# US 6,730,561 B2 · Method of forming a cup capacitor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,561 B2
- Document ID: US6730561B2
- Status: Granted
- Kind: B2
- Application number: 09/876,282
- Filed: 2001-06-06
- Published: 2003-01-16
- Granted: 2004-05-04
- Earliest claimed: 2001-06-06
- Assignees: Applied Materials, Inc.
- Inventors: Jeng H. Hwang; Guangxiang Jin
- Web page: https://patentgrep.com/patent/US6730561B2

## CPC

- H10D 1/042: {using deposition processes to form electrode extensions}
- H10D 1/716: {having vertical extensions}
- H10B 12/033: {the capacitor extending over the transistor}
- H10P 50/267: {using plasmas}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10B: ELECTRONIC MEMORY DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A simple method of forming a cup capacitor is disclosed. The method typically involves only “dry” deposition and etching steps, allowing applicants' method to be performed in a single processing apparatus, if so desired. The method includes the following steps: a) providing a semiconductor structure including a dielectric layer overlying a semiconductor substrate, wherein a cup is present in the dielectric layer, the cup having an opening at an upper surface of the dielectric layer; b) depositing a conformal layer of a conductive material over the dielectric layer, including the sidewalls and bottom of the cup; c) depositing a layer of a sacrificial material over the conductive material, in an amount sufficient to fill the cup; d) removing sacrificial material present on an upper surface (field surface) of the conductive layer outside of and adjacent to the cup by plasma etching, using a plasma source gas which selectively etches the sacrificial material relative to the conductive material; e) removing conductive material present on an upper surface (field surface) of the dielectric layer outside of and adjacent to the cup by plasma etching, using a plasma source gas which selectively etches the conductive material relative to the sacrificial material remaining inside of the cup; and f) removing sacrificial layer material remaining inside of the cup by etching, using an etchant which selectively etches the sacrificial material inside of the cup relative to the conductive material inside of the cup.

## Claims

### Claim 1

A method of forming a cup capacitor, comprising the following steps:
a) providing a semiconductor structure including a dielectric layer overlying a semiconductor substrate, wherein a cup is present in said dielectric layer, the cup having an opening at an upper surface of said dielectric layer;
b) depositing a conformal layer of a conductive material selected from the group consisting of platinum, iridium/iridium oxide, ruthenium/ruthenium oxide, and combinations thereof over said dielectric layer, including the sidewalls and bottom of said cup;
c) depositing a layer of a sacrificial material over said conductive material, in an amount sufficient to fill said cup;
d) removing sacrificial material present on an upper surface of said conductive layer outside of and adjacent to said cup by plasma etching, using a plasma source gas which selectively etches said sacrificial material relative to said conductive material;
e) removing conductive material present on an upper surface of said dielectric layer outside of and adjacent to said cup by plasma etching, using a plasma source gas which selectively etches said conductive material relative to said sacrificial material remaining inside of said cup; and
f) removing sacrificial material remaining inside of said cup by etching, using an etchant which selectively etches said sacrificial material inside of said cup relative to said conductive material inside of said cup, whereby said conductive material inside of said cup has an exposed upper surface which is flat and smooth.

### Claim 2 (depends on 1)

The method of claim 1, wherein said sacrificial material is capable of withstanding temperatures of at least 150° C. up to about 450° C.

### Claim 3 (depends on 1)

The method of claim 1, wherein said sacrificial material is a high-temperature organic material.

### Claim 4 (depends on 1)

The method of claim 1, wherein said high-temperature organic material is selected from the group consisting of: an amorphous carbon-comprising material, BCB, SILK™, FLARE™, poly(arylene) ethers, poly(arylene) ether oxazoles, Parylene-N, polyimides, polynaphthalene-N, polyphenyl-quinoxalines, polybenzoxazoles, polyphenylene-oxide, polyindane, polynorborene, divinylsiloxane, and combinations thereof.

### Claim 5 (depends on 1)

The method of claim 1, wherein said conductive material is platinum.

### Claim 6 (depends on 5)

The method of claim 5, wherein said sacrificial material is FLARE, and said FLARE is plasma etched in step d) using a plasma source gas comprising argon and oxygen.

### Claim 7 (depends on 6)

The method of claim 6, herein said plasma source gas used in step d) further comprises chlorine.

### Claim 8 (depends on 5)

The method of claim 5, wherein said platinum is plasma etched using a plasma source gas comprising argon, a chlorine-comprising gas, and a nitrogen-comprising gas.

### Claim 9 (depends on 8)

The method of claim 8, wherein said platinum is plasma etched using a plasma source gas comprising argon, Cl2, and N2.

### Claim 10 (depends on 5)

The method of claim 5, wherein said sacrificial material is FLARE, and said FLARE is plasma etched in step f) using a plasma source gas comprising oxygen and nitrogen.

### Claim 11 (depends on 1)

The method of claim 1, wherein said conductive material is ruthenium/ruthenium oxide.

### Claim 12 (depends on 11)

The method of claim 11, wherein said ruthenium/ruthenium oxide is plasma etched using a plasma source gas comprising an oxygen-comprising gas and a chlorine-comprising gas.

### Claim 13 (depends on 12)

The method of claim 12, wherein said ruthenium/ruthenium oxide is plasma etched using a plasma source gas comprising O2 and Cl2.

### Claim 14 (depends on 1)

The method of claim 1, wherein said semiconductor structure further includes a patterned etch stop layer overlying an upper surface of said dielectric layer and underlying an upper surface of said conductive material outside of said cup.

### Claim 15 (depends on 14)

The method of claim 14, wherein said etch stop layer comprises a dielectric material.

### Claim 16 (depends on 15)

The method of claim 15, wherein said dielectric material is selected from the group consisting of silicon nitride, silicon oxynitride, silicon carbide, or tantalum oxide.

### Claim 17 (depends on 14)

The method of claim 14, wherein said conductive material is plasma etched using a plasma source gas which selectively etches said conductive material relative to said etch stop layer.

### Claim 18 (depends on 16)

The method of claim 16, wherein said conductive material is platinum and said etch stop layer is silicon nitride.

### Claim 19 (depends on 18)

The method of claim 18, wherein said platinum is plasma etched using a plasma source gas comprising argon, Cl2, and N2.

### Claim 20 (depends on 16)

The method of claim 16, wherein said conductive material is ruthenium/ruthenium oxide and said etch stop layer is tantalum oxide.

### Claim 21 (depends on 20)

The method of claim 20, wherein said ruthenium/ruthenium oxide is plasma etched using a plasma source gas comprising an oxygen-comprising gas and a chlorine-comprising gas.

### Claim 22 (depends on 14)

The method of claim 14, wherein said sacrificial material is plasma etched in step f) using a plasma source gas which selectively etches said sacrificial material relative to said etch stop layer.

### Claim 23 (depends on 16)

The method of claim 16, wherein said sacrificial material is FLARE and said etch stop layer is silicon nitride.

### Claim 24 (depends on 23)

The method of claim 23, wherein said FLARE is plasma etched in step f) using a plasma source gas comprising oxygen and nitrogen.

### Claim 25 (depends on 1)

The method of claim 1, wherein said dielectric layer comprises silicon oxide.

### Claim 26 (depends on 1)

The method of claim 1, wherein said substrate comprises silicon.

### Claim 27 (depends on 1)

The method of claim 1, wherein steps b), c), d), e), and f) are performed in a multi-chambered processing apparatus.

### Claim 28 (depends on 14)

The method of claim 14, wherein said method further comprises the following step:
g) depositing a conformal layer of a dielectric material over said etch stop layer and said conductive material layer, including the sidewalls and bottom of said cup.

### Claim 29 (depends on 28)

The method of claim 28, wherein said dielectric material deposited in step g) is a high dielectric constant material.

### Claim 30 (depends on 29)

The method of claim 29, wherein said high dielectric constant material is selected from the group consisting of BST, PZT, SBT, and Ta2O5.

### Claim 31 (depends on 28)

The method of claim 28, wherein said method further comprises the following step:
h) depositing a second layer of a conductive material over said conformal dielectric material layer, in an amount sufficient to fill said cup.

### Claim 32 (depends on 31)

The method of claim 31, wherein said conductive material deposited in step h) is selected from the group consisting of platinum, iridium/iridium oxide, and ruthenium/ruthenium oxide.

### Claim 33 (depends on 31)

The method of claim 31, wherein said method further comprises the following step:
i) depositing a masking layer over said second conductive material layer.

### Claim 34 (depends on 33)

The method of claim 33, wherein said method further comprises the following step:
j) patterning said masking layer.

### Claim 35 (depends on 34)

The method of claim 34, wherein said method further comprises the following step:
k) pattern etching said second conductive material layer.

### Claim 36 (depends on 1)

The method of claim 1, wherein said conductive material comprises a metal.

### Claim 37 (depends on 5)

The method of claim 5, wherein said sacrificial material is a high temperature organic material, and said high temperature organic material is plasma etched in step d) using a plasma source gas comprising argon and oxygen.

### Claim 38 (depends on 37)

The method of claim 37, wherein said plasma source gas used in step d) further comprises chlorine.