# US 6,730,584 B2 · Methods for forming wordlines, transistor gates, and conductive interconnects, and wordline, transistor gate, and conductive interconnect structures

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,584 B2
- Document ID: US6730584B2
- Status: Granted
- Kind: B2
- Application number: 09/333,770
- Filed: 1999-06-15
- Published: 2002-07-04
- Granted: 2004-05-04
- Earliest claimed: 1999-06-15
- Assignees: Micron Technology, Inc.
- Inventors: Klaus Florian Schuegraf; Carl Powell; Randhir P. S. Thakur
- Web page: https://patentgrep.com/patent/US6730584B2

## CPC

- H10D 64/664: {the additional layers comprising a barrier layer between the layer of silicon and an upper metal or metal silicide layer}
- H10D 64/01312: {the additional layer comprising a metal or metal silicide formed by deposition, i.e. without a silicidation reaction, e.g. sputter deposition}
- H10D 64/035: {comprising conductor-insulator-conductor-insulator-semiconductor structures}
- H10D 64/661: {the conductor comprising a layer of silicon contacting the insulator, e.g. polysilicon having vertical doping variation (having lateral variation in the gate structure H10D64/671)}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

The invention encompasses stacked semiconductor devices including gate stacks, wordlines, PROMs, conductive interconnecting lines, and methods for forming such structures. The invention also includes a method of forming a transistor gate comprising: a) forming gate dielectric layer; b) forming a polysilicon gate layer against the gate dielectric layer; and c) doping the polysilicon gate layer with a conductivity-enhancing dopant, the dopant being provided in a concentration gradient within the polysilicon layer, the concentration gradient increasing in a direction toward the gate dielectric layer. The invention also includes a wordline comprising: a) a polysilicon line; a substantially fluorine impervious barrier layer over the polysilicon line; and a b) layer of metal-silicide over the substantially fluorine impervious barrier layer.

## Claims

### Claim 1

A method of forming a transistor gate comprising the following steps:
forming gate dielectric layer;
forming a polysilicon gate layer against the gate dielectric layer;
doping the polysilicon gate layer with a conductivity-enhancing dopant, the dopant being provided in a concentration gradient within the polysilicon layer, the concentration gradient comprising more than two concentrations of dopant and increasing in a direction toward the gate dielectric layer, the dopant concentration being highest adjacent the gate dielectric layer;
forming a substantially fluorine impervious barrier layer over the polysilicon gate layer; and forming a metal silicide layer over the substantially fluorine impervious barrier layer.

### Claim 2 (depends on 1)

The method of claim 1 wherein the gate dielectric layer is elevationally beneath the polysilicon gate layer and wherein the concentration gradient decreases with increasing elevation within the polysilicon gate layer.

### Claim 3 (depends on 1)

The method of claim 1 wherein the gate dielectric layer comprises silicon dioxide.

### Claim 4 (depends on 1)

The method of claim 1 wherein the step of doping the polysilicon layer comprises ion implanting a dopant into the layer.

### Claim 5 (depends on 1)

The method of claim 1 wherein the step of doping the polysilicon layer comprises providing a dopant within the layer and diffusing the dopant to form the concentration gradient.

### Claim 6

A method of forming a transistor gate comprising:
forming polysilicon gate layer;
forming a substantially fluorine impervious barrier layer adjacent the polysilicon gate layer;
forming a metal-silicide layer adjacent the substantially fluorine impervious barrier layer; and
doping the polysilicon gate layer with a conductivity-enhancing dopant, the dopant being provided in a concentration gradient within the polysilicon layer, the concentration gradient comprising more than two concentrations of dopant and increasing in a direction away from the metal-silicide layer, the dopant concentration being highest at an elevation within the polysilicon gate layer farthest from the metal-silicide layer.

### Claim 7

A method of forming a transistor gate comprising:
forming a gate layer of polysilicon;
providing a gradient of conductivity-enhancing impurity within the gate layer of polysilicon;
forming a substantially fluorine impervious barrier layer over the gate layer, wherein the substantially fluorine impervious barrier layer comprises a thickness of less than or equal to 20 Angstroms; and
forming a layer of metal-silicide over the substantially fluorine impervious barrier layer, the forming the layer of metal-silicide comprising depositing a metal from a fluorine containing reactant.

### Claim 8 (depends on 7)

The method of claim 7 wherein the substantially fluorine impervious barrier layer comprises TiN.

### Claim 9 (depends on 7)

The method of claim 7 wherein the substantially fluorine impervious barrier layer is a dielectric layer having a thickness of about 20 Angstroms.

### Claim 10 (depends on 7)

The method of claim 7 wherein the substantially fluorine impervious barrier layer comprises nitrogen.

### Claim 11 (depends on 7)

The method of claim 7 wherein the substantially fluorine impervious barrier layer comprises nitrogen provided at an interface between the polysilicon gate layer and the metal-silicide layer.

### Claim 12 (depends on 7)

The method of claim 7 wherein the step of forming the substantially fluorine impervious barrier layer comprises chemical vapor depositing a barrier layer material.

### Claim 13 (depends on 7)

The method of claim 7 wherein the step of forming the substantially fluorine impervious barrier layer comprises sputtering a barrier layer material.

### Claim 14 (depends on 7)

The method of claim 7 further comprising:
after forming the substantially fluorine impervious barrier layer, subjecting the gate layer to rapid thermal processing at a temperature of at least 850° C. for at least 10 seconds.

### Claim 15 (depends on 7)

The method of claim 7 further comprising:
after forming the substantially fluorine impervious barrier layer, subjecting the transistor gate to a temperature of at least 850° C. in an oxygen-comprising atmosphere to 1) activate the impurity; and 2) oxidize a corner of the polysilicon gate layer.

### Claim 16 (depends on 15)

The method of claim 15 wherein the oxygen comprising atmosphere comprises at least one compound selected from the group consisting of O2, O3, N2O, and NO.

### Claim 17 (depends on 7)

The method of claim 7 further comprising:
after forming the substantially fluorine impervious barrier layer, subjecting the transistor gate to a temperature of at least 850° C. in an oxygen-comprising atmosphere to 1) activate the impurity; and 2) form a layer of oxide over the metal-silicide layer.

### Claim 18

A method of forming a wordline comprising:
forming a polysilicon layer;
non-homogeneously doping the polysilicon layer with a conductivity enhancing impurity;
forming a substantially fluorine impervious barrier layer over the polysilicon layer, wherein the substantially fluorine impervious barrier layer comprises a thickness of less than or equal to 20 Angstroms;
forming a layer of metal-silicide over the substantially fluorine impervious barrier layer, the forming the layer of metal-silicide comprising depositing a metal from a fluorine containing reactant; and
providing the polysilicon layer, fluorine impervious barrier layer, and metal-silicide layer in the shape of a conductive line over a gate dielectric layer.

### Claim 19 (depends on 18)

The method of claim 18 wherein the substantially fluorine impervious barrier layer comprises TiN.

### Claim 20 (depends on 18)

The method of claim 18 wherein the substantially fluorine impervious barrier layer comprises a thickness of about 20 Angstroms.

### Claim 21 (depends on 18)

The method of claim 18 wherein the substantially fluorine impervious barrier layer comprises nitrogen.

### Claim 22 (depends on 18)

The method of claim 18 wherein the step of forming the substantially fluorine impervious barrier layer comprises chemical vapor depositing a barrier layer material.

### Claim 23 (depends on 18)

The method of claim 18 wherein the step of forming the substantially fluorine impervious barrier layer comprises sputtering a barrier layer material.

### Claim 24 (depends on 18)

The method of claim 18 further comprising:
after forming the substantially fluorine impervious barrier layer, subjecting the wordline to a temperature of at least 850° C. for at least 10 seconds.

### Claim 25

A method of forming a transistor gate comprising the following steps:
forming polysilicon layer over a substrate, the polysilicon layer comprising a gradient of conductivity-enhancing dopant concentration which is greatest proximate the substrate;
forming a substantially fluorine impervious barrier layer over the polysilicon gate layer; and
forming a metal silicide layer over the substantially fluorine impervious barrier layer.

### Claim 26 (depends on 25)

The method of claim 25 wherein the substantially fluorine impervious barrier layer comprises nitrogen.

### Claim 27 (depends on 25)

The method of claim 25 wherein the forming the substantially fluorine impervious barrier layer comprises sputtering a barrier layer material.

### Claim 28 (depends on 25)

The method of claim 25 wherein the forming the substantially fluorine impervious barrier layer comprises chemical vapor depositing a barrier layer material.

### Claim 29 (depends on 25)

The method of claim 25 wherein the substantially fluorine impervious barrier layer is a dielectric layer having a thickness of about 20 Angstroms.