# US 6,730,525 B2 · Method of manufacturing a electrode of capacitor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,525 B2
- Document ID: US6730525B2
- Status: Granted
- Kind: B2
- Application number: 10/393,001
- Filed: 2003-05-12
- Published: 2004-01-22
- Granted: 2004-05-04
- Earliest claimed: 1997-11-28
- Assignees: Rohm Co., Ltd.
- Inventors: Takashi Nakamura
- Web page: https://patentgrep.com/patent/US6730525B2

## CPC

- H10P 14/46: using a liquid
- H10P 14/412: {Deposition of metallic or metal-silicide materials}
- H10P 14/69398: {the material having a perovskite structure, e.g. BaTiO3}
- H10D 1/684: {the dielectrics comprising multiple layers, e.g. comprising buffer layers, seed layers or gradient layers}
- H10D 1/694: {comprising noble metals or noble metal oxides}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

An organic compound of a noble metal is dissolved in an alcohol to make a coating agent wherein the electrode material configuring a lower electrode is liquefied. On the surface of a substrate 1, the coating agent is applied by spin coating to a thickness of 100 to 1000 Å or so. Heating is performed, using a drying apparatus such as a hot plate or oven to a temperature of 400 to 600° C., and the halogen and organic solvent are evaporated. Even then there is foreign matter 5 underneath, a lower electrode 2 is formed having a flattened surface. On the surface of the lower electrode 2 are formed PZT and an upper electrode 4. Heat treatment is then performed in an oxidizing atmosphere at a high temperature of 650 to 850° C. or so. The ferroelectric material is subjected to crystallization. A lower electrode of a ferroelectric layer having a flat surface is formed.

## Claims

### Claim 1

A method of forming a device on a semiconductor substrate, the device having a noble metal electrode, a dielectric layer on the noble metal electrode and an upper-electrode on the dielectric layer, the method comprising the steps of:
A) forming said noble metal electrode which having a fiat surface for receiving said dielectric layer of uniform thickness by performing the following steps:
a1) providing said semiconductor substrate for forming said noble metal electrode on an electrode receiving surface of said substrate, said electrode receiving surface having irregularities;
a2) preparing a coating agent wherein said noble metal that has been converted into a compound soluble in a solvent is liquefied by said solvent;
a3) applying an effective amount of said liquefied coating agent to said electrode receiving surface to avoid influence of said irregularities on said electrode receiving surface of said semiconductor substrate; and
a4) removing said solvent from said coating agent to form said noble metal electrode having said fiat surface for receiving the dielectric layer wherein said thickness of the dielectric layer is uniform and avoid influence of said irregularities on said electrode receiving surface of said semiconductor substrate;
B) forming said dielectric layer on said noble metal electrode; and
C) forming said upper electrode on said dielectric layer.

### Claim 2 (depends on 1)

The method according to claim 1,
wherein said coating agent is an organic solvent in which an organic compound of a noble metal is dissolved; and
wherein said organic material is evaporated from said organic solvent to remove said solvent.

### Claim 3 (depends on 1)

The method according to claim 1,
wherein said coating agent is an organic solvent in which a halide of a noble metal is dissolved; and
wherein halogen is evaporated from said organic solvent to remove said solvent.

### Claim 4 (depends on 2)

The method according to claim 2, wherein, when evaporating said organic material, an electrically conductive oxide consisting of an oxide of said noble metal is formed.

### Claim 5 (depends on 3)

The method according to claim 3, wherein, when evaporating said halogen, an electrically conductive oxide consisting of an oxide of said noble metal is formed.

### Claim 6 (depends on 4)

The method according to claim 4, wherein said electrically conductive oxide is reduced.

### Claim 7 (depends on 5)

The method according to claim 5, wherein said electrically conductive oxide is reduced.

### Claim 8 (depends on 1)

The method according to claim 1, wherein said lower electrode is a laminated structure of electrically conductive material, and at least one layer in said laminated structure is formed by application of said coating agent.

### Claim 9 (depends on 3)

The method according to claim 3, wherein said halide of said noble metal is PtCl4.

### Claim 10 (depends on 3)

The method according to claim 3, wherein said halide of said noble metal is PtBr2.

### Claim 11 (depends on 3)

The method according to claim 3, wherein said halide of said noble metal is PtBr4.

### Claim 12 (depends on 3)

The according to claim 3, wherein said halide of said noble metal is PtI2.

### Claim 13 (depends on 3)

The method according to claim 3, wherein said halide of said noble metal is IrF3.

### Claim 14 (depends on 3)

The method according to claim 3, wherein said halide of said noble metal is RhCl3.

### Claim 15 (depends on 3)

The method according to claim 3, wherein said halide of said noble metal is OsBr4.

### Claim 16 (depends on 3)

The method according to claim 3, wherein said halide of said noble metal is OsCl3.

### Claim 17 (depends on 3)

The method according to claim 3, wherein said halide of said noble metal is RhF6.

### Claim 18 (depends on 3)

The method according to claim 3, wherein said halide of said noble metal is RhBr3.

### Claim 19 (depends on 2)

The method according to claim 2, wherein said halide of said noble metal is Ir(C3H5)3.

### Claim 20 (depends on 2)

The method according to claim 2, wherein said halide of said noble metal is Pt(C3H5)3.

### Claim 21 (depends on 2)

The method according to claim 2, wherein said halide of said noble metal is Ir(C3H5)(C5H5).

### Claim 22 (depends on 2)

The method according to claim 2, wherein said halide of said noble metal is Pt(C3H5)(C5H5).