# US 6,730,523 B2 · Low temperature chemical vapor deposition process for forming bismuth-containing ceramic thin films useful in ferroelectric memory devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,523 B2
- Document ID: US6730523B2
- Status: Granted
- Kind: B2
- Application number: 09/873,138
- Filed: 2001-06-01
- Published: 2001-11-15
- Granted: 2004-05-04
- Earliest claimed: 1997-06-26
- Assignees: Advanced Technology Materials, Inc.; Siemens Aktiengesellschaft
- Inventors: Frank S. Hintermaier; Christine Dehm; Wolfgang Hoenlein; Peter C. Van Buskirk; Jeffrey F. Roeder; Bryan C. Hendrix; Thomas H. Baum; Debra A. Desrochers
- Web page: https://patentgrep.com/patent/US6730523B2

## CPC

- H10P 14/69398: {the material having a perovskite structure, e.g. BaTiO3}
- C23C 16/40: Oxides
- C23C 16/56: After-treatment
- H10P 14/668: {the materials being characterised by the deposition precursor materials}
- H10P 14/6334: {using decomposition or reaction of gaseous or vapour phase compounds, i.e. chemical vapour deposition (deposition by physical ablation of a target H10P14/6329)}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A low temperature CVD process using a tris (β-diketonate) bismuth precursor for deposition of bismuth ceramic thin films suitable for integration to fabricate ferroelectric memory devices. Films of amorphous SBT can be formed by CVD and then ferroannealed to produce films with Aurivillius phase composition having superior ferroelectric properties suitable for manufacturing high density FRAMs.

## Claims

### Claim 1

A method of depositing bismuth or a bismuth-containing film on a substrate from a precursor therefor, comprising vaporizing a bismuth β-diketonate precursor to form a vaporized precursor, and contacting the vaporized precursor with the substrate to deposit bismuth or a bismuth-containing film thereon, wherein the bismuth β-diketonate precursor comprises an anhydrous mononuclear bismuth β-diketonate.

### Claim 2

A CVD process for depositing bismuth on a substrate from a bismuth precursor, comprising using as said bismuth precursor anhydrous mononuclear tris (β-diketonate) bismuth, and carrying out said CVD process at a deposition temperature not exceeding 400°C.

### Claim 3

A CVD process according to ciaim 2, wherein said bismuth precursor is anhydrous mononuclear tris(2,2,6,6-tetramethyl-3,5-heptanedionato) bismuth.

### Claim 4 (depends on 2)

A CVD process according to claim 2, for forming a film comprising bismuth which can be transformed into a ferroelectric film with a layered pseudo-perovskite structure (Aurivillius phase) having the general formula:
(Bi2O2)2+(Am−1BmO3m+1)2+, where A=Bi3+,
L3+, L2+, Ca2+, Sr2+, Ba2+, Pb2+, Na+,
B=Fe3+,
Al3+, Sc3+, Y3+, L3+, L4+, Ti4+,
Nb5+, Ta5+,
W6+, Mo6+, L=a lanthanide metal, and m=1,2,3,4,5.

### Claim 5 (depends on 2)

A CVD process according to claim 2, for deposition of a bismuth phase selected from the group consisting of:
Bi2WO6
BiMO3 (M=Fe, Mn)
Ba2BiMO6 (M=V, Nb, Ta)
Pb2BiMO6 (M=V, Nb, Ta)
Ba3Bi2MO9 (M=Mo, W)
Pb3Bi2MO9 (M=Mo, W)
Ba6BiMO18 (M=Mo, W)
Pb6BiMO18 (M=Mo, W)
KBiTi2O6
K2BiNb5O15.

### Claim 6 (depends on 2)

A CVD process according to claim 2, further comprising deposition of Sr from a precursor therefor selected from the group consisting of Sr(thd)2 and Sr(thd)2 adducts.

### Claim 7 (depends on 2)

A CVD process according to claim 2, comprising multiple precursors in a single solution.

### Claim 8 (depends on 2)

A CVD process according to claim 2, comprising combining multiple precursors together in a single solution as a precursor cocktail and delivering the precursors from said cocktail.

### Claim 9 (depends on 2)

A CVD process according to claim 2, using combinations of single, binary or ternary precursor solutions for precursors therein.

### Claim 10 (depends on 2)

A CVD process according to claim 2, wherein the precursor is vaporized at a temperature of 170-230° C.

### Claim 11 (depends on 2)

A CVD process according to claim 2, wherein a bismuth-containing film is deposited over a bottom electrode formed of a material selected from the group consisting of: metals Pt, Pd, Au, Ir, Rh, and alloys thereof, conducting metal oxides IrOx, RhOx, RuOx (0<x<2), and mixtures of thereof with one or more of said metals, conducting metal nitrides TiNx, ZrNx, (0<x<1.1), Wx,TaNx (0<x<1.7), and superconducting oxides selected from the group consisting of YBa2Cu2O7-x and Bi2Sr2Ca2Cu3O10.

### Claim 12 (depends on 2)

A CVD process according to claim 2, using a substrate comprising at least one of the following: Si, n- or p-doped Si, SiO2, Si3N4, or a complex integrated circuit.

### Claim 13 (depends on 2)

A CVD process according to claim 2, using a substrate which comprises at least one of the following: GaAs, SiC, MgO, Al2O3, ZrO2 and MTiO3 (M=Sr, Ba, Pb).

### Claim 14 (depends on 2)

A CVD process according to claim 2, having a deposition pressure of 0.001 to 760 torr.

### Claim 15 (depends on 2)

A CVD process according to claim 2, having a deposition pressure of 0.1-10 torr.

### Claim 16 (depends on 2)

A CVD process according to claim 2, having a total gas flow during the deposition of 1-16,000 sccm.

### Claim 17 (depends on 2)

A CVD process according to claim 2, having Ar, He and/or N2 as an inert gas for the precursor.

### Claim 18 (depends on 2)

A CVD process according to claim 2, wherein an oxidizer is mixed with the precursor vapor, and said oxidizer is selected from the group consisting of O2, singlet O2, ozone, NOx wherein x=1, 2, or 3, hydrogen peroxide, oxygen plasma, N2O, and mixtures thereof.

### Claim 19 (depends on 2)

A CVD process according to claim 2, enhanced by any physical or chemical techniques.

### Claim 20 (depends on 2)

A CVD process according to claim 2, for integration of SBT.

### Claim 21 (depends on 2)

A CVD process according to claim 2, for forming a bismuth containing film of a material selected from the group consisting of:
SrBi2Ta2O9
SrBi2Ta2-xNbxO9 (0<x<2)
SrBi2Nb2O9
Sr1-xBaxBi2Ta2-yNbyO9 (0≦x≦1, 0≦y≦2)
Sr1-xCaxBi2Ta2-yNbyO9 (0≦x≦1, 0≦y≦2)
Sr1-xPbxBi2Ta2-yNbyO9 (0≦x≦1, 0≦y≦2)
Sr1-x-y-zBaxCayPbzBi2Ta2-pNbpO9 (0≦x≦1, 0≦y≦1, 0≦z≦1, 0≦p≦2).

### Claim 22 (depends on 2)

A CVD process according to claim 2, for deposition of a bismuth titanate material selected from the group consisting of:
Bi4Ti3O12
PrBi3Ti3O12
HoBi3Ti3O12
LaBi3Ti3O12
Bi3TiTaO9
Bi3TiNbO9
SrBi4Ti4O15
CaBiTi4O15
BaBi4Ti4O15
PbBi4Ti4O15
Sr1-x-y-zCaxBayPbzBi4Ti4O15 (0≦x≦1, 0≦y≦1, 0≦z≦1)
Sr2Bi4Ti5O18
Ca2Bi4Ti5O18
Ba2Bi4Ti5O18
Pb2Bi4Ti5O18
Sr2-x-y-zCaxBayPbzBi4Ti5O18 (0≦x≦2, 0≦y≦2, 0≦z≦2)
SrBi5Ti4FeO18
CaBi5Ti4FeO18
BaBi5Ti4FeO18
PbBi5Ti4FeO18
Sr1-x-y-zCaxBayPbzBi5Ti4FeO18 (0≦xφ1, 0≦y≦1, 0≦z≦1)
Bi5Ti3FeO15
LaBi4Ti3FeO15
PrBi4Ti3FeO15
Bi6Ti3FeO18
Bi9Ti3Fe5O27.

### Claim 23 (depends on 2)

A CVD process according to claim 2, including the process steps of:
inserting the substrate into a CVD reactor chamber,
heating the substrate up to the deposition temperature,
flushing the substrate with a mixture of an inert gas and an optionally an oxidizer,
delivering precursor vapor mixed with an inert carrier gas, and optionally an oxidizer,
exposing the substrate to the precursor vapor,
discontinuing the flow of precursor vapor,
flushing the substrate with a mixture of an inert gas and optionally an oxidizer, and cooling the substrate.

### Claim 24 (depends on 21)

A CVD process according to claim 21, wherein at least one of the elements of the film is substituted or doped by a metal of the lanthanide series.

### Claim 25 (depends on 22)

A CVD process according to claim 22, wherein at least one of the elements of the film is substituted or doped by a metal of the lanthanide series.

### Claim 26 (depends on 23)

A CVD process according to claim 23, comprising pretreating the substrate in the CVD reactor before deposition by (1) exposure to a predetermined atmosphere and/or (2) annealing.

### Claim 27 (depends on 23)

A CVD process according to claim 23, further comprising the post-processing steps of:
annealing the film at 600-800° C.,
depositing a top electrode on the film, and
further annealing the film at a temperature in the range of 600-800° C.

### Claim 28 (depends on 23)

A CVD process according to claim 23, further comprising the post-processing steps of:
depositing a top electrode on the film, and
annealing the film at 600-800° C.

### Claim 29 (depends on 23)

A CVD process according to claim 23, comprising a multiple step CVD process.

### Claim 30 (depends on 23)

A CVD process according to claim 23, including an intermediate removal of the substrate from the chamber, conducting other processes and reentering the substrate into the CVD chamber to continue CVD of the bismuth-containing film.

### Claim 31 (depends on 23)

A CVD process according to claim 23, comprising changing process parameters during the process selected from the group consisting of temperature, pressure, gas flows, and gas phase composition.

### Claim 32 (depends on 27)

A CVD process according to claim 27, comprising carrying out the annealing steps in an oxidizing atmosphere.

### Claim 33 (depends on 32)

A CVD process according to claim 32, comprising carrying out the annealing step in an oxidizing atmosphere.

### Claim 34 (depends on 2)

A CVD process according to claim 2, enhanced by an enhancement technique selected from plasma enhancement and photoactivation enhancement.

### Claim 35 (depends on 27)

A CVD process according to claim 27, comprising carrying out the annealing steps in an oxidizing atmosphere comprising O2 or O3.

### Claim 36

A CVD process for depositing bismuth on a substrate from a bismuth precursor, comprising using tris (β-diketonate) bismuth as said bismuth precursor, and carrying out said CVD process at a deposition temperature not exceeding 600° C., and further comprising deposition of Sr from a precursor therefor selected from the group consisting of Sr(thd)2 and Sr(thd)2 adducts where the Sr adduct is selected from the group consisting of tetraglyme (═MeO—(CH2CH2O)4—Me), triglyme (═MeO—(CH2CH2O)3—Me), N,N,N′,N″,N″-pentamethyldiethylenetriamine (═Me2N—(CH2CH2NMe)2—Me) and N,N,N′,N″,N′″,N′″-hexamethyltriethylenetetramine (═Me2N—(CH2CH2NMe)3—Me).

### Claim 37

A CVD process for depositing bismuth on a substrate from a bismuth precursor, comprising using as said bismuth precursor tris (β-diketonate) bismuth, and carrying out said CVD process at a deposition temperature not exceeding 600° C., further comprising depositing tantalum from a Ta precursor of the general formula Ta(OR)5-n(X)n wherein R=Me, Et, n-Pr, i-Pr, n-Bu, i-Bu, t-Bu, n-pentyl, or i-pentyl, X=β-diketonate, and n=1,2,3,4, or 5.

### Claim 38 (depends on 37)

A CVD process according to claim 37, employing Ta(OiPr)4(thd) as the Ta precursor.

### Claim 39

A CVD process for depositing bismuth on a substrate from a bismuth precursor, comprising using as said bismuth precursor tris (β-diketonate) bismuth, and carrying out said CVD process at a deposition temperature not exceeding 600° C., wherein the precursor is provided in a solvent comprising an aliphatic, a cyclophatic or an aromatic hydrocarbon solvent.

### Claim 40 (depends on 39)

A CVD process according to claim 39, using a mixture of THF, iPrOH and tetraglyme as the precursor solvent.

### Claim 41 (depends on 39)

A CVD process according to claim 39, using a mixture of THF, iPrOH and a polyamine as the precursor solvent.

### Claim 42 (depends on 39)

A CVD process according to claim 39, using a hydrocarbon solvent comprising an alkane having a carbon number greater than 7 as the precursor solvent.

### Claim 43 (depends on 42)

A CVD process according to claim 42, wherein said alkane is selected from octane, nonane, decane, undecane, dodecane, tridecane, tetradecane, and mixtures comprising one or more of the foregoing species.

### Claim 44 (depends on 39)

A CVD process according to claim 39, using a mixture of octane, decane, and pentamethyldiethylenetriamine as the precursor solvent.

### Claim 45

A CVD process for depositing a conformal bismuth film on a substrate from a bismuth precursor, comprising using as said bismuth precursor anhydrous mononuclear tris (β-diketonate) bismuth, and carrying out said CVD process at a deposition temperature not exceeding 400° C.

### Claim 46

A CVD process for depositing bismuth on a substrate from a bismuth precursor, comprising using as said bismuth precursor tris (β-diketonate) bismuth, and carrying out said CVD process at a deposition temperature not exceeding 600° C., wherein the precursor is provided in a solvent comprising a substituted hydrocarbon solvent, wherein the substituted hydrocarbon includes a functional group selected from alcohols, ethers, esters, amines, ketones, and aldehydes.

### Claim 47

A method of depositing bismuth or a bismuth-containing film on a substrate from a precursor therefor, comprising:
(a) vaporizing a bismuth β-diketonate precursor to form a vaporized precursor, wherein the bismuth β-diketonate precursor comprises an anhydrous mononuclear bismuth β-diketonate;
(b) contacting the vaporized precursor with the substrate to deposit bismuth or a bismuth-containing film thereon at temperatures not exceeding 600° C. to form a substantially amorphous bismuth or bismuth-containing film; and