# US 6,730,524 B2 · Method for manufacturing ferroelectric thin film device, ink jet recording head, and ink jet printer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,524 B2
- Document ID: US6730524B2
- Status: Granted
- Kind: B2
- Application number: 10/290,290
- Filed: 2002-11-08
- Published: 2003-05-15
- Granted: 2004-05-04
- Earliest claimed: 1998-10-14
- Assignees: Seiko Epson Corporation
- Inventors: Masami Murai
- Web page: https://patentgrep.com/patent/US6730524B2

## CPC

- B41J 2/1628: {dry etching}
- B41J 2/14233: {of film type, deformed by bending and disposed on a diaphragm}
- B41J 2/161: {of film type, deformed by bending and disposed on a diaphragm}
- B41J 2/1623: {bonding and adhesion}
- B41J 2/1629: {wet etching}
- B41J 2/1642: {thin film formation by CVD [chemical vapor deposition]}
- B41J 2/1645: {thin film formation by spincoating}
- B41J 2/1646: {thin film formation by sputtering}
- H10N 30/078: by sol-gel deposition
- H10N 30/2047: {Membrane type}
- H10N 30/8554: {Lead-zirconium titanate [PZT] based}
- B41J: TYPEWRITERS; SELECTIVE PRINTING MECHANISMS, i.e. MECHANISMS PRINTING OTHERWISE THAN FROM A FORME; CORRECTION OF TYPOGRAPHICAL ERRORS
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR

## Abstract

It is an object of the present invention to control the crystal orientation of a ferroelectric thin film as dictated by the application of a ferroelectric thin film device. To accomplished the stated object, a bottom electrode containing at least iridium is formed over a surface preparation layer whose main component is zirconium oxide, and an ultra-thin titanium layer is laminated over the bottom electrode. An amorphous layer containing the elemental metal and elemental oxygen that constitute the ferroelectric is formed over the titanium layer, and a crystallized ferroelectric thin film is formed by heat treating this amorphous layer. If the thickness of the titanium layer is kept between 2 nm and 10 nm in the lamination thereof, the ferroelectric thin film will have a priority orientation of (100), and if it is kept between 10 nm and 20 nm, the ferroelectric thin film will have a priority orientation of (111).

## Claims

### Claim 1

A method for manufacturing an electromechanical transducer, comprising the steps of:
using a compound selected from the group consisting of zirconium oxide, tantalum oxide, silicon nitride, and aluminum oxide to form an interlayer on the surface where said transducer is installed;
forming a bottom electrode over said interlayer, wherein said step of forming said bottom electrode comprises the steps of,
using iridium to form a first iridium layer,
using a specific metal to form a metal layer of said first iridium layer, and
using iridium to form a second iridium layer over said metal layer;
forming a ferroelectric thin film precursor over said bottom electrode; and
baking said ferroelectric thin film precursor at a temperature of 750° C. or lower, thereby diffusing iridium of said first iridium layer and converting said first iridium layer and said metal layer into an alloy layer in which indium is alloyed with said metal.

### Claim 2

A method for manufacturing an electromechanical transducer, comprising the steps of:
using a compound selected from the group consisting of zirconium oxide, tantalum oxide, silicon nitride, and aluminum oxide to form an interlayer on the surface where said transducer is installed;
forming a bottom electrode over said interlayer, wherein said step of forming said bottom electrode comprises the steps of,
using iridium to form a first iridium layer,
using a specific metal to form a metal layer of said first iridium layer, and
using iridium to form a second iridium layer over said metal layer;
forming a ferroelectric thin film precursor over said bottom electrode; and
baking said ferroelectric thin film precursor at a temperature higher than 750° C., thereby diffusing the iridium of said first iridium layer and moving the iridium of said first iridium layer to said second iridium layer.

### Claim 3 (depends on 1)

The method for manufacturing an electromechanical transducer according to claim 1, wherein the ratio of the thickness of said first iridium layer prior to baking to the thickness of said bottom electrode overall is set to be between 1/3 and 4/5.

### Claim 4 (depends on 1)

The method for manufacturing an electromechanical transducer according to claim 1, further comprising the step of:
using a metal that will adhere to the layers above and below to form an adhesive layer between said bottom electrode and said interlayer.

### Claim 5 (depends on 4)

The method for manufacturing an electromechanical transducer according to claim 4, wherein said step of forming a bottom electrode is a step of forming a film such that the following relationship is satisfied:
dT=3.6×d0+2.4×d1+0.8×d2+2.3×d3
where d0 is the thickness of said adhesive layer prior to baking, d1 is the thickness of said first iridium layer, d2 is the thickness of said metal layer, d3 is the thickness of said second iridium layer, and dT is the thickness of said bottom electrode overall after baking.

### Claim 6 (depends on 2)

The method for manufacturing an electromechanical transducer according to claim 2, wherein the ratio of the thickness of said first iridium layer prior to baking to the thickness of said bottom electrode overall is set to be between 1/3 and 4/5.

### Claim 7 (depends on 6)

The method for manufacturing an electromechanical transducer according to claim 6, further comprising the step of:
using a metal that will adhere to the layers above and below to form an adhesive layer between said bottom electrode and said interlayer.

### Claim 8 (depends on 7)

The method for manufacturing an electromechanical transducer according to claim 7, wherein said step of forming a bottom electrode is a step of forming a film such that the following relationship is satisfied:
dT=3.6×d0+2.4×d1+0.8×d2+2.3×d3
where d0 is the thickness of said adhesive layer prior to baking, d1 is the thickness of said first iridium layer, d2 is the thickness of said metal layer, d3 is the thickness of said second iridium layer, and dT is the thickness of said bottom electrode overall after baking.

### Claim 9 (depends on 2)

The method for manufacturing an electromechanical transducer according to claim 2, further comprising the step of:
using a metal that will adhere to the layers above and below to form an adhesive layer between said bottom electrode and said interlayer.

### Claim 10 (depends on 9)

The method for manufacturing an electromechanical transducer according to claim 9, wherein said step of forming a bottom electrode is a step of forming a film such that the following relationship is satisfied:
dT=3.6×d0+2.4×d1+0.8×d2+2.3×d3
where d0 is the thickness of said adhesive layer prior to baking, d1 is the thickness of said first iridium layer, d2 is the thickness of said metal layer, d3 is the thickness of said second iridium layer, and dT is the thickness of said bottom electrode overall after baking.

### Claim 11 (depends on 3)

The method for manufacturing an electromechanical transducer according to claim 3, further comprising the step of:
using a metal that will adhere to the layers above and below to form an adhesive layer between said bottom electrode and said interlayer.

### Claim 12 (depends on 11)

The method for manufacturing an electromechanical transducer according to claim 11, wherein said step of forming a bottom electrode is a step of forming a film such that the following relationship is satisfied:
dT=3.6×d0+2.4×d1+0.8×d2+2.3×d3
where d0 is the thickness of said adhesive layer prior to baking, d1 is the thickness of said first iridium layer, d2 is the thickness of said metal layer, d3 is the thickness of said second iridium layer, and dT is the thickness of said bottom electrode overall after baking.

### Claim 13 (depends on 1)

The method for manufacturing an electromechanical transducer according to claim 1, wherein the metal layer is a platinum layer.

### Claim 14 (depends on 2)

The method for manufacturing an electromechanical transducer according to claim 2, wherein the metal layer is a platinum layer.