# US 6,730,770 B2 · Method of preparing a higher solids phenolic resin

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,770 B2
- Document ID: US6730770B2
- Status: Granted
- Kind: B2
- Application number: 10/160,324
- Filed: 2002-05-31
- Published: 2003-12-04
- Granted: 2004-05-04
- Earliest claimed: 2002-05-31
- Assignees: CertainTeed Corporation
- Inventors: Kathleen H. Coventry-Saylor
- Web page: https://patentgrep.com/patent/US6730770B2

## CPC

- C03C 25/34: Condensation polymers of aldehydes, e.g. with phenols, ureas, melamines, amides or amines
- C09J 161/34: Condensation polymers of aldehydes or ketones with monomers covered by at least two of the groups C09J161/04, C09J161/18 and C09J161/20
- H05K 1/0366: {reinforced, e.g. by fibres, fabrics (H05K1/036 takes precedence)}
- Y10T 428/2938: Coating on discrete and individual rods, strands or filaments
- Y10T 428/2967: Synthetic resin or polymer
- Y10T 428/31601: Quartz or glass
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A phenol-formaldehyde resole resin for use as a binder for glass fibers is acidified with sulfamic acid to a pH of 3 or less after base-catalyzed resinification. An increase in actual solids observed compared with neutralized resin, reflecting a desired improvement in efficiency.

## Claims

### Claim 1

A process for preparing a phenolic binder for glass fibers, the process comprising a) preparing a water-soluble phenol-formaldehyde resole resin by:
1) preparing an initial aqueous mixture including formaldehyde and phenol;
2) adding a basic polymerization catalyst to the initial aqueous mixture;
3) maintaining the aqueous mixture at a predetermined temperature during reaction of the phenol and formaldehyde to form the water-soluble phenol-formaldehyde resole resin until the free formaldehyde content of the aqueous mixture drops to a predefined level;
4) cooling the aqueous mixture; and
5) acidifying the aqueous mixture with sulfamic acid to a pH of no greater than 3;
b) subsequently completing preparation of the binder by adding a catalyst for curing the modified resole resin.

### Claim 2 (depends on 1)

A process according to claim 1 further comprising
a) preparing an aqueous, reaction mixture including the phenol-formaldehyde resole resin and urea; and
b) permitting the urea to react with the phenol-formaldehyde resole resin to form a modified resin.

### Claim 3 (depends on 1)

A process according to claim 1 further comprising mixing an acidic modifier with the aqueous mixture.

### Claim 4 (depends on 3)

A process according to claim 3 wherein the acidic modifier is a latent catalyst.

### Claim 5 (depends on 3)

A process according to claim 3 wherein the acidic modifier is a reactive diluent.

### Claim 6 (depends on 1)

A process according to claim 1 wherein the phenol-formaldehyde resin has a formaldehyde-to-phenol mole ratio of from about 25:1 to 4.2:1.

### Claim 7 (depends on 6)

A process according to claim 6 wherein the phenol-formaldehyde resin has a formaldehyde-to-phenol ratio of from about 3.2:1 to 4.0:1.

### Claim 8 (depends on 1)

A process according to claim 1 wherein the predefined level is about 40 percent by weight of the free formaldehyde in the initial aqueous mixture.

### Claim 9 (depends on 2)

A process according to claim 2 further comprising adding ammonia to the reaction mixture wherein the ammonia is added in sufficient quantity to give a weight ratio of ammonia to solids of unmodified resin of from about 1.0:100 to 3.0:100.

### Claim 10 (depends on 1)

A process according to claim 1 wherein the aqueous mixture including the unmodified resole resin is acidified to a pH from about 2 to 3.

### Claim 11 (depends on 2)

A process according to claim 2 wherein the mole ratio of the urea to the free formaldehyde of the phenol-formaldehyde resin is from about 1:1 to 1.75:1.

### Claim 12 (depends on 2)

A process according to claim 2 wherein the aqueous mixture is agitated for at least a time sufficient to ensure complete mixing.

### Claim 13 (depends on 2)

A process according to claim 2 wherein the aqueous mixture is maintained at a temperature of from about 5° C. to 30° C. while permitting the urea to react with the resole resin.

### Claim 14 (depends on 2)

A process according to claim 2 wherein completing preparation of the binder further includes adding a mineral oil lubricant and an organo-silane adhesion promoter to the aqueous mixture including the modified resole resin.

### Claim 15 (depends on 1)

An improved binder for glass fibers prepared according to the process of claim 1.

### Claim 16

A process for producing a glass fiber batt, the process comprising:
a) preparing a water-soluble phenol-formaldehyde resole resin by:
1) preparing an initial aqueous mixture including formaldehyde and phenol;
2) adding a basic polymerization catalyst to the initial aqueous mixture;
3) maintaining the aqueous mixture at a predetermined temperature during reaction of the phenol and formaldehyde to form the water-soluble phenol-formaldehyde resole resin until the free formaldehyde content of the aqueous mixture drops to a predefined level;
4) cooling the aqueous mixture; and
5) acidifying the aqueous mixture with sulfamic acid to a pH of no greater than 3;
b) preparing a binder for the glass fibers by subsequently adding a catalyst for curing the modified resole resin,
c) spraying the binder on glass fibers to form a batt and
d) curing the binder at an elevated temperature.

### Claim 17 (depends on 16)

The process of claim 16 further comprising
a) preparing an aqueous reaction mixture including the phenol-formaldehyde resole resin and urea; and
b) permitting the urea to react with the phenol-formaldehyde resole resin to form a modified resin.

### Claim 18 (depends on 17)

A process according to claim 17 further comprising adding ammonia to the reaction mixture.

### Claim 19 (depends on 16)

A process according to claim 16 further comprising mixing an acidic additive with the aqueous mixture.

### Claim 20 (depends on 16)

A product prepared by the process of claim 16.