# US 6,730,615 B2 · High reflector tunable stress coating, such as for a MEMS mirror

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,615 B2
- Document ID: US6730615B2
- Status: Granted
- Kind: B2
- Application number: 10/079,614
- Filed: 2002-02-19
- Published: 2003-08-21
- Granted: 2004-05-04
- Earliest claimed: 2002-02-19
- Assignees: Intel Corporation
- Inventors: Michael Goldstein
- Web page: https://patentgrep.com/patent/US6730615B2

## CPC

- B81C 1/00666: {Treatments for controlling internal stress or strain in MEMS structures}
- G02B 5/0833: {comprising inorganic materials only}
- G02B 26/0833: {the reflecting element being a micromechanical device, e.g. a MEMS mirror, DMD (G02B26/0825 takes precedence; micromechanical devices in general B81B)}
- B81B 2201/042: Micromirrors, not used as optical switches
- B81C 2201/0167: by adding further layers of materials having complementary strains, i.e. compressive or tensile strain
- Y10S 438/954: Making oxide-nitride-oxide device
- B81C: PROCESSES OR APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OR TREATMENT OF MICROSTRUCTURAL DEVICES OR SYSTEMS (making microcapsules or microballoons B01J13/02; processes or apparatus specially adapted for the manufacture or treatment of piezoelectric, electrostrictive or magnetostrictive elements per se H10N30/01)
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- B81B: MICROSTRUCTURAL DEVICES OR SYSTEMS, e.g. MICROMECHANICAL DEVICES (piezoelectric, electrostrictive or magnetostrictive elements per se H10N30/00, H10N35/00)
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

An optical device having a high reflector tunable stress coating includes a micro-electromechanical system (MEMS) platform, a mirror disposed on the MEMS platform, and a multiple layer coating disposed on the mirror. The multiple layer coating includes a layer of silver (Ag), a layer of silicon dioxide (SiO2) deposited on the layer of Ag, a layer of intrinsic silicon (Si) deposited on the layer of SiO2, and a layer of silicon oxynitride (SiOxNy) deposited on the layer of Si. The concentration of nitrogen is increased and/or decreased to tune the stress (e.g., tensile, none, compressive).

## Claims

### Claim 1

A method, comprising:
forming a layer of silver (Ag) having a first physical thickness on a substrate;
forming a layer of silicon oxide (SiO2) having a second physical thickness on the layer of Ag;
forming a layer of silicon (Si) having a third physical thickness on the layer of SiO2; and
tuning a layer of silicon oxynitride (SiOxNy) on the layer of Si to a fourth physical thickness, a ratio of Ny within a range of interest, and an optical thickness of a percentage of a quarter of a wavelength of interest within a band of wavelengths of interest.

### Claim 2 (depends on 1)

The method of claim 1, wherein forming the layer of SiOxNy comprises sputter-depositing the layer of SiOxNy on the layer of Si.

### Claim 3 (depends on 1)

The method of claim 1, wherein forming the layer of Si comprises evaporating Si on the layer of SiO2.

### Claim 4 (depends on 1)

The method of claim 1, wherein the first physical thickness is approximately one hundred nanometers.

### Claim 5 (depends on 4)

The method of claim 4, wherein the second physical thickness is approximately two hundred seventy nanometers.

### Claim 6 (depends on 5)

The method of claim 5, wherein the third physical thickness is approximately fifty nanometers.

### Claim 7 (depends on 6)

The method of claim 6, wherein tuning the layer of SiOxNy on the layer of Si comprises tuning the layer of SiOxNy to a physical thickness within a range from approximately one hundred nanometers to one hundred ten nanometers, a ratio of Ny within a range from approximately sixty percent Ny to twenty percent Ny, and an optical thickness of approximately 0.44 quarter of the wavelength.

### Claim 8 (depends on 1)

The method of claim 1, wherein tuning the layer of SiOxNy on the layer of Si comprises tuning the layer of SiOxNy to an index of refraction and a reflectance greater than ninety-nine percent over the range of angles of incidence.

### Claim 9

A method, comprising:
forming a layer of gold (Au) having a first physical thickness on a substrate;
forming a layer of dielectric material having a second physical thickness on the layer of Au;
forming a layer of silicon (Si) having a third physical thickness on the layer of dielectric material; and
tuning a layer of silicon oxynitride (SiOxNy) on the layer of Si to a fourth physical thickness, a ratio of Ny within a range of interest, and an optical thickness of a percentage of a quarter of a wavelength of interest within a band of wavelengths of interest.

### Claim 10 (depends on 9)

The method of claim 9, wherein forming a layer of dielectric material having a second physical thickness on the layer of Au comprises forming a layer of silver dioxide (AgO2) having a second physical thickness on the layer of Au.

### Claim 11 (depends on 9)

The method of claim 9, wherein forming at least one of the layers of Au, dielectric material, Si, or SiOxNy comprises forming at least one of the layers of Au, dielectric material, Si, or SiOxNy by at least one of implantation, doping, evaporation, physical vapor deposition, ion assisted deposition, magnetron sputtering, electron beam sputtering, masking, or reactive ion etching.