# US 6,730,588 B1 · Method of forming SiGe gate electrode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,588 B1
- Document ID: US6730588B1
- Status: Granted
- Kind: B1
- Application number: 10/026,407
- Filed: 2001-12-20
- Granted: 2004-05-04
- Earliest claimed: 2001-12-20
- Assignees: LSI Logic Corporation
- Inventors: Richard Schinella
- Web page: https://patentgrep.com/patent/US6730588B1

## CPC

- H10D 64/01314: {the conductor comprising a layer of Ge, C or of compounds of Si, Ge or C contacting the insulator}
- H10P 14/416: {of highly doped semiconductor materials, e.g. polysilicon layers or amorphous silicon layers}
- Y10S 438/933: Germanium or silicon or Ge-Si on III-V
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

The present invention provides a method of forming SiGe gate electrodes using a thin nucleation layer. A dielectric layer is formed on a semiconductor wafer and a thin silicon nucleation layer deposited on top of the dielectric layer. A SiGe conducting film is deposited on the patterned silicon layer. The ratio of germanium to silicon in the gaseous source mixture for the silicon and germanium layer is selected so that the SiGe conducting film deposits on the nucleation layer but fails to deposit on the dielectric.

## Claims

### Claim 1

A method of forming a gate electrode on a semiconductor device, the method comprising:
forming a dielectric layer on a semiconductor wafer;
depositing a thin silicon layer having a thickness in the range of 100 to 500 Angstroms on the dielectric layer;
patterning and etching the thin silicon layer to form a silicon nucleation layer and to expose portions of the dielectric layer;
forming a self-aligned gate electrode by depositing a silicon germanium conducting film on the silicon nucleation layer using a material which selectively deposits on the nucleation layer and which fails to deposit on the exposed portions of the dielectric layer; and
depositing a metal layer on the deposited silicon germanium conducting film.

### Claim 2 (depends on 1)

The method recited in claim 1 wherein the metal layer is one of titanium and cobalt.

### Claim 3 (depends on 1)

The method recited in claim 1 further comprising annealing the metal layer to form a germanide silicide contact.

### Claim 4 (depends on 1)

The method recited in claim 1 wherein the silicon layer comprises at least one of amorphous silicon and polycrystalline silicon.

### Claim 5 (depends on 1)

The method recited in claim 1 wherein the dielectric layer comprises silicon dioxide (SiO2).

### Claim 6 (depends on 1)

The method recited in claim 1 wherein the silicon germanium conducting film is deposited at a temperature in the range from about 300 to 800 degrees C.

### Claim 7 (depends on 1)

The method recited in claim 1 wherein the metal layer is formed in situ during the formation of the silicon germanium film.

### Claim 8 (depends on 1)

The method recited in claim 1 wherein the silicon germanium conducting film is deposited using a gaseous mixture comprising germane and at least one of silane (SiH4) and dichlorosilane (SiH2Cl2).

### Claim 9 (depends on 1)

The method recited in claim 1 wherein the patterning and etching of the silicon layer comprises depositing a photoresist layer on the silicon layer.

### Claim 10 (depends on 8)

The method recited in claim 8 wherein the proportions of germane and at least one of silane and dichlorosilane (SiH2Cl2) are selected to preclude deposition of SiGe on the dielectric layer.

### Claim 11 (depends on 8)

The method recited in claim 8 wherein the selective depositing of the silicon germanium conducting film is performed by adjusting the ratio of germane to dichlorosilane (SiH2Cl2) in the gaseous mixture to about 1:5.

### Claim 12 (depends on 8)

The method recited in claim 8 wherein the ratio of germane to dichlorosilane (SiH2Cl2) is in the range from about 0.025 to 1.00.

### Claim 13 (depends on 9)

The method recited in claim 9 wherein the photoresist layer ranges from about 100 Angstroms to 2000 Angstroms in thickness.

### Claim 14 (depends on 8)

The method recited in claim 8 wherein the gaseous mixture further comprises dopants for doping the silicon germanium conducting film.

### Claim 15 (depends on 14)

The method recited in claim 14 wherein the dopants are maintained at a constant concentration during the deposition of the silicon germanium conducting film.

### Claim 16 (depends on 14)

The method recited in claim 14 wherein the dopant concentration is changed during the deposition of the silicon germanium conducting film to provide a doping gradient in the silicon germanium conducting film.

### Claim 17

A method of forming a gate electrode on a semiconductor device, the method comprising:
forming a dielectric layer on a semiconductor wafer;
depositing a silicon layer having a thickness in the range of 100 to 500 Angstroms on the dielectric layer;
patterning and etching the silicon layer to form a gate electrode nucleation layer; and
forming a gate electrode by depositing a silicon germanium conducting film on the gate electrode nucleation layer using a material which selectively deposits on the nucleation layer and which fails to deposit on the dielectric layer.

### Claim 18

A method of forming a gate electrode on a semiconductor device, the method comprising:
forming a dielectric layer on a semiconductor wafer;
depositing a silicon layer on the dielectric layer;
patterning and etching the silicon layer to form a gate electrode nucleation layer; and
forming a gate electrode by depositing a silicon germanium conducting film on the gate electrode nucleation layer using a gaseous mixture comprising germane and at least one of silane (SiH4) and dichlorosilane (SiH2Cl2) which selectively deposits on the nucleation layer and which fails to deposit on the dielectric layer,
wherein the gaseous mixture further comprises dopants for doping the silicon layer and the dopant concentration is changed during the deposition of the silicon germanium conducting film to provide a doping gradient in the silicon germanium conducting film.