# US 6,730,458 B1 · Method for forming fine patterns through effective glass transition temperature reduction

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,458 B1
- Document ID: US6730458B1
- Status: Granted
- Kind: B1
- Application number: 10/376,604
- Filed: 2003-03-03
- Granted: 2004-05-04
- Earliest claimed: 2003-03-03
- Assignees: Samsung Electronics Co., Ltd.
- Inventors: Hyunwoo Kim; Sanggyun Woo
- Web page: https://patentgrep.com/patent/US6730458B1

## CPC

- G03F 7/40: Treatment after imagewise removal, e.g. baking
- Y10S 430/143: Electron beam
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A method for forming fine patterns, particularly contact holes, on semiconductor devices by forming an ArF resist pattern and then reducing the size of pattern openings by exposing the resist pattern to radiation from an VUV (vacuum ultraviolet) excimer laser or E-beam radiation during thermal treatment to reduce, temporarily, the Tg of the resist pattern and allow it to flow, thereby reducing the size of the spaces and openings in the pattern.

## Claims

### Claim 1

A method of forming a fine pattern on a substrate comprising:
forming a photoresist layer on the substrate, the photoresist being adapted for exposure by UV radiation of wavelength W1 and having a glass transition temperature Tg and a decomposition temperature Td;
exposing portions of the photoresist layer with the UV radiation to form an exposed photoresist layer with exposed portions and unexposed portions;
developing the exposed photoresist layer to form a first photoresist pattern, the first photoresist pattern having an opening having a critical dimension d1; and
exposing the first photoresist pattern to VUV radiation of wavelength W2 thereby temporarily producing an effective glass transition temperature Tgeff wherein Tgeff<Tg while simultaneously heating the first photoresist pattern to a temperature at or above the Tgeff to produce a second photoresist pattern in which the opening has a critical dimension d2, wherein d2<d1.

### Claim 2 (depends on 1)

A method of forming a fine pattern on a substrate according to claim 1, further comprising:
baking the exposed photoresist layer at a temperature below Td before developing the exposing photoresist layer.

### Claim 3 (depends on 1)

A method of forming a fine pattern on a substrate according to claim 1, wherein developing the exposed photoresist layer further comprises:
wetting the exposed photoresist layer with an alkaline solution to dissolve the exposed portions of the exposed photoresist layer; and
removing the alkaline solution and the dissolved portion of the exposed photoresist layer from the substrate.

### Claim 4 (depends on 3)

A method of forming a fine pattern on a substrate according to claim 3, wherein the alkaline solution is an aqueous solution of tetramethylammonium hydroxide.

### Claim 5 (depends on 4)

A method of forming a fine pattern on a substrate according to claim 4, wherein the alkaline solution comprises between 0.1 and 10 weight percent tetramethylammonium hydroxide (TMAH).

### Claim 6 (depends on 5)

A method of forming a fine pattern on a substrate according to claim 5, wherein the aqueous solution also includes at least one additive selected from a group consisting of alcohols and surfactants.

### Claim 7 (depends on 6)

A method of forming a fine pattern on a substrate according to claim 6, wherein
a total quantity of all additives is less than 5 weight percent of the aqueous solution and
tetramethylammonium hydroxide is present in the solution in an amount between about 2 and about 2.5 weight percent.

### Claim 8 (depends on 2)

A method of forming a fine pattern on a substrate according to claim 2, wherein:
the photoresist layer is a photoresist selected from a group consisting of KrF photoresists, ArF photoresists and F2 photoresists;
the UV radiation wavelength W1 is selected from the group consisting of 248 nm, 193 nm and 157 nm; and
the VUV radiation wavelength W2 is selected from the group consisting of 172 nm, 146 nm and 126 nm.

### Claim 9 (depends on 8)

A method of forming a fine pattern on a substrate according to claim 8, wherein:
Tg−Tgeff≧20° C.; and
W1>W2.

### Claim 10 (depends on 9)

A method of forming a fine pattern on a substrate according to claim 9, wherein:
the VUV radiation is applied at a level of between 0.1 and 100 J/cm2; and
Tgeff≦100° C.

### Claim 11 (depends on 2)

A method of forming a fine pattern on a substrate according to claim 2, wherein:
Td<Tg.

### Claim 12

A method of forming a fine pattern on a substrate comprising:
forming a photoresist layer on the substrate, the photoresist being adapted for exposure by UV radiation having a wavelength of less than 250 nm, the photoresist also having a decomposition temperature Td and a glass transition temperature Tg;
exposing portions of the photoresist layer with UV radiation having a wavelength of less than 250 nm to form an exposed photoresist layer having exposed portions and unexposed portions;
developing the exposed photoresist layer to form a first photoresist pattern, the first photoresist pattern having an opening having a critical dimension d1; and
exposing the first photoresist pattern to E-beam radiation, the E-beam radiation temporarily producing an effective glass transition temperature Tgeff wherein Tgeff<Tg while simultaneously heating the first photoresist pattern to a temperature at or above the Tgeff to produce a second photoresist pattern in which the opening has a critical dimension d2, wherein d2<d1.

### Claim 13 (depends on 12)

A method of forming a fine pattern on a substrate according to claim 12, further comprising:
baking the exposed photoresist layer at a temperature below Td before developing the exposed photoresist layer.

### Claim 14 (depends on 12)

A method of forming a fine pattern on a substrate according to claim 12, wherein developing the exposed photoresist layer further comprises:
wetting the exposed photoresist layer with an alkaline solution to dissolve exposed portions of the exposed photoresist layer; and
removing the alkaline solution and the dissolved portion of the exposed photoresist layer from the substrate.

### Claim 15 (depends on 13)

A method of forming a fine pattern on a substrate according to claim 13, wherein the alkaline solution comprises an aqueous solution of less than 10 weight percent tetramethylammonium hydroxide.

### Claim 16 (depends on 15)

A method of forming a fine pattern on a substrate according to claim 15, wherein the aqueous solution further comprises at least one additive selected from a group consisting of alcohols, viscosity modifiers and surfactants.

### Claim 17 (depends on 13)

A method of forming a fine pattern on a substrate according to claim 13, wherein:
the photoresist layer comprises a photoresist selected from a group consisting of KrF photoresists, ArF photoresists and F2 photoresists; and
the UV radiation has a wavelength selected from the group consisting of 248 nm, 193 nm and 157 nm.

### Claim 18 (depends on 13)

A method of forming a fine pattern on a substrate according to claim 13, wherein:
Tg−Tgeff≧20° C.

### Claim 19 (depends on 13)

A method of forming a fine pattern on a substrate according to claim 13, wherein:
the E-beam radiation is applied at a level of between 0.1 and 100 J/cm2; and
Tgeff≦100° C.

### Claim 20 (depends on 13)

A method of forming a fine pattern on a substrate according to claim 13, wherein:
Td<Tg.

### Claim 21 (depends on 12)

A method of forming a fine pattern on a substrate according to claim 12, wherein:
the first photoresist pattern is simultaneously exposed to E-beam radiation and VUV radiation having a wavelength not greater than about 172 nm, the E-beam radiation and the VUV radiation cooperating to temporarily produce an effective glass transition temperature Tgeff wherein Tgeff<Tg.