- Number: US 6,730,583 B2
- Document ID: US6730583B2
- Status: Granted
- Kind: B2
- Application number: 09/984,030
- Filed: 2001-10-26
- Published: 2002-05-09
- Granted: 2004-05-04
- Earliest claimed: 2000-10-26
- Assignees: Hynix Semiconductor Inc.
- Inventors: Jae-Geun Oh; Byung-Seop Hong
- Web page: https://patentgrep.com/patent/US6730583B2

## CPC

- H10P 30/21: {of electrically active species}
- H10D 30/0227: {having both lightly-doped source and drain extensions and source and drain regions self-aligned to the sides of the gate, e.g. lightly-doped drain [LDD] MOSFET or double-diffused drain [DDD] MOSFET}
- H10P 30/204: {into Group IV semiconductors}
- H10P 30/225: {of a molecular ion, e.g. decaborane}
- H10P 30/28: characterised by an annealing step, e.g. for activation of dopants
- H10D 64/021: {using multiple gate spacer layers, e.g. bilayered sidewall spacers}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A source/drain formation method using multi-boron implantation instead of single-boron implantation is disclosed. The multi-boron implantation method includes a first step, in which boron-fluorine compounds are implanted for forming an amorphous layer in the source/drain region, and a second step, in which boron ions are implanted.

## Claims

### Claim 1

A method for fabricating a semiconductor memory device having a p-type source/drain, the method comprising the steps of:
forming a first amorphous layer in a p-type source/drain region by implanting first dopants including fluorine and boron;
implanting second dopants including boron in the first amorphous layer formed in the p-type source/drain region;
performing a plurality of subsequent processes accompanying a thermal treatment;
performing a first rapid thermal annealing process for activating the first dopants and the second dopants;
forming the p-type source/drain by performing a thermal treatment for activating the first dopants and the second dopants;
forming a contact hole that exposes the p-type source/drain region by selectively removing an insulating layer covering the P-type source/drain region;
forming a second amorphous layer in a second p-type source/drain region exposed under the contact hole by implanting third dopants including fluorine and boron;
implanting fourth dopants including boron in the second amorphous layer; and
performing a thermal treatment for activating the third dopants and the fourth dopants.

### Claim 2 (depends on 1)

The method as recited in claim 1, wherein the first dopants and the third dopants are selected from a group consisting BF2 and BF.

### Claim 3 (depends on 2)

The method as recited in claim 2, wherein the second dopants and the fourth dopants are selected from a group consisting BF and B.

### Claim 4 (depends on 1)

The method as recited in claim 1, wherein the first dopants are BF2 and the second dopants are B.

### Claim 5 (depends on 4)

The method as recited in claim 4, wherein a dosage of the first dopants is in a range of 1×1015#/cm3 to 2×1015#/cm3 and a dosage of the second dopants is in a range of 1×1015#/cm3 to 2×1015#/cm3 wherein “#” is defined as a number of dopants.

### Claim 6 (depends on 5)

The method as recited in claim 5, wherein the first dopants are implanted with an energy of 10 KeV to 30 KeV and the second dopants are implanted with an energy of 3 KeV to 4.5 KeV.

### Claim 7

A method for fabricating semiconductor memory device having a p-type source/drain, the method comprising:
forming an amorphous layer in a p-type source/drain region by implanting first dopants including fluorine and boron;
implanting second dopants including boron in the amorphous layer formed in the p-type source/drain region;
performing a plurality of subsequent processes accompanying a thermal treatment at a temperature in the range of 600° C. to 850° C.; and
performing a first rapid thermal annealing process (RTA) for activating the first dopants and the second dopants at a temperature in the range of 900° C. to 1100° C.

### Claim 8 (depends on 7)

The method as recited in claim 7, wherein the method further comprises after implanting second dopants, performing a second RTA process for forming a p-type source/drain by activating the first dopants and the second dopants.

### Claim 9 (depends on 7)

The method as recited in claim 7, wherein the first rapid thermal annealing is performed right after the thermal treatments accompanying the subsequent processes.

### Claim 10 (depends on 9)

The method as recited in claim 9, further including forming an interlayer insulating layer and wherein a thermal treatment for forming the interlayer insulating layer is one of the plurality of thermal treatments accompanying the subsequent processes.

### Claim 11 (depends on 7)

The method as recited in claim 7, wherein the first rapid thermal annealing process is performed in ambient N2 gas atmosphere for 5 seconds to 60 seconds.

### Claim 12 (depends on 11)

The method as recited in claim 11, wherein the flow rate of N2 gas is 1 slpm to 20 slpm.

### Claim 13 (depends on 12)

The method as recited in claim 12, wherein a ramping rate of the first rapid thermal treatment is 20° C./sec to 250° C./sec and wherein a cooling rate of the first rapid thermal treatment is 20° C./sec to 100° C./sec.

### Claim 14 (depends on 7)

The method as recited in claim 7, wherein one of the plurality of subsequent processes is a formation process for a polylsilicon plate electrode, and wherein the thermal treatment is for activating dopants in the polysilicon.