# US 6,730,587 B1 · Titanium barrier for nickel silicidation of a gate electrode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,587 B1
- Document ID: US6730587B1
- Status: Granted
- Kind: B1
- Application number: 09/731,006
- Filed: 2000-12-07
- Granted: 2004-05-04
- Earliest claimed: 2000-12-07
- Assignees: Advanced Micro Devices, Inc.
- Inventors: Jacques J. Bertrand; Christy Mei-Chu Woo; Minh Van Ngo; George Kluth
- Web page: https://patentgrep.com/patent/US6730587B1

## CPC

- H10D 64/664: {the additional layers comprising a barrier layer between the layer of silicon and an upper metal or metal silicide layer}
- H10D 64/0131: {the additional conductive layer comprising a silicide layer formed by the silicidation reaction between the layer of silicon with a metal layer which is not formed by metal implantation}
- H10D 30/0212: {using self-aligned silicidation}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

Nickel silicidation of a gate electrode is controlled using a titanium barrier layer. Embodiments include forming a gate electrode structure comprising a lower polycrystalline silicon layer, a layer of titanium thereon and an upper polycrystalline silicon layer on the titanium layer, depositing a layer of nickel and silicidizing, whereby the upper polycrystalline silicon layer is converted to nickel silicide and a titanium silicide barrier layer is formed preventing nickel from reacting with the lower polycrystalline silicon layer.

## Claims

### Claim 1

A method of manufacturing a semiconductor device, the method comprising:
forming a gate insulating layer on a silicon (Si)-containing semiconductor substrate;
depositing a first layer of Si on the gate insulating layer;
depositing a layer of titanium (Ti) on the first Si layer;
depositing a second Si layer on the Ti layer;
patterning the second Si layer, Ti layer, first Si layer and gate insulating layer to form a transistor gate electrode structure having an upper surface and opposing side surfaces;
forming a silicon nitride sidewall spacer on the side surfaces of the gate electrode structure leaving exposed adjacent surfaces of the substrate;
depositing a layer of nickel on the upper surface of the gate electrode structure, sidewall spacers and exposed surfaces of the substrate; and
heating to react the nickel layer on the upper surface of the gate electrode structure with the second Si layer to form a layer of nickel silicide, to react the nickel layer with Si in the substrate to form nickel silicide layers on the exposed surfaces of the substrate, wherein a layer of titanium silicide is formed preventing nickel silicidation of the first Si layer.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the first and second Si layers comprise polycrystalline silicon.

### Claim 3 (depends on 1)

The method according to claim 1, comprising forming source/drain regions in the substrate proximate the opposing side surfaces of the gate electrode structure, wherein the nickel silicide layers on the exposed substrate surfaces function as source/drain contacts.

### Claim 4 (depends on 1)

The method according to claim 1, comprising forming an oxide liner on the side surfaces of the gate electrode structure before forming the silicon nitride sidewall spacers.

### Claim 5 (depends on 1)

The method according to claim 1, comprising heating at a temperature of about 400° C. to about 600° C. to form the nickel silicide layers.

### Claim 6 (depends on 1)

The method according to claim 1, comprising depositing the nickel layer at a thickness of about 150 Å to about 500 Å.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the gate electrode structure comprises a gate electrode having a height of about 1,000 Å, to about 3,000 Å on a gate insulating layer.

### Claim 8 (depends on 7)

The method according to claim 7, comprising heating to react the nickel layer with the second Si layer to form the nickel silicide layer having a thickness of about ½ to about ⅔ of the height of the gate electrode.

### Claim 9 (depends on 8)

The method according to claim 8, comprising depositing the titanium layer at a thickness of about 10 Å to about 50 Å.

### Claim 10 (depends on 4)

The method according to claim 4, comprising forming the oxide liner at a thickness of about 130 Å to about 170 Å, and forming the silicon nitride sidewall spacers at a thickness of about 850 Å to about 950 Å.

### Claim 11 (depends on 1)

The method according to claim 1, comprising removing unreacted nickel from the silicon nitride sidewall spacers after heating.