# US 6,730,602 B2 · Method for forming aluminum bumps by sputtering and chemical mechanical polishing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,602 B2
- Document ID: US6730602B2
- Status: Granted
- Kind: B2
- Application number: 09/822,532
- Filed: 2001-03-30
- Published: 2002-10-03
- Granted: 2004-05-04
- Earliest claimed: 2001-03-30
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Cheng-Wei Lee
- Web page: https://patentgrep.com/patent/US6730602B2

## CPC

- H10W 72/20: Bump connectors, e.g. solder bumps or copper pillars; Dummy bumps; Thermal bumps
- H10W 72/012: {of bump connectors, dummy bumps or thermal bumps}
- H10W 72/01255: {by using masks}
- H10W 72/07251: {characterised by changes in properties of the bump connectors during connecting}
- H10W 72/251: {Materials}
- H10W 72/252: {comprising solid metals or solid metalloids, e.g. PbSn, Ag or Cu}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method for forming aluminum bumps by first sputter aluminum and then chemical mechanical polishing to remove excess aluminum is disclosed. In the method, a pre-processed electronic substrate which has a plurality of I/O pads formed on top is first provided. An insulating material layer such as SiO2, Si3N4, SOG or polyimide is then deposited on the pads to a thickness that is essentially the thickness of the aluminum bumps to be formed. A plurality of openings with one on each of the plurality of I/O pads is then photolithographically formed, followed by a sputtering deposition to fill the plurality of openings with a metal that includes aluminum. A chemical mechanical polishing technique is then used to remove the excess aluminum so that a top surface of the aluminum bump is flush with the top surface of the insulating material layer, followed by the final step of removing at least partially a thickness of the insulating material layer by a wet etch process.

## Claims

### Claim 1

A method for forming aluminum bumps by sputtering and chemical mechanical polishing comprising the steps of:
providing a pre-processed electronic substrate with a plurality of input/output (I/O) pads formed on a top surface;
depositing an insulating material layer on top of said plurality of I/O pads to a thickness that is substantially the thickness of Al bumps to be formed;
photolithographically forming a plurality of openings with one on each of said plurality of I/O pads;
sputter depositing a metal comprising Al filling said plurality of openings and covering a top surface of said insulating material layer;
chemical mechanical polishing said electronic substrate until a plurality of Al bumps is formed with a top surface of the bump flush with said top surface of the insulating material layer; and
removing at least partially a thickness of said insulating material layer by a wet etch process.

### Claim 2 (depends on 1)

A method for forming aluminum bumps by sputtering and chemical mechanical polishing according to claim 1 further comprising the step of forming said plurality of I/O pads in a metal comprising Al.

### Claim 3 (depends on 1)

A method for forming aluminum bumps by sputtering and chemical mechanical polishing according to claim 1 further comprising the step of depositing said insulating material layer of a thickness of at least 5 μm.

### Claim 4 (depends on 1)

A method for forming aluminum bumps by sputtering and chemical mechanical polishing according to claim 1 further comprising the step of depositing said insulating material layer of a material selected from the group consisting of silicon oxide, spin-on-glass and polyimide.

### Claim 5 (depends on 1)

A method for forming aluminum bumps by sputtering and chemical mechanical polishing according to claim 1 further comprising the step of depositing said insulating material layer by at least two layers of different materials.

### Claim 6 (depends on 1)

A method for forming aluminum bumps by sputtering and chemical mechanical polishing according to claim 1 further comprising the step of depositing said insulating material layer by a first layer of Si3N4 or SiO2 and a second layer of polyimide on top of said first layer.

### Claim 7 (depends on 1)

A method for forming aluminum bumps by sputtering and chemical mechanical polishing according to claim 1 further comprising the step of depositing said insulating material layer by at least two layers of different materials to a total thickness of at least 5 μm.

### Claim 8 (depends on 1)

A method for forming aluminum bumps by sputtering and chemical mechanical polishing according to claim 1 further comprising the step of depositing said insulating material layer by at least two layers of different materials to a total thickness between about 5 μm and about 10 μm.

### Claim 9 (depends on 1)

A method for forming aluminum bumps by sputtering and chemical mechanical polishing according to claim 1 further comprising the step of sputter depositing a metal that consists of Al and Cu.

### Claim 10 (depends on 1)

A method for forming aluminum bumps by sputtering and chemical mechanical polishing according to claim 1 further comprising the step of sputter depositing a metal that consists of Al and less than 3 wt. % Cu.

### Claim 11 (depends on 1)

A method for forming aluminum bumps by sputtering and chemical mechanical polishing according to claim 1 further comprising the step of conducting said wet etch process incorporating buffered oxide etch (BOE).

### Claim 12

A method for forming aluminum bumps on a semiconductor structure comprising the steps of:
providing a pre-proceased semiconductor structure with a plurality of I/O pads on top;
printing a layer of polyimide-containing material having a thickness of at least 5 μm on top of said structure;
forming a plurality of openings on each of said plurality of I/O pads exposed;
filling said plurality of openings with a metal comprising Al;
removing excess metal from areas other than said plurality of openings; and
removing at least partially said layer of polyimide-containing material by a wet etch process.

### Claim 13 (depends on 12)

A method for forming aluminum bumps on a semiconductor structure according to claim 12 further comprising the step of forming said plurality of I/O pads in a metal comprising Al.

### Claim 14 (depends on 12)

A method for forming aluminum bumps on a semiconductor structure according to claim 12 further comprising the step of printing said layer of polyimide-containing material by a screen printing or stencil printing technique.

### Claim 15 (depends on 12)

A method for forming aluminum bumps on a semiconductor structure according to claim 12 further comprising the step of printing said layer of polyimide-containing material to a thickness between about 5 μm and about 10 μm.

### Claim 16 (depends on 12)

A method for forming aluminum bumps on a semiconductor structure according to claim 12 further comprising the step of filling said plurality of openings with a metal comprising Al and Cu.

### Claim 17 (depends on 12)

A method for forming aluminum bumps on a semiconductor structure according to claim 12 further comprising the step of removing excess metal until a surface of said metal in the plurality of openings is flush with a top surface of said layer of polyimide-containing material.

### Claim 18 (depends on 12)

A method for forming aluminum bumps on a semiconductor structure according to claim 12 further comprising the step of removing at least partially said layer of polyimide-containing material by an etchant comprising HE and NH4F.

### Claim 19 (depends on 12)

A method for forming aluminum bumps on a semiconductor structure according to claim 12 further comprising the step of removing at least ½ of a total thickness of said layer of polyimide-containing material to facilitate bonding to said Al bumps formed in said plurality of openings.

### Claim 20 (depends on 12)

A method for forming aluminum bumps on a semiconductor structure according to claim 12 further comprising the step of removing completely said layer of polyimide-containing material to facilitate bonding to said Al bumps formed in said plurality of openings.