# US 6,730,551 B2 · Formation of planar strained layers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,551 B2
- Document ID: US6730551B2
- Status: Granted
- Kind: B2
- Application number: 10/211,126
- Filed: 2002-08-02
- Published: 2003-02-06
- Granted: 2004-05-04
- Earliest claimed: 2001-08-06
- Assignees: Massachusetts Institute of Technology
- Inventors: Minjoo L. Lee; Christopher W. Leitz; Eugene A. Fitzgerald
- Web page: https://patentgrep.com/patent/US6730551B2

## CPC

- H10D 30/751: {having composition variations in the channel regions}
- H10D 30/60: Insulated-gate field-effect transistors [IGFET] (H10D30/40 takes precedence)
- H10D 30/798: {being provided in or under the channel regions}
- H10D 30/801: {FETs having heterojunction gate electrodes}
- H10D 84/0167: {Manufacturing their channels}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 84/85: Complementary IGFETs, e.g. CMOS
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A structure and a method for forming the structure, the method including forming a compressively strained semiconductor layer, the compressively strained layer having a strain greater than or equal to 0.25%. A tensilely strained semiconductor layer is formed over the compressively strained layer. The compressively strained layer is substantially planar, having a surface roughness characterized in (i) having an average wavelength greater than an average wavelength of a carrier in the compressively strained layer or (ii) having an average height less than 10 nm.

## Claims

### Claim 1

A method for forming a structure, the method including:
forming a compressively strained semiconductor layer, the compressively strained layer having a strain greater than or equal to 0.25%; and
forming a tensilely strained semiconductor layer over the compressively strained layer,
wherein the compressively strained layer is substantially planar, having a surface roughness characterized by at least one of (i) an average roughness wavelength greater than an average wavelength of a carrier in the compressively strained layer and (ii) an average roughness height less than 10 nm.

### Claim 2 (depends on 1)

The method of claim 1, wherein the compressively strained layer comprises at least one group IV element.

### Claim 3 (depends on 1)

The method of claim 1, wherein the compressively strained layer comprises at least one of silicon and germanium.

### Claim 4 (depends on 3)

The method of claim 3, wherein the compressively strained layer comprises >1% germanium.

### Claim 5 (depends on 1)

The method of claim 1, wherein the tensilely strained layer comprises silicon.

### Claim 6 (depends on 1)

The method of claim 1, wherein the compressively strained layer comprises at least one of a group III and a group V element.

### Claim 7 (depends on 6)

The method of claim 6, wherein the compressively strained layer comprises indium gallium arsenide.

### Claim 8 (depends on 6)

The method of claim 6, wherein the compressively strained layer comprises indium gallium phosphide.

### Claim 9 (depends on 6)

The method of claim 6, wherein the compressively strained layer comprises gallium arsenide.

### Claim 10 (depends on 1)

The method of claim 1, wherein the compressively strained layer comprises at least one of a group II and a group VI element.

### Claim 11 (depends on 10)

The method of claim 10, wherein the compressively strained layer comprises zinc selenide.

### Claim 12 (depends on 10)

The method of claim 10, wherein the compressively strained layer comprises sulphur.

### Claim 13 (depends on 10)

The method of claim 10, wherein the compressively strained layer comprises cadmium telluride.

### Claim 14 (depends on 10)

The method of claim 10, wherein the compressively strained layer comprises mercury telluride.

### Claim 15 (depends on 1)

The method of claim 1, wherein the compressively strained layer has a thickness of less than 500 Å.

### Claim 16 (depends on 15)

The method of claim 15, wherein the compressively strained layer has a thickness of less than 200 Å.

### Claim 17 (depends on 1)

The method of claim 1, wherein the compressively strained layer is formed at a first temperature, at least a portion of the tensilely strained layer is formed at a second temperature, and the second temperature is greater than the first temperature.

### Claim 18 (depends on 17)

The method of claim 17, wherein the tensilely strained layer comprises silicon and the second temperature is greater than 450° C.

### Claim 19 (depends on 17)

The method of claim 17, wherein forming the tensilely strained layer at a second temperature includes initially forming a first portion of the tensilely strained layer at the first temperature and forming a second portion of the tensilely strained layer at the second temperature, the first temperature being sufficiently low to substantially avoid disruption of planarity, the first portion of the tensilely strained layer maintaining the planarity of the compressively strained layer notwithstanding transition to the second temperature.

### Claim 20 (depends on 1)

The method of claim 1, wherein the tensilely strained layer is formed at a rate greater than 100 Å/hour.

### Claim 21 (depends on 1)

The method of claim 1, wherein the compressively strained layer is formed by chemical vapor deposition.

### Claim 22 (depends on 1)

The method of claim 1, wherein the tensilely strained layer is formed by chemical vapor deposition.

### Claim 23 (depends on 1)

The method of claim 1, wherein the wavelength of the surface roughness is greater than 10 nanometers.