# US 6,730,619 B2 · Method of manufacturing insulating layer and semiconductor device including insulating layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,619 B2
- Document ID: US6730619B2
- Status: Granted
- Kind: B2
- Application number: 10/122,272
- Filed: 2002-04-16
- Published: 2002-09-19
- Granted: 2004-05-04
- Earliest claimed: 2000-06-15
- Assignees: Samsung Electronics Co., Ltd.
- Inventors: Woo-Chan Jung; Jin-Ho Jeon; Jeon-Sig Lim; Jong-Seung Yi
- Web page: https://patentgrep.com/patent/US6730619B2

## CPC

- H10P 14/6923: {the material being boron or phosphorus doped silicon oxides, e.g. BPSG, BSG or PSG}
- C23C 16/401: {containing silicon}
- C23C 16/56: After-treatment
- H10P 14/6506: {Formation of intermediate materials}
- H10P 14/6529: {by exposure to a gas or vapour}
- H10P 14/6334: {using decomposition or reaction of gaseous or vapour phase compounds, i.e. chemical vapour deposition (deposition by physical ablation of a target H10P14/6329)}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6686: {the compound being a molecule comprising at least one silicon-oxygen bond and the compound having hydrogen or an organic group attached to the silicon or oxygen, e.g. a siloxane}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 14/6922: {the material containing Si, O and at least one of H, N, C, F or other non-metal elements, e.g. SiOC, SiOC:H or SiONC}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A method of manufacturing an insulating layer that ensures reproducibility across like manufacturing apparatus. The insulating layer is formed on the substrate by (a) flowing an oxidizing gas at an oxidizing gas flow rate, (b) flowing a first carrier gas at a first carrier gas flow rate while carrying a first impurity including boron flowing at a first impurity flow rate, (c) flowing a second carrier gas at a second carrier gas flow rate while carrying a second impurity including phosphorus flowing at a second impurity flow rate, and (d) flowing a silicon source material at a silicon source flow rate. The second carrier gas flow rate is greater than the first carrier gas flow rate.

## Claims

### Claim 1

A method of manufacturing an insulating layer comprising:
creating a process atmosphere in a chamber for forming a fluidal insulating layer by (a) flowing an oxidizing gas at an oxidizing gas flow rate for forming an oxidizing atmosphere, (b) flowing a first carrier gas at a first carrier gas flow rate, and (c) flowing a second carrier gas at a second carrier gas flow rate, the second carrier gas flow rate being greater than the first carrier gas flow rate; and
forming the fluidal insulating layer on a substrate positioned in the chamber by (d) flowing the oxidizing gas at the oxidizing gas flow rate, (e) flowing the first carrier gas at the first carrier gas flow rate while carrying a first impurity including boron flowing at a first impurity flow rate, (f) flowing the second carrier gas at the second carrier gas flow rate while carrying a second impurity including phosphorus flowing at a second impurity flow rate, the second carrier gas flow rate being greater than the first carrier gas flow rate, and (g) flowing a silicon source material at a silicon source flow rate.

### Claim 2 (depends on 1)

A method of manufacturing an insulating layer as claimed in claim 1, wherein during the creating and forming steps, the oxidizing gas is one selected from a group consisting of oxygen gas, ozone gas and a mixture thereof, the first carrier gas is a nitrogen gas, the second carrier gas is a helium gas, the silicon source material is tetraethylorthosilicate (TEOS), the first impurity is one selected from a group consisting of triethylborate (TEB), trimethylborate (TMB), and a mixture thereof, and the second impurity is one selected from a group consisting of triethylphosphate (TEPO), trimethylphosphate (TMPO) and a mixture thereof.

### Claim 3 (depends on 1)

A method of manufacturing an insulating layer as claimed in claim 1, wherein for the forming of the process atmosphere, a ratio of the oxidizing gas flow rate, the first carrier gas flow rate, and the second carrier gas flow rate is about 1.00-2.50:0.70-0.95:1.

### Claim 4 (depends on 3)

A method of manufacturing an insulating layer as claimed in claim 3, wherein the second carrier gas flow rate is at least 4,000 sccm.

### Claim 5 (depends on 1)

A method of manufacturing an insulating layer as claimed in claim 1, wherein for the forming of the fluidal insulating layer, a ratio of the oxidizing gas flow rate, the first carrier gas flow rate, the second carrier gas flow rate, the silicon source flow rate, the first impurity flow rate, and the second impurity flow rate is about 2.00-2.50:0.70-0.95:1:0.15-0.25:0.040-0.045:0.013-0.014.

### Claim 6 (depends on 5)

A method of manufacturing an insulating layer as claimed in claim 5, wherein the second carrier gas flow rate is at least 4,000 sccm.

### Claim 7 (depends on 1)

A method of manufacturing an insulating layer as claimed in claim 1, further comprising forming an etch stop layer on the substrate prior to forming the fluidal insulating layer.

### Claim 8 (depends on 1)

A method of manufacturing an insulating layer as claimed in claim 1, wherein before forming the fluidal insulating layer, further comprising forming an undoped fluidal insulating layer on the substrate, and wherein for forming the undoped fluidal insulating layer, the ratio of the oxidizing gas flow rate, the first carrier gas flow rate, the second carrier gas flow rate, and the silicon source flow rate is about 2.00-2.50:0.70-0.95:1:0.15-0.25.

### Claim 9 (depends on 8)

A method of manufacturing an insulating layer as claimed in claim 8, wherein the second carrier gas flow rate is at least 4,000 sccm.

### Claim 10 (depends on 8)

A method of manufacturing an insulating layer as claimed in claim 8, wherein the undoped fluidal insulating layer is formed within about three seconds.

### Claim 11 (depends on 1)

A method of manufacturing an insulating layer as claimed in claim 1, further comprising reflowing the fluidal insulating layer after the forming thereof.

### Claim 12 (depends on 1)

A method of manufacturing an insulating layer as claimed in claim 1, wherein the creating of the process atmosphere in the chamber includes,
flowing the oxidizing gas, the first carrier gas, and the second carrier gas in the chamber in a flow rate ratio of about 1.00-1.25:0.70-0.95:1;
forming a pressurized atmosphere in the chamber utilizing a pumping apparatus communicating with the chamber, while flowing the oxidizing gas, the first carrier gas, and the second carrier gas in the chamber in a flow rate ratio of about 2.00-2.50:0.70-0.95:1; and
stabilizing the pressurized atmosphere formed in the chamber by flowing the oxidizing gas, the first carrier gas, and the second carrier gas in the chamber in a flow rate ratio of about 2.00-2.50:0.70-0.95:1.

### Claim 13 (depends on 12)

A method of manufacturing an insulating layer as claimed in claim 12, wherein the flowing continues for less than five seconds, the forming a pressurized atmosphere continues for less than 60 seconds at a pressure of at least 160 Torr, and the stabilizing continues for less than fifteen seconds.

### Claim 14 (depends on 1)

A method of manufacturing an insulating layer as claimed in claim 1, wherein the fluidal insulating layer is formed within fifteen seconds.

### Claim 15

A method of manufacturing a semiconductor device comprising:
forming an etch stop layer on a substrate positioned in a chamber;
creating a process atmosphere in the chamber for forming a fluidal insulating layer by (a) flowing an oxidizing gas at an oxidizing gas flow rate for forming an oxidizing atmosphere, (b) flowing a first carrier gas at a first carrier gas flow rate, and (c) flowing a second carrier gas at a second carrier gas flow rate, the second carrier gas flow rate being greater than the first carrier gas flow rate;
forming a fluidal insulating layer on the etch stop layer by (d) flowing the oxidizing gas at the oxidizing gas flow rate, (e) flowing the first carrier gas at the first carrier gas flow rate while carrying a first impurity including boron flowing at a first impurity flow rate, (f) flowing the second carrier gas at the second carrier gas flow rate while carrying a second impurity including phosphorus flowing at a second impurity flow rate, the second carrier gas flow rate being greater than the first carrier gas flow rate, and (g) flowing a silicon source material at a silicon source flow rate;
reflowing the fluidal insulating layer utilizing oxygen gas and hydrogen gas to planarize an upper surface of the fluidal insulating layer and to fill recessed portions on the substrate with the fluidal insulating layer; and
forming a pattern having a window in the fluidal insulating layer for exposing a surface of the etch stop layer by etching a predetermined portion of the fluidal insulating layer.

### Claim 16 (depends on 15)

A method of manufacturing a semiconductor device as claimed in claim 15, wherein the etch stop layer comprises silicon nitride and is formed to a thickness of about 60-150 Å.

### Claim 17 (depends on 15)

A method of manufacturing a semiconductor device as claimed in claim 15, wherein the oxidizing gas is one selected from a group consisting of oxygen gas, ozone gas and a mixture thereof, the first carrier gas is a nitrogen gas, the second carrier gas is a helium gas, and wherein ratio of the oxidizing gas flow rate, the first carrier gas flow rate, and the second carrier gas flow rate is about 1.00-2.50:0.70-0.95:1.

### Claim 18 (depends on 17)

A method of manufacturing a semiconductor device as claimed in claim 17, wherein the second carrier gas flow rate is at least 4,000 sccm.

### Claim 19 (depends on 17)

A method of manufacturing a semiconductor device as claimed in claim 17, wherein the creating of the process atmosphere in the chamber includes,
flowing the oxidizing gas, the first carrier gas, and the second carrier gas in the chamber in a flow rate ratio of about 1.00-1.25:0.70-0.95:1;
forming a pressurized atmosphere in the chamber utilizing a pumping apparatus communicating with the chamber, while flowing the oxidizing gas, the first carrier gas, and the second carrier gas in the chamber in a flow rate ratio of about 2.00-2.50:0.70-0.95:1; and
stabilizing the pressurized atmosphere formed in the chamber by flowing the oxidizing gas, the first carrier gas, and the second carrier gas in the chamber in a flow rate ratio of about 2.00-2.50:0.70-0.95:1.

### Claim 20 (depends on 19)

A method of manufacturing a semiconductor device as claimed in claim 19, wherein the flowing continues for less than five seconds, the forming a pressurized atmosphere continues for less than 60 seconds at a pressure of at least 160 Torr, and the stabilizing continues for less than fifteen seconds.

### Claim 21 (depends on 15)

A method of manufacturing a semiconductor device as claimed in claim 15, wherein during the creating and forming steps, the oxidizing gas is one selected from a group consisting of oxygen gas, ozone gas and a mixture thereof, the first carrier gas is a nitrogen gas, the second carrier gas is a helium gas, the silicon source material is tetraethylorthosilicate (TEOS), the first impurity is one selected from a group consisting of triethylborate (TEB), trimethylborate (TM B), and a mixture thereof, and the second impurity is one selected from a group consisting of triethylphosphate (TEPO), trimethylphosphate (TMPO) and a mixture thereof.

### Claim 22 (depends on 21)

A method of manufacturing a semiconductor device as claimed in claim 21, wherein for the forming of the fluidal insulating layer, a ratio of the oxidizing gas flow rate, the first carrier gas flow rate, the second carrier gas flow rate, the silicon source flow rate, the first impurity flow rate, and the second impurity flow rate is about 2.00-2.50:0.70-0.95:1:0.15-0.25:0.040-0.045:0.013-0.014.

### Claim 23 (depends on 22)

A method of manufacturing a semiconductor device as claimed in claim 22, wherein the second carrier gas flow rate is at least 4,000 sccm.

### Claim 24 (depends on 23)

A method of manufacturing a semiconductor device as claimed in claim 23, wherein the fluidal insulating layer is formed to a thickness of about 8,000-10,000 Å within fifteen seconds.

### Claim 25 (depends on 15)

A method of manufacturing a semiconductor device as claimed in claim 15, wherein the pattern having the window is formed by etching the fluidal insulating layer by utilizing an etching gas including CFx.

### Claim 26 (depends on 15)

A method of manufacturing a semiconductor device as claimed in claim 15, wherein before forming the fluidal insulating layer, further comprising forming an undoped fluidal insulating layer the substrate, and wherein for the forming of the undoped fluidal insulating layer, the ratio of the oxidizing gas flow rate, the first carrier gas flow rate, the second carrier gas flow rate, and the silicon source flow rate is about 2.00-2.50:0.70-0.95:1:0.15-0.25.

### Claim 27 (depends on 26)

A method of manufacturing a semiconductor device as claimed in claim 26, wherein a flow rate of the second carrier gas is at least 4,000 sccm.

### Claim 28 (depends on 27)

A method of manufacturing a semiconductor device as claimed in claim 27, wherein the undoped fluidal insulating layer is formed to a thickness of about 30-50 Å within five seconds.