# US 6,730,595 B2 · Protecting method for semiconductor wafer and surface protecting adhesive film for semiconductor wafer used in said method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,595 B2
- Document ID: US6730595B2
- Status: Granted
- Kind: B2
- Application number: 10/003,227
- Filed: 2001-12-06
- Published: 2002-08-08
- Granted: 2004-05-04
- Earliest claimed: 2000-12-12
- Assignees: Mitsui Chemicals, Inc.
- Inventors: Yoshihisa Saimoto; Yasuhisa Fujii; Makoto Kataoka; Kentaro Hirai; Hideki Fukumoto; Takanobu Koshimizu
- Web page: https://patentgrep.com/patent/US6730595B2

## CPC

- H10P 72/74: {using temporarily an auxiliary support}
- C09J 7/22: Plastics; Metallised plastics
- C09J 7/38: Pressure-sensitive adhesives [PSA]
- H10P 72/7402: {Wafer tapes, e.g. grinding or dicing support tapes}
- C09J 2203/326: for bonding electronic components such as wafers, chips or semiconductors
- H10P 72/7416: {used during dicing or grinding}
- H10P 72/7422: {used to protect an active side of a device or wafer}
- H10W 72/01331: {using blanket deposition}
- H10W 72/073: {of die-attach connectors}
- H10W 72/07337: {using a polymer adhesive, e.g. an adhesive based on silicone or epoxy}
- H10W 72/354: {comprising polymers}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

This invention aims to provide a protecting method for a semiconductor wafer which can prevent breakage of a semiconductor wafer even when a semiconductor wafer is thinned to a thickness of 200 μm or less, and a surface protecting adhesive film for a semiconductor wafer used in the protecting method. According to this invention, there is provided a protecting method for a semiconductor wafer comprising a first step of adhering a surface protecting adhesive film for a semiconductor wafer to a circuit-formed surface of the semiconductor wafer, a second step of processing a non-circuit-formed surface of the semiconductor wafer and a third step of adhering a bonding film for die bonding to the non-circuit-formed surface of the semiconductor wafer, characterized in that the third step is performed without peeling the surface protecting adhesive film for the semiconductor wafer, and an adhesive film in which an adhesive layer is formed on one surface of a substrate film at least one layer of which is made of a resin having a melting point of 200° C. or more is used, and a surface protecting adhesive film for a semiconductor wafer used in the protecting method.

## Claims

### Claim 1

A protecting method for a semiconductor wafer in a step of thinning the semiconductor wafer comprising a first step of adhering a surface protecting adhesive film for a semiconductor wafer to a circuit-formed surface of the semiconductor wafer, a second step of processing a non-circuit-formed surface of the semiconductor wafer to reduce the thickness of the wafer, and a third step of adhering a bonding film for die bonding to the non-circuit-formed surface of the semiconductor wafer, characterized in that the third step is performed without peeling the surface protecting adhesive film from the semiconductor wafer, and a surface protecting adhesive film for a semiconductor wafer in which an adhesive layer having a storage elastic modulus at 150° C. of at least 1×105 Pa, an adhesion of 5 to 500 g/25 mm and a thickness of 3 to 100 μm is formed on one surface of a substrate film at least one layer of which is made of a resin having a melting point of 200° C. or more.

### Claim 2 (depends on 1)

The protecting method for the semiconductor wafer according to claim 1 wherein the second step includes at least one step selected from the group consisting of a back grinding step, a wet etching step and a polishing step.

### Claim 3 (depends on 1)

The protecting method for the semiconductor wafer according to claim 1, wherein the thickness of the semiconductor wafer after the second step is 200 μm or less.

### Claim 4 (depends on 1)

The protecting method for the semiconductor wafer according to claim 1, wherein the resin having the melting point of 200° C. or more is at least one resin selected from the group consisting of a polyester, a polyimide, a polyether ether ketone and a polyether sulfone.

### Claim 5 (depends on 1)

The protecting method for the semiconductor wafer according to claim 1, wherein the thickness of the substrate film layer made of the resin having the melting point of 200° C. or more is 10 to 300 μm.