# US 6,730,712 B2 · Method of manufacturing porous cross-linked polymer sheet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,712 B2
- Document ID: US6730712B2
- Status: Granted
- Kind: B2
- Application number: 10/169,182
- Filed: 2002-09-27
- Published: 2003-08-14
- Granted: 2004-05-04
- Earliest claimed: 2000-10-25
- Assignees: Nippon Shokubai Co., Ltd.
- Inventors: Masazumi Sasabe; Katsuhiko Sakamoto; Kozo Nogi; Motohiro Arakawa
- Web page: https://patentgrep.com/patent/US6730712B2

## CPC

- C08J 9/28: by elimination of a liquid phase from a macromolecular composition or article, e.g. drying of coagulum
- B29C 44/5654: {Subdividing foamed articles to obtain particular surface properties, e.g. on multiple modules}
- C08J 2201/028: Foaming by preparing of a high internal phase emulsion
- C08J 2201/0504: the liquid phase being aqueous
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)

## Abstract

A method for producing a porous cross-linked polymer sheet capable of slicing quickly is provided. This method comprises a step for obtaining a porous cross-linked polymer by forming and polymerizing an HIPE, a step for dehydrating the porous cross-linked polymer, and a step for subsequently slicing the dehydrated porous cross-linked polymer. According to this invention, by performing the step of dehydration prior to the conventional step of slicing, it is made possible to prevent the porous cross-linked polymer from adhering to the blade and the guides provided for a slicer, and allow the slicing to be attained quickly. By removing the salt from the polymer, it is further made possible to prevent a production device from gathering rust and the porous cross-linked polymer from permitting adhesion of rust thereto.

## Claims

### Claim 1

A method for the production of a porous cross-linked polymer sheet, comprising a step for obtaining a porous cross-linked polymer by forming and polymerizing a water-in-oil type high internal phase emulsion, a step for dehydrating the porous cross-linked polymer, and a step for subsequently slicing the porous cross-linked polymer.

### Claim 2

A method for the production of a porous cross-linked polymer sheet, comprising a step for obtaining a porous cross-linked former-stage polymer by forming a water-in-oil type high internal phase emulsion and subjecting the formed water-in-oil type high internal phase emulsion to a former-stage polymerization, a step for dehydrating the porous cross-linked former-stage polymer, a step of subsequently slicing the porous cross-linked former-stage polymer into pieces of a prescribed thickness, and a step for subjecting the porous cross-linked former-stage polymer to a latter-stage polymerization thereby obtaining a porous cross-linked polymer.

### Claim 3 (depends on 2)

A method according to claim 2, which further comprises a step of dehydrating said porous cross-linked polymer subsequent to said step of obtaining said porous cross-linked polymer.

### Claim 4 (depends on 1)

A method according to claim 1, wherein the step of dehydrating the porous cross-linked polymer or the porous cross-linked former-stage polymer is carried out by a compressing operation.

### Claim 5 (depends on 1)

A method according to claim 1, wherein the porous cross-linked polymer has a thickness of not more than 100 mm prior to said dehydration.

### Claim 6 (depends on 2)

A method according to claim 2, wherein the step of dehydrating the porous cross-linked polymer or the porous cross-linked former-stage polymer is carried out by a compressing operation.

### Claim 7 (depends on 3)

A method according to claim 3, wherein the step of dehydrating the porous cross-linked polymer or the porous cross-linked former-stage polymer is carried out by a compressing operation.

### Claim 8 (depends on 2)

A method according to claim 2, wherein the porous cross-linked former-stage polymer or the porous cross-linked polymer has a thickness of not more than 100 mm prior to said dehydration.

### Claim 9 (depends on 3)

A method according to claim 3, wherein the porous cross-linked former-stage polymer or the porous cross-linked polymer has a thickness of not more than 100 mm prior to said dehydration.

### Claim 10 (depends on 4)

A method according to claim 4, wherein the porous cross-linked polymer has a thickness of not more than 100 mm prior to said dehydration.

### Claim 11 (depends on 6)

A method according to claim 6, wherein the porous cross-linked former-stage polymer or the porous cross-linked polymer has a thickness of not more than 100 mm prior to said dehydration.

### Claim 12 (depends on 7)

A method according to claim 7, wherein the porous cross-linked former-stage polymer or the porous cross-linked polymer has a thickness of not more than 100 mm prior to said dehydration.