# US 6,730,566 B2 · Method for non-thermally nitrided gate formation for high voltage devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,566 B2
- Document ID: US6730566B2
- Status: Granted
- Kind: B2
- Application number: 10/264,729
- Filed: 2002-10-04
- Published: 2004-04-08
- Granted: 2004-05-04
- Earliest claimed: 2002-10-04
- Assignees: Texas Instruments Incorporated
- Inventors: Hiroaki Niimi; Rajesh Khamankar; Husam N. Alshareef
- Web page: https://patentgrep.com/patent/US6730566B2

## CPC

- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 84/0144: {Manufacturing their gate insulating layers}
- Y10S 438/92: Controlling diffusion profile by oxidation
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A method is provided for non-thermally nitrided gate formation of high voltage transistor devices. The non-thermally nitrided gate formation is useful in the formation of dual thickness gate dielectric structures. The non-thermally nitrided gate formation comprises nitridation to introduce nitrogen atoms into the gate dielectric layer of the high voltage transistor devices to mitigate leakage associated with the high voltage transistor devices. The nitridation of the gate dielectric layer damages the surface of the gate dielectric layer. The damaged surface of the gate dielectric layer is removed by a relatively low temperature re-oxidation process. The low temperature re-oxidation process minimizes nitrogen loss during a subsequent photoresist stripping process and mitigates film densification, such that the structure can be readily etched by standard etching chemicals in subsequent processing.

## Claims

### Claim 1

A method for fabrication of a transistor device, the method comprising:
forming a gate dielectric layer over a substrate;
introducing nitrogen atoms into the gate dielectric layer to mitigate leakage associated with the operation of the transistor device, the introduction of nitrogen atoms causing surface damage to the gate dielectric layer; and
performing a re-oxidation process at a relatively low temperature on the gate dielectric layer to remove the surface damage from the gate dielectric layer.

### Claim 2 (depends on 1)

The method of claim 1, the relatively low temperature re-oxidation process being performed at a temperature of about 400° C. to about 600° C.

### Claim 3 (depends on 2)

The method of claim 2, the relatively low temperature re-oxidation process being performed for about 30 to about 60 seconds with a gas having about 1% to about 50% of an oxygen-source in an inert gas.

### Claim 4 (depends on 3)

The method of claim 3, the oxygen-source comprising at least one of O2, N2O, and NO and the inert gas comprising at least one of He, Ne, Ar, Kr, Xe and N2.

### Claim 5 (depends on 2)

The method of claim 2, the gate dielectric layer having a thickness of about 15 Å to about 35 Å.

### Claim 6 (depends on 1)

The method of claim 1, further comprising forming a second gate dielectric layer over the substrate, the second gate dielectric layer being associated with a second transistor device, the second gate dielectric layer having a thickness that is thinner than the gate dielectric layer.

### Claim 7 (depends on 1)

The method of claim 1, the introduction of nitrogen atoms comprising performing a plasma nitridation process on the gate dielectric layer by applying one of a nitrogen-source gas and a mixture of a nitrogen-source gas and an inert gas to an exposed surface the gate dielectric layer for about 3 seconds to about 60 seconds at a power of about 2 watts to about 2000 watts at a pressure of about 5 mTorr to about 50 Torr, the nitrogen-source gas comprising one of N2, N2O, NO, and NH3 and the inert gas comprising one of He, Ne, Ar, Kr, and Xe.

### Claim 8 (depends on 1)

The method of claim 1, further comprising forming a photoresist layer over the gate dielectric layer, patterning the photoresist layer to expose portions of the gate dielectric layer that does not form part of the transistor device, etching the gate layer to remove the exposed portions of the gate dielectric layer and stripping the patterned photoresist layer by an Ultra-Violet (UV) Ozone (O3)/Sulfuric Acid (H2SO4) stripping process at about 130° C.

### Claim 9

A method for fabrication of a semiconductor device having dual gate dielectric thickness layers, the method comprising:
forming a first gate dielectric layer in a first active region of a semiconductor device;
performing a plasma nitridation process to introduce nitrogen atoms into the first gate dielectric layer, the plasma nitridation process causing surface damage to the gate dielectric layer;
performing a re-oxidation process at a relatively low temperature on the gate dielectric layer to remove the surface damage from the gate dielectric layer,
forming a second gate dielectric layer in a second active region, the second gate dielectric layer being thinner than the first gate dielectric layer; and
forming a first transistor device associated with the first gate dielectric layer and a second transistor device associated with the second gate dielectric layer, the nitrogen atoms mitigating leakage associated with the operation of the first transistor device.

### Claim 10 (depends on 9)

The method of claim 9, the relatively low temperature re-oxidation process being performed at a temperature of about 400° C. to about 600° C. for about 30 to about 60 seconds with a gas having about 1% to about 50% of an oxygen-source in an inert gas, the oxygen-source comprising at least one of O2, N2O, and NO and the inert gas comprising at least one of He, Ne, Ar, Kr, Xe and N2, the relatively low temperature reoxidation process mitigates nitrogen loss in the dielectric layer caused by subsequent photoresist stripping and mitigates film densification for a subsequent etching process.

### Claim 11 (depends on 9)

The method of claim 9, the first gate dielectric layer having a thickness of about 15 Å to about 35 Å and the second gate dielectric layer having a thickness of about 8 Å to about 14 Å.

### Claim 12 (depends on 9)

The method of claim 9, the first gate dielectric layer and the second dielectric layer comprising an oxide.

### Claim 13 (depends on 9)

The method of claim 9, the plasma nitridation process on the first gate dielectric layer comprising applying one of a nitrogen-source gas and a mixture of a nitrogen-source gas and an inert gas to an exposed surface the first gate dielectric layer for about 3 seconds to about 60 seconds at a power of about 2 watts to about 2000 watts at a pressure of about 5 mTorr to about 50 Torr, the nitrogen-source gas comprising one of N2, N2O, NO, and NH3 and the inert gas comprising one of He, Ne, Ar, Kr, and Xe,.

### Claim 14 (depends on 9)

The method of claim 9, further comprising forming a photoresist layer over the first gate dielectric layer, patterning the photoresist layer to expose portions of the first gate dielectric layer that do not form part of the first transistor device, etching the first gate dielectric layer to remove the exposed portions of the first gate dielectric layer and stripping the patterned photoresist layer by an Ultra-Violet (UV)/Ozone (O3)/Sulfuric Acid (H2SO4) stripping process at about 130° C.

### Claim 15 (depends on 14)

The method of claim 14, further comprising performing a wet chemical cleanup on the semiconductor device after stripping the patterned photoresist layer.

### Claim 16 (depends on 9)

The method of claim 9, the forming a first gate dielectric layer in a first active region of a semiconductor device comprising performing a first oxidation process to form the first gate dielectric layer and the forming a second gate dielectric layer in a second active region comprising performing a second oxidation process to form the second gate dielectric layer.

### Claim 17 (depends on 9)

The method of claim 9, further comprising:
performing a second plasma nitridation process to introduce nitrogen atoms into the second gate dielectric layer, the second plasma nitridation comprising applying one of a nitrogen-source gas and a mixture of nitrogen-source gas and inert gas to an exposed surface the second gate dielectric layer for about 3 seconds to about 60 seconds at a power of about 2 watts to about 2000 watts at a pressure of about 5 mTorr to about 50 Torr, the nitrogen-source gas comprising at least one of N2, N2O, NO, and the inert gas comprising NH3 He, Ne, Ar, Kr, and Xe,; and
performing a second re-oxidation process on the second gate dielectric layer to remove damage to the second gate dielectric layer caused by the second plasma nitridation process, the second re-oxidation process being performed at a temperature of about 400° C. to about 1200° C. for about 1 to about 60 seconds with a gas having about 1% to about 50% of an oxygen-source gas in an inert gas, the oxygen-source gas being one of O2, N2O, and NO and the inert gas being one of He, Ne, Ar, Kr, Xe and N2.

### Claim 18

A method for fabricating a first transistor device having a first gate oxide thickness and a second transistor device having a second gate oxide thickness on the same substrate, the method comprising:
forming a first gate oxide layer having a thickness of about 15 Å to about 35 Å in a first active region of a substrate;
performing a plasma nitridation process to introduce nitrogen atoms into the first gate oxide layer, the plasma nitridation process comprising applying one of a nitrogen-source gas and a mixture of a nitrogen-source gas and inert gas to an exposed surface the first gate oxide layer for about 3 seconds to about 60 seconds at a power of about 2 watts to about 2000 watts at a pressure of about 5 mTorr to about 50 Torr, the nitrogen-source gas comprising at least one of N2, N2O, NO, and NH3 and the inert gas comprising at least one of He, Ne, Ar, Kr, and Xe;
performing a relatively low temperature re-oxidation process on the first gate oxide layer to remove damage to the first gate oxide layer caused by the plasma nitridation process, the relatively low temperature re-oxidation process being performed at a temperature of about 400° C. to about 600° C. for about 30 to about 60 seconds with a gas having about 1% to about 50% of an oxygen-source in an inert gas, the oxygen-source comprising at least one of O2, N2O, and NO and the inert gas comprising at least one of He, Ne, Ar, Kr, Xe and N2;
forming a second gate oxide layer having a thickness of about 8 Å to about 14 Å in a second active region of the substrate; and
forming a first transistor device associated with the first gate oxide layer and a second transistor device associated with the second gate oxide layer, the nitrogen atoms in the first gate oxide layer mitigates leakage associated with the operation of the first transistor device.

### Claim 19 (depends on 9)

The method of claim 9, further comprising forming a photoresist layer over the first gate oxide layer, patterning the photoresist layer to expose portions of the first gate oxide layer that do not form part of the first transistor device, etching the first gate oxide layer to remove the exposed portions of the first gate oxide layer and stripping the patterned photoresist layer by a Ultra-Violet (UV)/Ozone (O3)/Sulfuric Acid (H2SO4) stripping process at about 130° C.

### Claim 20 (depends on 19)

The method of claim 19, further comprising:
performing a second plasma nitridation process to introduce nitrogen atoms into the second gate oxide layer comprising applying one of a nitrogen-source gas and a mixture of a nitrogen-source and inert gas to an exposed surface the second gate oxide layer for about 3 seconds to about 60 seconds at a power of about 2 watts to about 2000 watts at a pressure of about 5 mTorr to about 50 Torr, the nitrogen-source gas comprising one of N2, N2O, NO, and NH3 and the inert gas comprising at least one of He, Ne, Ar, Kr, and Xe; and
performing a second re-oxidation process on the second gate dielectric layer to remove damage to the second gate dielectric layer caused by the second plasma nitridation process, the second re-oxidation process being performed at a temperature of about 400° C. to about 1200° C. for about 1 to about 60 seconds with a gas having about 1% to about 50% of an oxygen-source in an inert gas, the oxygen-source comprising at least one of O2, N2O, and NO and the inert gas comprising at least one of He, Ne, Ar, Kr, Xe and N2.