# US 6,730,600 B2 · Method of dry etching a semiconductor device in the absence of a plasma

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,600 B2
- Document ID: US6730600B2
- Status: Granted
- Kind: B2
- Application number: 10/259,256
- Filed: 2002-09-27
- Published: 2004-04-01
- Granted: 2004-05-04
- Earliest claimed: 2002-09-27
- Assignees: Agere Systems Inc.
- Inventors: Nace Layadi; Simon John Molloy; Sailesh Mansinh Merchant; Isik C. Kizilyalli
- Web page: https://patentgrep.com/patent/US6730600B2

## CPC

- H10P 50/266: {by vapour etching only}
- C23F 1/12: Gaseous compositions
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23F: NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE (working metal by laser beams B23K26/00; desurfacing by applying flames B23K7/00; working of metal by electro-erosion B23H; producing decorative effects by removing surface material, e.g. by engraving, by etching, B44C1/22; electrolytic etching or polishing C25F); INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25

## Abstract

A method for dry etching a material deposited on semiconductor device is performed by chemically reacting the material with an etchant gas. The etching process is conducted in a reaction chamber at a predetermined temperature and predetermined pressure within the reaction chamber and without the need of generating a plasma within the chamber or applying an electrical bias to the semiconductor device. A sufficient amount of gas is introduced into the reaction chamber to selectively remove the material from the semiconductor device.

## Claims

### Claim 1

A method for dry etching a material layer deposited on a semiconductor device, the layer having a known thickness, the method comprising:
a. positioning the semiconductor device in an etch reaction chamber;
b. exposing the material layer to at least one etchant gas that is chemically reactive with the material of the layer, at a predetermined temperature and predetermined pressure within the reaction chamber, without generating a plasma in the reaction chamber and without providing an electrical bias to the semiconductor device, to remove at least a portion of the material layer from said semiconductor device;
c. selecting the material layer from the group of compounds including a refractory metal and a refractory metal alloy and wherein the etchant gas comprises a halogen-based etchant gas; and
d. selecting a halogen-based etchant gas from a group of compounds comprising hydrogen bromide, methane bromide, dibromomethane and bromoform.

### Claim 2 (depends on 1)

The method of claim 1 wherein the step of exposing the material to the etchant gas comprises injecting the etchant gas into the chamber at a predetermined flow rate and for a predetermined timed duration.

### Claim 3 (depends on 1)

The method of claim 1 further comprising venting of gaseous by-products, resulting from a chemical reaction between said refractory metal and said etchant, from the reaction chamber.

### Claim 4 (depends on 1)

The method of claim 1 wherein the step of exposing the material layer to the etchant gas comprises etching at least a portion of the material layer to a predetermined thickness.

### Claim 5 (depends on 1)

The method of claim 1 wherein the etchant gas has a known etch rate with respect to the material of the layer, and further comprising estimating a predetermined timed duration to which the material layer is exposed to the etchant gas in order to etch said material layer to a desired, substantially uniform thickness.

### Claim 6 (depends on 1)

The method of claim 1 further comprising adjusting the temperature within the reaction chamber to between about 300° C. to about 500° C., before introducing the etchant gas into the reaction chamber.

### Claim 7 (depends on 1)

The method of claim 1 further comprising adjusting the pressure within the reaction chamber to between about 100 Torr to about 200 Torr before introducing the etchant gas into the reaction chamber.

### Claim 8

A method for fabricating a semiconductor device on a wafer substrate, comprising the steps of:
a. depositing a material layer to a predetermined thickness over said wafer substrate;
b. forming a mask layer for transferring a patterned feature to a material layer subjacent the mask layer, and said material forming at least one film within the mask layer;
c. positioning the substrate within a reaction chamber; and,
d. introducing an etchant gas into the reaction chamber at a predetermined temperature and predetermined pressure within the reaction chamber to etch at least a portion of the material layer from the substrate without generating a plasma within the chamber and without applying an electrical bias to said wafer substrate.

### Claim 9 (depends on 8)

The method of claim 8 further comprising patterning a feature on a material layer of the semiconductor device, and etching a topographical feature corresponding to the patterned feature wherein the topographical feature has a substantially vertical dimension intersecting a lateral dimension forming a step therein, and the material layer having been deposited along said vertical and lateral dimensions, and said etchant gas removing at least a portion of the material layer along the vertical and lateral dimensions at substantially the same etch rate.

### Claim 10 (depends on 8)

The method of claim 8 wherein said step of depositing the material comprises the blanket deposition of the material layer over the substrate and further comprising the step of patterning a feature on the device to be etched into the material layer and said step of introducing the etchant gas comprises the step of selectively removing at least a portion of the material layer to a predetermined thickness and corresponding to the patterned feature.

### Claim 11

A method for dry etching a refractory metal film formed over a wafer substrate of a semiconductor device, and said refractory metal film having a known thickness, comprising the steps of:
a. positioning the wafer substrate within a reaction chamber;
b. isotropically etching at least a portion of the refractory metal film to a predetermined thickness by introducing at least one halogen-based etchant gas into the reaction chamber at a predetermined temperature and predetermined pressure within the reaction chamber, without generating a plasma within the chamber or applying an electrical bias to the wafer substrate; and;
c. selecting the halogen-based etchant gas from a group of compounds comprising hydrogen bromide, methane bromide, dibromomethane and bromoform.

### Claim 12 (depends on 11)

The method of claim 11 comprising adjusting the temperature to said predetermined temperature within the reaction chamber from about 300° C. to about 500° C., before introducing the etchant gas into the reaction chamber.

### Claim 13 (depends on 11)

The method of claim 11 further comprising adjusting the pressure within the reaction chamber to said predetermined pressure from about 100 Torr to about 200 Torr, before introducing the etchant gas into the reaction chamber.

### Claim 14

A method for dry etching a refractory metal film formed over a wafer substrate of a semiconductor device, and said refractory metal film having a known thickness, comprising the steps of:
a. positioning the wafer substrate within a reaction chamber; and,
b. isotropically etching at least a portion of the refractory metal film to a predetermined thickness by introducing at least one gaseous compound having at least one brominated methyl group into the reaction chamber at a predetermined temperature and predetermined pressure within the reaction chamber, without generating a plasma within the chamber or applying an electrical bias to the wafer substrate.

### Claim 15 (depends on 14)

The method of claim 14 further comprising the step of selecting the gaseous compound from a group of compounds comprising hydrogen bromide, methane bromide, dibromomethane and bromoform.