å.

### Claim 7 (depends on 1)

A light emitting diode (LED) comprising at least one thin layer in its active zone, according to claim 1.

### Claim 8 (depends on 7)

The light emitting diode according to claim 7, emitting white light.

### Claim 9 (depends on 7)

A lighting device comprising at least one light emitting diode according to claim 7.

### Claim 10 (depends on 8)

A lighting device emitting white light, comprising at least one light emitting diode according to claim 8.

### Claim 11

A method for preparing of a single, thin, semi conducting layer of GaInN comprising:
successively growing deposits of GaInN with the same composition, an interruption in the growth being allowed between each deposit, each of said deposits emitting a visible light with a determined colour, wherein the layer of GaInN comprises these deposits and a small percentage of arsenic, phosphorus or antimony, said layer emitting visible lights with at least two determined colors.

### Claim 12 (depends on 11)

The method according to claim 11, in which the combination of said visible lights with at least two determined colors produces white light.

### Claim 13 (depends on 11)

The method according to claim 11 further comprising, varying the temperature and/or the growth duration of the deposit and/or the other parameters governing growth of the deposit, if any, and/or the temperature during the interruption of growth, and/or the duration of said interruption to fix the colour of the light emitted by each deposit.

### Claim 14 (depends on 13)

The method according to claim 13 further comprising, varying the duration and/or temperature of growth of each deposit to fix the colour of light emitted by each deposit.

### Claim 15 (depends on 11)

The method according to claim 11 further comprising, further increasing the temperature while interrupting the growth.

### Claim 16 (depends on 11)

The method according to claim 11, in which the deposits are made by Molecular Jet Epitaxy (EJM).

### Claim 17 (depends on 11)

The method according to claim 11, in which the deposits are made by Organo-Metallic Vapour Phase Epitaxy (EPVOM).