# US 6,730,538 B1 · Fabricating electronic devices using actinide oxide semiconductor materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,538 B1
- Document ID: US6730538B1
- Status: Granted
- Kind: B1
- Application number: 09/599,341
- Filed: 2000-06-22
- Granted: 2004-05-04
- Earliest claimed: 2000-06-22
- Assignees: The University of Tennessee Research Corporation
- Inventors: Thomas T. Meek; Michael Z. Hu
- Web page: https://patentgrep.com/patent/US6730538B1

## CPC

- H10F 71/00: Manufacture or treatment of devices covered by this subclass (patterning processes to connect thin photovoltaic cells in integrated devices, or assemblies of multiple devices, having photovoltaic cells H10F19/33; manufacture or treatment of encapsulations or containers for integrated devices, or assemblies of multiple devices, having photovoltaic cells H10F19/80; manufacture or treatment of integrated devices, or assemblies of multiple devices, comprising at least one element in which radiation controls the flow of current H10F39/00)
- H10F 10/18: Photovoltaic cells having only Schottky potential barriers
- H10F 77/12: Active materials
- H10N 10/855: comprising compounds containing boron, carbon, oxygen or nitrogen
- H10P 14/6328: {Deposition from the gas or vapour phase}
- C22B 58/00: Obtaining gallium or indium {(treatment or purification of solutions by liquid-liquid extraction, by ion-exchange or by adsorption C22B3/20)}
- Y02E 10/50: Photovoltaic [PV] energy
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for fabricating electronic devices. First, an actinide oxide semiconductor material is provided. Next, an electronic device is fabricated using the actinide oxide semiconductor material.

## Claims

### Claim 1

A method for fabricating solar cells, comprising:
a. providing an actinide oxide semiconductor oxide selected from the group consisting of uranium and plutonium; and
b. fabricating a solar cell using the actinide oxide semiconductor material.

### Claim 2 (depends on 1)

The method of claim 1, wherein the actinide oxide semiconductor material is selected from the group consisting of UO2 and U3O8.

### Claim 3 (depends on 1)

The method of claim 1, wherein actinide oxide semiconductor material comprises a mixture of two or more semiconductive actinide oxides.

### Claim 4 (depends on 1)

The method of claim 1, wherein the solar cell is a Schottky-barrier solar cell.

### Claim 5 (depends on 1)

The method of claim 1, wherein step (b) comprises the step of radiation-hardening the solar cell.

### Claim 6 (depends on 1)

The method of claim 1, wherein the solar cell is one of an optical and an IR solar cell.

### Claim 7 (depends on 1)

An electronic device fabricated in accordance with the method of claim 1.

### Claim 8

A method of fabricating a solar cell comprising:
a. providing a raw semiconductive actinide oxide as a by-product of a nuclear energy process;
b. forming refined actinide oxide semiconductor material from the raw semiconductive actinide oxide; and
c. fabricating a solar cell using said refined actinide oxide semiconductor material.

### Claim 9

A method for fabricating a thermoelectric device comprising:
a. providing UO2; and
b. using the UO2 to fabricate a thermoelectric device comprising a junction between the UO2 portion and a Bi2Te3 thermoelectric material, wherein a thermal gradient across the junction will generate an electric current via the Seebeck effect.

### Claim 10

A method of fabricating an electronic device comprising:
a. providing depleted uranium raw semiconductive actinide oxide formed as a by product of uranium enrichment;
b. converting the raw semiconductive actinide oxide into an ingot of refined actinide oxide material;
c. slicing the ingot into a plurality of wafers; and
d. fabricating an electronic device using one of the wafers.

### Claim 11 (depends on 10)

The method of claim 10 wherein the refined actinide oxide material is one of single and polycrystalline form.

### Claim 12

A method of fabricating an electronic device comprising:
a. providing actinide oxide fuel pellets comprising raw UO2 encased in a graphite coating;
b. stripping the graphite coating off the raw UO2;
c. grinding the raw UO2 into a powder;
d. converting the powder form of raw UO2 into an ingot;
e. slicing the ingot into an plurality of wafers; and
f. fabricating an electronic device using one of the wafers.

### Claim 13 (depends on 12)