# US 6,730,611 B2 · Nitride semiconductor growing process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,611 B2
- Document ID: US6730611B2
- Status: Granted
- Kind: B2
- Application number: 10/216,400
- Filed: 2002-08-12
- Published: 2003-02-27
- Granted: 2004-05-04
- Earliest claimed: 2001-08-13
- Assignees: Sony Corporation
- Inventors: Katsunori Yanashima; Hiroshi Nakajima
- Web page: https://patentgrep.com/patent/US6730611B2

## CPC

- C30B 29/40: AIIIBV compounds {wherein A is B, Al, Ga, In or Tl and B is N, P, As, Sb or Bi}
- C30B 25/02: Epitaxial-layer growth
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/2908: {Nitrides}
- H10P 14/2921: {being crystalline insulating materials}
- H10P 14/3416: {Nitrides}
- H10P 14/3442: {N-type}
- H10P 14/3602: {In-situ cleaning}
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A process of growing a nitride semiconductor on a crystalline nitride semiconductor substrate is disclosed, which is carried out by heating the substrate and initiating supply of source gases onto a surface of the substrate before the substrate temperature exceeds 1200° C., to initiate growth of the nitride semiconductor on the substrate. The nitride semiconductor growth is initiated after the substrate temperature has reached 300° C., and also after supply of a nitrogen source gas has been initiated and before the substrate temperature exceeds 1200° C.

## Claims

### Claim 1

A process of growing a nitride semiconductor on a crystalline nitride semiconductor substrate, comprising the steps of:
starting a supply of a nitrogen source gas from among source gases onto a surface of said substrate before or after heating said substrate,
starting growth of said nitride semiconductor on said substrate by starting a supply of a second source gas from among said source gases that differs from said nitrogen source gas before the temperature of said substrate exceeds 1200° C., said second source gas being supplied onto the surface of said substrate while heating said substrate is being heated.

### Claim 2 (depends on 1)

A process according to claim 1, wherein said second source gas is supplied after the temperature of said substrate has reached 300° C.

### Claim 3 (depends on 2)

A process according to claim 2, wherein said nitride semiconductor comprises AlxGa1-xN(0≦x≦1).

### Claim 4 (depends on 1)

A process according to claim 1, wherein said second source gas from among said source gases comprises a group III source gas.

### Claim 5 (depends on 4)

A process according to claim 4, wherein said nitride semiconductor comprises AlxGa1-xN(0≦x≦1).

### Claim 6 (depends on 1)

A process according to claim 1, wherein said substrate comprises gallium nitride.

### Claim 7

A process of growing a nitride semiconductor on a crystalline nitride semiconductor substrate, comprising the steps of:
starting a supply of a nitrogen source gas from among source gases onto a surface of said substrate before or after heating said substrate,
submitting said surface of said substrate to thermal cleaning by heating said substrate to a temperature not exceeding 1200° C., starting growth of said nitride semiconductor on said substrate after said thermal cleaning by starting a supply of a second source gas from among said source gases that differs from said nitrogen source gas before the temperature of said substrate exceeds 1200° C., said second source gas being supplied onto the surface of said substrate while said substrate is being heated.

### Claim 8 (depends on 7)

A process according to claim 7, wherein said thermal cleaning is performed while said substrate is held at a prescribed temperature range not exceeding 1200° C.

### Claim 9 (depends on 8)

A process according to claim 8, wherein said nitride semiconductor comprises AlxGa1-xN(0≦x≦1).

### Claim 10 (depends on 7)

A process according to claim 7, wherein said thermal cleaning is performed while nitrogen source gas is continuously supplied onto said surface of said substrate.

### Claim 11 (depends on 7)

A process according to claim 7, wherein said second source gas from among said source gases comprises a group III source gas.

### Claim 12 (depends on 11)

A process according to claim 11, wherein said nitride semiconductor comprises AlxGa1-xN(0≦x≦1).

### Claim 13 (depends on 7)

A process according to claim 7, wherein said substrate comprises gallium nitride.