# US 6,730,738 B2 · Hot-melt adhesive

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,738 B2
- Document ID: US6730738B2
- Status: Granted
- Kind: B2
- Application number: 10/310,081
- Filed: 2002-12-04
- Published: 2003-06-12
- Granted: 2004-05-04
- Earliest claimed: 2001-12-06
- Assignees: Rohm and Haas Company
- Inventors: Larry Frank Brinkman
- Web page: https://patentgrep.com/patent/US6730738B2

## CPC

- C08G 18/6696: {with compounds of group C08G18/36 or hydroxylated esters of higher fatty acids of C08G18/38}
- C08G 18/12: using two or more compounds having active hydrogen in the first polymerisation step
- C08G 18/4063: {Mixtures of compounds of group C08G18/62 with other macromolecular compounds}
- C08G 18/6212: {Polymers of alkenylalcohols; Acetals thereof; Oxyalkylation products thereof}
- C08G 18/6547: {the low-molecular compounds being compounds of group C08G18/36 or hydroxylated esters of higher fatty acids of C08G18/38}
- C08G 2170/20: Compositions for hot melt adhesives
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

A moisture-reactive hot-melt adhesive composition is provided. Particularly, a composition that includes a polyether polyol, a polyester polyol, a styrene/allyl alcohol copolymer, and a polyisocyanate. More particularly, the components are chosen so that the ratio of NCO/OH groups on an equivalents basis is from 1.8/1 to 3.0/1; the components contain less than 1% by weight of water; the weight ratio of polyether polyol to polyester polyol is at least 0.42; and the free NCO content is at least 5.5% by weight. Also provided are a method for forming the adhesive composition and a method for bonding substrates using the adhesive.

## Claims

### Claim 1

A moisture-reactive hot-melt adhesive composition formed by admixing components comprising a polyether polyol, a polyester polyol, a styrene/allyl alcohol copolymer, and a polyisocyanate; wherein the ratio of NCO/OH groups of said components on an equivalents basis is from 1.8/1 to 3.0/1; wherein said components contain less than 1%, by weight based on the total weight of said components, water; and wherein the free NCO content of said components is at least 4%, based on the total weight of said components.

### Claim 2 (depends on 1)

The composition of claim 1, wherein the ratio of the weight of said polyether polyol to the weight of said polyester polyol is at least 0.42.

### Claim 3 (depends on 1)

The composition of claim 1, wherein said polyether polyol comprises polypropylene glycol with molecular weight of between 1,000 and 3,000.

### Claim 4 (depends on 1)

The composition of claim 1, wherein said polyisocyanate comprises 4,4′ diphenylmethane diisocyanate.

### Claim 5 (depends on 4)

The composition of claim 4 wherein the ratio of the weight of said polyether polyol to the weight of said polyester polyols is at least 0.42; and wherein said polyether polyol comprises polypropylene glycol with molecular weight of between 1,000 and 3,000.

### Claim 6

A method for forming a moisture-reactive hot-melt adhesive comprising admixing components comprising a polyether polyol, a polyester polyol, a styrene/allyl alcohol copolymer, and a polyisocyanate; wherein the ratio of NCO/OH groups of said components on an equivalents basis is from 1.8/1 to 3.0/1; wherein said components contain less than 1%, by weight based on the total weight of said components, water; and wherein the free NCO content of said components is at least 4%, based on the total weight of said components.

### Claim 7 (depends on 6)

The method of claim 6 wherein the ratio of the weight of said polyether polyol to the weight of said polyester polyols is at least 0.42; wherein said polyether polyol comprises polypropylene glycol with molecular weight of between 1,000 and 3,000; and wherein said polyisocyanate comprises 4,4′ diphenylmethane diisocyanate.

### Claim 8

A method for bonding substrates comprising
(a) forming a moisture-reactive hot-melt adhesive by admixing components comprising a polyether polyol, a polyester polyol, a styrene/allyl alcohol copolymer, and a polyisocyanate; wherein the ratio of NCO/OH groups of said components on an equivalents basis is from 1.8/1 to 3.0/1; wherein said components contain less than 1%, by weight based on the total weight of said components, water; and wherein the free NCO content of said components is at least 4%, based on the total weight of said components;
(b) heating said hot-melt adhesive;
(c) applying said heated hot-melt adhesive to a first substrate in the presence of moisture;
(d) contacting said applied heated hot-melt adhesive with a second substrate; and
(e) cooling, or allowing to cool, said hot-melt adhesive.

### Claim 9 (depends on 8)

The method of claim 8 wherein the ratio of the weight of said polyether polyol to the weight of said polyester polyols is at least 0.42; wherein said polyether polyol comprises polypropylene glycol with molecular weight of between 1,000 and 3,000; and wherein said polyisocyanate comprises 4,4′ diphenylmethane diisocyanate.