# US 6,730,576 B1 · Method of forming a thick strained silicon layer and semiconductor structures incorporating a thick strained silicon layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,576 B1
- Document ID: US6730576B1
- Status: Granted
- Kind: B1
- Application number: 10/335,447
- Filed: 2002-12-31
- Granted: 2004-05-04
- Earliest claimed: 2002-12-31
- Assignees: Advanced Micro Devices, Inc.
- Inventors: Haihong Wang; Paul R. Besser; Jung-Suk Goo; Minh V. Ngo; Eric N. Paton; Qi Xiang
- Web page: https://patentgrep.com/patent/US6730576B1

## CPC

- H10D 30/601: {having lightly-doped drain or source extensions, e.g. LDD IGFETs or DDD IGFETs (lightly doped source or drain extensions for TFTs H10D30/6715)}
- H10D 30/751: {having composition variations in the channel regions}
- H10D 30/798: {being provided in or under the channel regions}
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/271: {characterised by the preparation of substrate for selective deposition}
- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10P 14/3211: {Silicon, silicon germanium or germanium}
- H10P 14/3254: {Graded layers}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10D 30/0212: {using self-aligned silicidation}
- H10D 30/0227: {having both lightly-doped source and drain extensions and source and drain regions self-aligned to the sides of the gate, e.g. lightly-doped drain [LDD] MOSFET or double-diffused drain [DDD] MOSFET}
- H10D 64/021: {using multiple gate spacer layers, e.g. bilayered sidewall spacers}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A strained silicon layer is grown on a layer of silicon germanium and a layer of silicon germanium is grown on the strained silicon in a single continuous in situ deposition process with the strained silicon. Shallow trench isolations are formed in the lower layer of silicon germanium prior to formation of the strained silicon layer. The two silicon germanium layers effectively provide dual substrates at both surfaces of the strained silicon layer that serve to maintain the tensile strain of the strained silicon layer and resist the formation of misfit dislocations that might otherwise result from temperature changes during processing. Consequently the critical thickness of strained silicon that can be grown without significant misfit dislocations during later processing is effectively doubled for a given germanium content of the silicon germanium layers. The formation of shallow trench isolations prior to formation of the strained silicon layer avoids subjecting the strained silicon layer to extreme thermal stresses and further reduces the formation of misfit dislocations.

## Claims

### Claim 1

A method for forming a strained silicon layer, comprising:
providing a substrate comprising a first layer of silicon germanium;
forming a layer of strained silicon on the first layer of silicon germanium; and
forming a second layer of silicon germanium on the strained silicon layer in a single continuous in situ deposition process with the layer of strained silicon,
wherein the first and second silicon germanium layers support a tensile strain of the strained silicon layer and resist the formation of misfit dislocations in the strained silicon layer.

### Claim 2 (depends on 1)

The method claimed in claim 1, wherein the first silicon germanium layer has a composition Si1−xGex, where x is in the range of 0.1 to 0.4.

### Claim 3 (depends on 2)

The method claimed in claim 2, wherein x is approximately 0.3 and the thickness of the strained silicon layer exceeds 140 Angstroms.

### Claim 4 (depends on 1)

The method claimed in claim 1, wherein the first and second silicon germanium layers have an approximately equal germanium content at respective junctions with the strained silicon layer.

### Claim 5 (depends on 1)

The method claimed in claim 1, wherein the layer of strained silicon has a thickness in excess of a critical thickness determined in accordance with a germanium content of the first layer of silicon germanium.

### Claim 6

A method for forming a semiconductor device, comprising:
providing a substrate comprising a first layer of silicon germanium;
forming shallow trench isolations in the first layer of silicon germanium;
forming a layer of strained silicon on the first layer of silicon germanium; and
forming a second layer of silicon germanium on the strained silicon layer in a single continuous in situ deposition process with the layer of strained silicon,
wherein the first and second silicon germanium layers support a tensile strain of the strained silicon layer and resist the formation of misfit dislocations in the strained silicon layer.

### Claim 7 (depends on 6)

The method claimed in claim 6, wherein the layer of strained silicon has a thickness in excess of a critical thickness determined in accordance with a germanium content of the first layer of silicon germanium.

### Claim 8 (depends on 6)

The method claimed in claim 6, wherein the first silicon germanium layer and the second silicon germanium layer each have a composition Si1−xGex, where x is in the range of 0.1 to 0.4.

### Claim 9 (depends on 8)

The method claimed in claim 8, wherein the first silicon germanium layer and the second silicon germanium layer each have a germanium content of approximately 30%.

### Claim 10 (depends on 9)

The method claimed in claim 9, wherein the thickness of the strained silicon layer exceeds 140 Angstroms.

### Claim 11 (depends on 6)

The method claimed in claim 6, wherein the first and second silicon germanium layers have an approximately equal germanium contents at their junctions with the strained silicon layer.

### Claim 12 (depends on 6)

The method claimed in claim 6, further comprising:
removing the second layer of silicon germanium; and
forming a metal oxide semiconductor field effect transistor (MOSFET) comprising the layer of strained silicon between the shallow trench isolations.

### Claim 13 (depends on 12)

The method claimed in claim 12, wherein the strained silicon layer is cooled prior to removing the second layer of silicon germanium.

### Claim 14 (depends on 12)

The method claimed in claim 12, wherein forming a MOSFET on the strained silicon comprises:
forming a gate insulating layer on the strained silicon layer;
forming a gate conductive layer on the gate insulating layer;
patterning the gate conductive layer and the gate insulating layer to form a gate overlying a gate insulator;
implanting shallow source and drain extensions;
implanting deep source and drain regions; and
forming silicide source and drain contacts and a silicide gate contact.

### Claim 15 (depends on 14)

The method claimed in claim 14, wherein the silicide source and drain contacts and the silicide gate contact comprise nickel.

### Claim 16 (depends on 14)

The method claimed in claim 14, wherein implanting shallow source and drain extensions is preceded by forming a first spacer around the gate and gate insulator.

### Claim 17 (depends on 16)

The method claimed in claim 16, wherein implanting deep source and drain regions is preceded by forming a second spacer around the first spacer, and
wherein the second spacer serves as an implantation mask during implanting of the deep source and drain regions.

### Claim 18 (depends on 14)

The method claimed in claim 14, further comprising annealing to activate implanted dopants.

### Claim 19 (depends on 14)

The method claimed in claim 14, wherein implanting source and drain extensions is preceded by implanting halo regions, the halo regions extending toward a channel region beyond ends of the source and drain extensions to be formed, the halo regions comprising a dopant having a conductivity type opposite to the conductivity type of a dopant of the source and drain extensions.

### Claim 20 (depends on 6)

The method claimed in claim 6, wherein forming the strained silicon layer is preceded by removing a portion of the first silicon germanium layer to lower an upper surface of the first silicon germanium layer relative to upper surfaces of the shallow trench isolations.