# US 6,730,624 B2 · Non-reducing dielectric ceramic, monolithic ceramic capacitor using the same, and method for making non-reducing dielectric ceramic

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,624 B2
- Document ID: US6730624B2
- Status: Granted
- Kind: B2
- Application number: 10/427,978
- Filed: 2003-05-02
- Published: 2003-11-13
- Granted: 2004-05-04
- Earliest claimed: 2000-04-07
- Assignees: Murata Manufacturing Co., Ltd.
- Inventors: Tomoo Motoki; Masahiro Naito; Harunobu Sano
- Web page: https://patentgrep.com/patent/US6730624B2

## CPC

- C04B 35/465: based on alkaline earth metal titanates
- H01G 4/1227: {based on alkaline earth titanates}
- H01G 4/1236: {based on zirconium oxides or zirconates (H01G4/1263 takes precedence)}
- H01G 4/1245: {containing also titanates}
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)

## Abstract

A non-reducing dielectric ceramic contains Ca, Zr and Ti as metallic elements and does not contain Pb. In a CuKα X-ray diffraction pattern, the ratio of the maximum peak intensity of secondary crystal phases to the maximum peak intensity at 2θ=25° to 35° of a perovskite primary crystal phase is about 12% or less, the secondary crystal phases including all the crystal phases other than the perovskite primary crystal phase. The non-reducing dielectric ceramic exhibits superior insulating resistance and dielectric loss after firing in a neutral or reducing atmosphere and high reliability in a high-temperature loading lifetime test and is useful for producing compact high-capacitance monolithic ceramic capacitors.

## Claims

### Claim 1

A monolithic ceramic capacitor comprising:
at least three dielectric ceramic layers;
at least one pair of internal electrodes each of which is disposed between a different pair of dielectric ceramic layers;
a pair of external electrodes, each of which is electrically connected to a different one of said pair of internal electrodes;
wherein the dielectric ceramic layers comprise a non-reducing dielectric ceramic comprising Ca, Zr and Ti as metallic elements, free of Pb, and having a perovskite primary crystal phase and other crystal phases;
wherein the ratio of the maximum peak intensity of secondary crystal phases to the maximum peak intensity at 2θ=25° to 35° of the perovskite primary crystal phase in a CuKα X-ray diffraction pattern is about 12% or less, wherein the secondary crystal phases include all the crystal phases other than the perovskite primary crystal phase; and
wherein the internal electrodes comprise a base metal.

### Claim 2 (depends on 1)

A monolithic ceramic capacitor according to claim 1, wherein the base metal is at least one member selected from the group consisting of elemental nickel, a nickel alloy, elemental copper and a copper alloy.

### Claim 3 (depends on 2)

A monolithic ceramic capacitor according to claim 2, wherein said ratio is about 5% or less.

### Claim 4 (depends on 2)

A monolithic ceramic capacitor according to claim 2, wherein said ratio is about 3% or less.

### Claim 5 (depends on 1)

A monolithic ceramic capacitor according to claim 1, wherein said ceramic is represented by the formula ApBO3 in which A comprises Ca, B comprises Zr and Ti, and p is about 0.98 to 1.02.

### Claim 6 (depends on 5)

A monolithic ceramic capacitor according to claim 5, wherein said ratio is about 5% or less.

### Claim 7 (depends on 5)

A monolithic ceramic capacitor according to claim 5, wherein p is about 0.99 to 1.01.

### Claim 8

A method for making a non-reducing dielectric ceramic comprising Ca, Zr and Ti as metallic elements, free of Pb, and having a ratio of the maximum peak intensity of secondary crystal phases to the maximum peak intensity at 20=25° to 35° of a perovskite primary crystal phase in a CuKα X-ray diffraction pattern of about 12% or less, wherein the secondary crystal phases include all the crystal phases other than the perovskite primary crystal phase, the method comprising the steps of:
(A) providing a calcined powder for providing the B-site component of a dielectric ceramic represented by the general formula ApBO3;
(B) providing powder for providing the A-site component;
(C) mixing the calcined B-site component powder and the A-site component powder to prepare an uncalcined primary material powder;
(D) calcining the uncalcined primary material powder to prepare a calcined primary material powder;
(E) adjusting the composition of the calcined primary material powder to realize the desired value of p by adding at least one of the A-site component powder and B-site component powder to the calcined primary material powder to prepare a secondary material powder; and
(F) molding and sintering the secondary material powder under a neutral or reducing atmosphere.

### Claim 9 (depends on 8)

A method for making a non-reducing dielectric ceramic according to claim 8, further comprising calcining a B-site component powder.

### Claim 10 (depends on 9)

A method for making a non-reducing dielectric ceramic according to claim 9, wherein the B-site component powder which is calcined has an average particle diameter of about 0.5 μm or less.

### Claim 11 (depends on 9)

A method for making a non-reducing dielectric ceramic according to claim 9, wherein the uncalcined B-site component powder is calcined at a temperature of about 1,050° C. to 1,200° C. for 1 to 2 hours.

### Claim 12 (depends on 11)

A method for making a non-reducing dielectric ceramic according to claim 11, wherein the calcined primary material powder has an average particle diameter of about 0.8 μm or less.

### Claim 13 (depends on 11)

A method for making a non-reducing dielectric ceramic according to claim 11, wherein the provided powders are such that the calcined primary material powder is a ceramic powder having a composition represented by
(Ca1-v-wSrvBaw)k(Zr1-x-yTixHfy)O3
wherein 0.95≦k≦1.00, v+w is 0 to less than 1, x is greater than 0, and x+y is less than 1.

### Claim 14 (depends on 13)

A method for making a non-reducing dielectric ceramic according to claim 13, wherein the secondary material powder is a ceramic powder having a composition represented by (Ca1-v-wSrvBaw)p(Zr1-x-yTixHfy)O3, and wherein p is adjusted to a value of about 0.98 to 1.02.

### Claim 15 (depends on 14)

A method for making a non-reducing dielectric ceramic according to claim 14, wherein p is adjusted to a value of about 0.98 to 1.02.

### Claim 16 (depends on 15)

A method for making a non-reducing dielectric ceramic according to claim 15, wherein the B-site component powder which is calcined has an average particle diameter of about 0.5 μm or less.