# US 6,730,761 B2 · Thermoprocessable copolymers of TFE

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,761 B2
- Document ID: US6730761B2
- Status: Granted
- Kind: B2
- Application number: 10/322,631
- Filed: 2002-12-19
- Published: 2003-08-21
- Granted: 2004-05-04
- Earliest claimed: 2001-12-21
- Assignees: Ausimont S.p.A.
- Inventors: Pasqua Colaianna; Giulio Brinati; Giambattista Besana
- Web page: https://patentgrep.com/patent/US6730761B2

## CPC

- C08F 214/26: Tetrafluoroethene
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

Thermoprocessable copolymers of TFE essentially formed by the following monomers: (a) FMVE; ((b) a perfluorodioxole of formula: the complement to 100% by weight being TFE.

## Claims

### Claim 1

Thermoprocessable copolymers of TFE consisiting essentially of the following monomers in the indicated amounts:
A)
(a) 8.6-9.8% by weight of perfluoromethylvinylether (FMVE);
(b) 0.3-1.2% by weight of a perfluorodioxole of formula:
wherein:
Y═F, ORf, Rf wherein Rf is a perfluoroalkyl having from 1 to 5 carbon atoms;
X1 and X2, equal to or different from each other, are —F or —CF3;
with the proviso that the sum of the percentages by weight of (a)+(b) is from 8.9 to 11% by weight; or
B)
(a) 4.5-8.5% by weight of perfluoromethylvinylether (FMVE);
(b) 1.7-7.5% by weight of a perfluorodioxole as defined in A);
with the proviso that the sum of the percentages by weight of (a)+(b) is from 6.2 to 11% by weight;
the complement to 100% by weight in compositions A) and B) being TFE;
said copolymers having:
an amount of ionic end groups —COOH and —COF, not higher than 5×10−4 moles/Kg polymer;
release values of F− ions, determined on the polymer in pellet, not higher than 1 ppm by weight with respect to the polymer weight;
wherein the manufactured articles obtained from the polymers having compositions A) or B) show the following mechanical properties:
elongation at break≧130% measured at 23° C. along the welding lines of the injection moulded articles;
stress at break≧2.5 MPa and elongation at break≧250%, measured at 250° C. on compression moulded plaque.

### Claim 2 (depends on 1)

Copolymers according to claim 1, wherein in formula (I) of comonomer (b) Y═ORf, Rf═—CF3; X1═X2═F.

### Claim 3 (depends on 1)

Copolymers according to claim 1, wherein the Melt Flow Index measured at 372° C. with a load of 5 Kg is from 1 to 40 g/10′ preferably from 6 to 30 g/10′.

### Claim 4 (depends on 1)

Manufactured articles obtainable by injection moulding of the thermoprocessable copolymers according to claim 1, having the following mechanical properties:
elongation at break measured at 23° on the welding lines from 150% to 300%;
stress at break at 250° C. from 2.5 to 6 MPa;
elongation at break at 250° from 270 to 500%.

### Claim 5 (depends on 4)

Manufactured articles according to claim 4 in the form of fittings.

### Claim 6 (depends on 1)

Process for obtaining manufactured articles by injection molding of copolymers according to claim 1.

### Claim 7 (depends on 2)

Process for obtaining manufactured articles by injection molding of copolymers according to claim 2.

### Claim 8 (depends on 3)

Process for obtaining manufactured articles by injection molding of copolymers according to claim 3.