# US 6,730,461 B2 · Thermally developable imaging materials with reduced mottle providing improved image uniformity

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,461 B2
- Document ID: US6730461B2
- Status: Granted
- Kind: B2
- Application number: 10/012,171
- Filed: 2001-10-26
- Published: 2003-07-24
- Granted: 2004-05-04
- Earliest claimed: 2001-10-26
- Assignees: Eastman Kodak Company
- Inventors: Bryan V. Hunt; Steven H. Kong; William D. Ramsden; Gary E. Labelle
- Web page: https://patentgrep.com/patent/US6730461B2

## CPC

- G03C 1/49854: {Dyes or precursors of dyes (for diffusion-transfer G03C8/10, G03C8/4013)}
- G03C 1/74: Applying photosensitive compositions to the base; Drying processes therefor (G03C1/496 takes precedence)
- G03C 1/127: {the polymethine chain forming part of a carbocyclic ring}
- G03C 1/20: with more than three CH groups
- G03C 1/49872: {Aspects relating to non-photosensitive layers, e.g. intermediate protective layers}
- G03C 1/825: characterised by antireflection means or visible-light filtering means, e.g. antihalation
- G03C 2001/7635: {Protective layer}
- Y10S 430/136: Coating process making radiation sensitive element
- Y10S 430/162: Protective or antiabrasion layer
- G03C: PHOTOSENSITIVE MATERIALS FOR PHOTOGRAPHIC PURPOSES (for photomechanical purposes G03F); PHOTOGRAPHIC PROCESSES, e.g. CINE, X-RAY, COLOUR, STEREO-PHOTOGRAPHIC PROCESSES; AUXILIARY PROCESSES IN PHOTOGRAPHY (photographic processes characterised by the use or manipulation of apparatus classifiable per se in subclass G03B, see G03B; photomechanical production of textured or patterned surfaces G03F; electrophotography, magnetography G03G)
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A photothermographic material that comprises a support having thereon one or more thermally-developable imaging layers comprising a binder and in reactive association, a photosensitive silver halide, a non-photosensitive source of reducible silver ions, and a reducing composition for the non-photosensitive source reducible silver ions. The thermally-developable layers further comprises one or more radiation absorbing compounds that provide a total absorbance of greater than 0.6 and up to and including 3 in the thermally-developable imaging layer(s). These photothermographic materials are independently coated and dried while the material is conveyed at a rate of at least 5 meters per minute.

## Claims

### Claim 1

A method of preparing a photothermographic material, comprising a support having thereon one or more thermally-developable imaging layers comprising a binder and in reactive association, a photosensitive silver halide, a non-photo-sensitive source of reducible silver ions, and a reducing composition for said non-photo-sensitive source of reducible silver ions.
wherein said one or more thermally-developable imaging layers further comprise one or more radiation absorbing substances that provide a total absorbance in said one or more thermally-developable imaging layers of greater than 0.6 and up to and including 3 at an exposure wavelength, comprising the steps of:
A) preparing a formulation or formulations comprising a binder and in reactive association, a photosensitive silver halide, a non-photosensitive source of reducible silver ions, a reducing composition for said non-photosensitive source reducible silver ions, and a radiation absorbing compound or compounds that absorb at an exposure wavelength,
B) independently coating said formulations on a support in a manner such that, at the exposure wavelength, the total absorbance of all thermally-developable imaging layers is greater than 0.6, and drying them while said material is conveyed at a rate of at least 5 meters per minute.

### Claim 2 (depends on 1)

The method of claim 1 wherein the one or more thermally-developable imaging layers have been independently coated and dried while said material is conveyed at a rate of at least 25 meters per minute.

### Claim 3

A method of reducing mottle in a photothermographic material, comprising the steps of:
A) preparing a formulation or formulations comprising a binder and in reactive association, a photosensitive silver halide, a non-photosensitive source of reducible silver ions, a reducing composition for said non-photosensitive source reducible silver ions, and a radiation absorbing compound or compounds that absorb at an exposure wavelength,
B) coating said formulations on a support in a manner such that, at the exposure wavelength, the total absorbance of all thermally-developable imaging layers is greater than 0.6.

### Claim 4 (depends on 3)

The method of claim 3 wherein said one or more thermally-developable imaging layers have been independently coated and dried while said material is conveyed at a rate of at least 25 meters per minute.

### Claim 5

A photothermographic material that comprises a support having thereon one or more thermally-developable imaging layers comprising a binder and in reactive association, a photosensitive silver halide, a non-photo-sensitive source of reducible silver ions, and a reducing composition for said non-photosensitive source of reducible silver ions,
wherein said one or more thermally-developable imaging layers further comprise one or more radiation absorbing substances that provide a total absorbance in said one or more thermally-developable imaging layers of greater than 0.6 and up to and including 3 at an exposure wavelength,
wherein said one or more radiation absorbing compounds are represented by the following Structure I:
wherein V1 and V2 independently represent the non-metallic atoms necessary to form substituted or unsubstituted 5-, 6-, or 7-membered heterocyclic rings, P15 and P16 independently represent alkyl, aryl, alkaryl, or heterocyclyl groups, P1, P2, P3, P4, P5, P6, P7, P8, P9, P11, P12, P13, and P14 independently represent methine groups or substituted methine groups that may optionally form a ring with one or more other methine groups or with an auxochrome, s1, s2, s3, s4, s5, and s6 are independently equal to 0 or 1, X is an electric charge neutralizing counterion, and k2 is an integer inclusive of 0 necessary to neutralize an electric charge in the molecule, and
wherein one or more of said substituted methine groups represented by P1, P2, P3, P4, P5, P6, P7, P8, and P9 are substituted with a substituted or unsubstituted heterocyclic ring group comprising up to 6 ring atoms.

### Claim 6 (depends on 5)

The photothermographic material of claim 5 wherein said one or more radiation absorbing substances is chosen from one or more of the following compounds:

### Claim 7

A photothermographic material that comprises a support having thereon one or more thermally-developable imaging layers comprising a binder and in reactive association, a photosensitive silver halide, a non-photo-sensitive source of reducible silver ions, and a reducing composition for said non-photosensitive source of reducible silver ions,
wherein said one or more thermally-developable imaging layers further comprise one or more radiation absorbing substances that provide a total absorbance in said one or more thermally-developable imaging layers of greater than 0.6 and up to and including 3 at an exposure wavelength,
wherein said one or more radiation absorbing compounds are represented by the following Structure I:
wherein V1 and V2 independently represent the non-metallic atoms necessary to form substituted or unsubstituted 5-, 6-, or 7-membered heterocyclic rings, P15 and P16 independently represent alkyl, aryl, alkaryl, or heterocyclyl groups, P1, P2, P3, P4, P5, P6, P7, P8, P9, P11, P12, P13, and P14 independently represent methine groups or substituted methine groups that may optionally form a ring with one or more other methine groups or with an auxochrome, s1, s2, s3, s4, s5, and s6 are independently equal to 0 or 1, X is an electric charge neutralizing counterion, and k1 is an integer inclusive of 0 necessary to neutralize an electric charge in the molecule, and
wherein the total of s1, s2, s3, and s6 is 3 to provide a heptamethine linkage.