# US 6,730,876 B2 · Highly ductile reduced imperfection weld for ductile iron and method for producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,876 B2
- Document ID: US6730876B2
- Status: Granted
- Kind: B2
- Application number: 09/866,258
- Filed: 2001-05-29
- Published: 2002-12-05
- Granted: 2004-05-04
- Earliest claimed: 2001-05-29
- Assignees: U.S. Pipe and Foundry Company
- Inventors: Daniel A. Copeland; David J. Farr; James E. Wren
- Web page: https://patentgrep.com/patent/US6730876B2

## CPC

- B23K 9/23: taking account of the properties of the materials to be welded
- B23K 35/3033: {Ni as the principal constituent}
- B23K 35/383: {mainly containing noble gases or nitrogen}
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

The art has experienced difficulty obtaining “sound” welds with high-nickel welds above the second pass. Particular problems are tension anomalies and sub-optimal interweld pass fusion at higher order passes of the weld wire, along with undesirably high heat levels transferred to the workpiece. The inventors have discovered that ductile iron-to-ductile iron welds can be reliably formed at mission-critical junctures by compensating for the brittle nature of the heat affected zone through enhancing ductility of the weld itself. The present invention provides in continuing part for a highly durable weld without soundness problems such as tension anomalies, multilayer fusion imperfections, or pinholes; and a method of forming such a weld. The weld is created using high nickel weld wire (filler metal or consumable electrode, or both) welded in a pure inert gas (or mixture of pure inert gasses and even reducing gasses). Additions of weld metal alloys, flux coring, and deoxidizing coatings are not required. The work pieces do not require pre- or post-heat treatment to minimize the effects of the HAZ. Additional inventive features are described more fully below.

## Claims

### Claim 1

A weld joint comprising a first workpiece, a second workpiece, and a weld body joining said first workpiece and said second workpiece, which weld body comprises lag-free weld puddle of substantially pure nickel that yields a weld joint substantially free of porosity.

### Claim 2 (depends on 1)

A weld joint as in claim 1, wherein said area attributable to a higher order pass comprises greater than or equal to approximately 83.5% nickel.

### Claim 3 (depends on 1)

A weld joint as in claim 1, wherein said area attributable to a higher order pass comprises greater than or equal to approximately 90% nickel.

### Claim 4

A weld joint comprising a first workpiece, a second workpiece, and a weld body joining said first workpiece and said second workpiece, said weld body comprising an area attributable to a higher order pass that comprises substantially pure nickel, the surface of which is substantially free of slag and slag residuals, and which surface exhibits an average of four or fewer pits visible to a naked eye per square inch.

### Claim 5 (depends on 4)

A weld joint as in claim 4, wherein said area attributable to a higher order pass comprises greater than or equal to approximately 83.5% nickel.

### Claim 6 (depends on 4)

A weld joint as in claim 4, wherein said area attributable to a higher order pass comprises greater than or equal to approximately 90% nickel.

### Claim 7 (depends on 4)

A weld joint as in claim 4, wherein said weld body has an average of three or fewer pits visible to a naked eye per square inch.

### Claim 8 (depends on 7)

A weld joint as in claim 7, wherein said area attributable to a higher order pass comprises greater than or equal to approximately 83.5% nickel.

### Claim 9 (depends on 7)

A weld joint as in claim 7, wherein said area attributable to a higher order pass comprises greater than or equal to approximately 90% nickel.

### Claim 10 (depends on 4)

A weld joint as in claim 4, wherein said weld body has an average of two or fewer pits visible to a naked eye per square inch.

### Claim 11 (depends on 10)

A weld joint as in claim 10, wherein said area attributable to a higher order pass comprises greater than or equal to approximately 83.5% nickel.

### Claim 12 (depends on 10)

A weld joint as in claim 10, wherein said area attributable to a higher order pass comprises greater than or equal to approximately 90% nickel.

### Claim 13 (depends on 4)

A weld joint as in claim 4, wherein said weld body has an average of one or fewer pits visible to a naked eye per square inch.

### Claim 14 (depends on 13)

A weld joint as in claim 13, wherein said area attributable to a higher order pass comprises greater than or equal to approximately 83.5% nickel.

### Claim 15 (depends on 13)

A weld joint as in claim 13, wherein said area attributable to a higher order pass comprises greater than or equal to approximately 90% nickel.

### Claim 16

A weld comprising a higher order pass, and having a gradient of nickel purity as measured along a throat of said weld that generally increases between a root of said weld and a point within said higher order pass, said higher order pass being weldable with another weld pass without removal of slag.

### Claim 17

A weld comprising a second order pass and a plurality of higher order passes, said plurality of higher order passes comprising at least a third order pass and a fourth order pass, the weld having a gradient of nickel purity that generally increases from a second order pass through said third order pass and said fourth order pass, and being substantially free of porosity and of slag.

### Claim 18

A weld comprising a higher order pass, and having a gradient of nickel purity as measured along a throat of said weld that generally increases as the distance from a root of said weld increases, a face of said weld having an average of four or fewer pits visible to a naked eye per square inch, said face being substantially free of slag.

### Claim 19 (depends on 18)

A weld as in claim 18, wherein the face of said weld has an average of three or fewer pits visible to a naked eye per square inch.

### Claim 20 (depends on 18)

A weld as in claim 18, wherein the face of said weld has an average of two or fewer pits visible to a naked eye per square inch.

### Claim 21 (depends on 18)

A weld as in claim 18, wherein the face of said weld has an average of one or fewer pits visible to a naked eye per square inch.

### Claim 22

A slag-free weld comprising a plurality of passes, which passes comprise a second order pass and at least one higher order pass; wherein
a. a plurality of said passes generally increase in nickel purity as the order number increases; and wherein further
b. the last of which passes to increase in nickel purity has an average of four or fewer pits visible to a naked eye per square inch; and wherein further
c. no pass comprises any flux inclusions.

### Claim 23 (depends on 22)

A weld as in claim 22, wherein the last of which second and higher order pass zones to increase in nickel purity has an average of three or fewer pits visible to a naked eye per square inch.

### Claim 24 (depends on 22)

A weld as in claim 22, wherein the last of which second and higher order pass zones to increase in nickel purity has an average of two or fewer pits visible to a naked eye per square inch.

### Claim 25 (depends on 22)

A weld as in claim 22, wherein the last of which second and higher order pass zones to increase in nickel purity has an average of one or fewer pits visible to a naked eye per square inch.

### Claim 26

A method of producing a highly ductile weld, comprising the steps of:
a. selecting a weld wire comprising substantially pure nickel
b. in the absence of flux, fusing a weld bead of said weld wire onto a workpiece, whereby a first weld pass of weld bead is welded
c. fusing to said first weld pass at least one weld pass of said weld wire, whereby an intermediary pass of weld bead is welded
d. in the presence of a substantially pure inert gas, fusing to said intermediary pass at least one weld pass of said weld wire in a substantially undiluted condition.

### Claim 27 (depends on 26)

A method of producing a highly ductile weld as in claim 26, wherein said substantially pure inert gas comprises an inert gas in combination with reducing gasses.

### Claim 28 (depends on 26)

A method of producing a highly ductile weld as in claim 26, wherein said substantially pure inert gas comprises argon gas.

### Claim 29 (depends on 26)

A method of producing a highly ductile weld as in claim 26, wherein said substantially pure inert gas comprises argon gas in combination with reducing gasses.

### Claim 30 (depends on 26)

The method of creating a welded ductile iron joint according to claim 26, further comprising the step of abstaining from pre-heating, post-heating, or chemical antimartensitizing treatment of a heat affected zone.

### Claim 31 (depends on 26)

The method of creating a welded ductile iron joint according to claim 26, wherein at least one of steps b, c, and d is accomplished by a skip welding technique.

### Claim 32 (depends on 26)

The method of creating a welded ductile iron joint according to claim 26, wherein at least one of steps b, c, and d is accomplished using a liquid cooled welding torch.

### Claim 33 (depends on 26)

The method of creating a welded ductile iron joint according to claim 26, wherein at least one of steps b, c, and d is accomplished using a pulse MIG welder.

### Claim 34 (depends on 26)

The method of creating a welded ductile iron joint according to claim 26, wherein said fusing in at least one of steps b, c, and d occurs by means of spray transfer welding.

### Claim 35

A method of producing a highly ductile weld, comprising the steps of:
a. selecting a weld wire comprising substantially pure nickel;
b. fusing by spray transfer a weld bead of said weld wire onto a workpiece using a liquid cooled welding torch operated in a skip welding technique, whereby a first weld pass of weld bead is welded;
c. fusing by spray transfer to said first weld pass at least one weld pass of said weld wire using a liquid cooled welding torch operated in a skip welding technique, whereby an intermediary pass of weld bead is welded;
d. in the presence of a substantially pure inert gas, using a liquid cooled welding torch operated in a skip welding technique to fuse, in the absence of flux, by spray transfer to said intermediary pass at least one weld pass of said weld wire in a substantially undiluted condition.

### Claim 36 (depends on 35)

The method of creating a welded ductile iron joint according to claim 35, wherein at least one of steps b, c, and d is accomplished using a pulse MIG welder.

### Claim 37 (depends on 35)

The method of creating a welded ductile iron joint according to claim 35, further comprising the step of abstaining from pre-heating, post-heating, or chemical antimartensitizing treatment of a heat affected zone.

### Claim 38 (depends on 35)

A method of producing a highly ductile weld as in claim 35, wherein said substantially pure inert gas comprises an inert gas in combination with reducing gasses.

### Claim 39 (depends on 35)

A method of producing a highly ductile weld as in claim 35, wherein said substantially pure inert gas comprises argon gas.

### Claim 40 (depends on 35)

A method of producing a highly ductile weld as in claim 35, wherein said substantially pure inert gas comprises argon gas in combination with a reducing gas.

### Claim 41

A method of creating a welded ductile iron joint having a yield strength of less than a tensile strength of a heat affected zone in said ductile iron joint, comprising compensating for a brittleness of said heat affected zone by creating a highly ductile weld bead in the absence of flux using a filler metal or a consumable electrode of a high ductility material consisting essentially of nickel.

### Claim 42 (depends on 41)

The method of creating a welded ductile iron joint according to claim 41, wherein said heat affected zone is not subjected to any of pre-heating, post-heating, or chemical antimartensitizing treatment.