# US 6,730,728 B2 · Propylene resin composition excellent in moldability and physical properties

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,728 B2
- Document ID: US6730728B2
- Status: Granted
- Kind: B2
- Application number: 09/926,063
- Filed: 2002-01-11
- Published: 2003-05-15
- Granted: 2004-05-04
- Earliest claimed: 1999-12-27
- Assignees: Japan Polychem Corporation; Toyota Jidosha Kabushiki Kaisha
- Inventors: Masatoshi Matsuda; Hisayuki Iwai; Takayuki Nagai; Yukihito Zanka; Mitsuhiro Murayama; Yuji Fujita; Hironari Sano
- Web page: https://patentgrep.com/patent/US6730728B2

## CPC

- C08L 53/00: Compositions of block copolymers containing at least one sequence of a polymer obtained by reactions only involving carbon-to-carbon unsaturated bonds; Compositions of derivatives of such polymers
- C08L 23/10: Homopolymers or copolymers of propene
- C08L 53/025: {modified}
- C08L 23/0815: {with aliphatic 1-olefins containing one carbon-to-carbon double bond}
- C08L 23/16: Ethylene-propylene or ethylene-propylene-diene copolymers
- C08L 53/02: of vinyl-aromatic monomers and conjugated dienes
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

The present invention provides a resin composition high in melting flow, exhibiting good properties, excellent in moldability and shrinkage properties, and hence suitable for automobile exteriors, by including (A) propylene/ethylene block copolymer having a melt flow rate (MFR) of 100 to 200 g/10 min., its propylene homopolymer component having an MFR of 210 to 400 g/10 min. and isotactic pentad fraction of 0.98 or more, and its copolymer portion containing propylene at 65 to 85% by weight; 50 to 70% by weight, (B) ethylene/octene and/or ethylene/butene random copolymer; 10 to 25% by weight, (C) styrene-based hydrogenated block copolymer rubber; 4 to 9% by weight and (D) talc; 16 to 24% by weight.

## Claims

### Claim 1

A polypropylene-based resin composition comprising the following components (A) to (D), characterized by its excellent moldability and other properties:
50 to 70% by weight component (A): propylene/ethylene block copolymer having a melt flow rate (MFR) of 100 to 200 g//10 min., its propylene homopolymer component having an MFR of 210 to 400 g/10 min. and isotactic pentad fraction of 0.98 or more, and its copolymer portion containing propylene at 65 to 85% by weight;
10 to 25% by weight component (B): ethylene/octene and/or ethylene/butene random copolymer, containing the comonomers at 28% by weight or more for the copolymerization and having an MFR of 0.5 to 20 g/10 min.;
4 to 9% by weight component (C): styrene-based hydrogenated block copolymer rubber having the structure A-B or A-B-A wherein the segment A is a polystyrene structure and segment B is an ethylene/butene or ethylene/propylene structure, containing the segment A of polystyrene structure at 1 to 25% by weight; and
16 to 24% by weight component (D): talc, having an average particle size of 10 mm or less, determined by the laser-aided diffractometry.

### Claim 2 (depends on 1)

The polypropylene based resin composition according to claim 1 having an internal molding pressure of 38 MPa or less, MFR of 36 to 50 g/10 min., flexural modulus of elasticity of 1750 MPa or more, brittleness temperature of −15° C. or lower, tensile elongation of 200% or more, and difference between molding shrinkage and shrinkage after heating of 1.5/1000 or less.