# US 6,730,445 B2 · Attenuated embedded phase shift photomask blanks

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,445 B2
- Document ID: US6730445B2
- Status: Granted
- Kind: B2
- Application number: 10/303,341
- Filed: 2002-11-22
- Published: 2003-10-16
- Granted: 2004-05-04
- Earliest claimed: 2002-04-12
- Assignees: International Business Machines Corporation
- Inventors: Marie Angelopoulos; Katherina Babich; S. Jay Chey; Michael Straight Hibbs; Robert N. Lang; Arpan Pravin Mahorowala; Kenneth Christopher Racette
- Web page: https://patentgrep.com/patent/US6730445B2

## CPC

- G03F 1/32: Attenuating PSM [att-PSM], e.g. halftone PSM or PSM having semi-transparent phase shift portion,; Preparation thereof
- C23C 14/0676: {Oxynitrides}
- C23C 14/08: Oxides (C23C14/10 takes precedence)
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

An attenuating embedded phase shift photomask blank that produces a phase shift of the transmitted light is formed with an optically translucent film made of metal, silicon, nitrogen and oxygen. An etch stop layer is added to improve the etch selectivity of the phase shifting layer. A wide range of optical transmission (0.001% up to 15% at 157 nm) is obtained by this process.

## Claims

### Claim 1

An attenuating phase shift mask blank for use in lithography comprising:
a substrate comprising a quartz or fluorinated quartz material;
an etch stop layer deposited on said substrate comprising a metal selected from groups II, IV, V, transition metals, lanthanides and actinides, said etch stop layer exhibiting improved etch selectivity;
a phase shifting layer disposed on said etch stop layer, the phase shifting layer comprising a composite material of formula AwBxNyOz, where A is an element selected from the group consisting of Groups IVA, VA, or VIA; and B is selected from the group consisting of an element from Groups II, IV, V, the transition metals, the lanthanides and the actinides; wherein w is from about 0.1 to about 0.6, x is from about 0 to about 0.2, y is from about 0 to about 0.6, and z is from about 0 to about 0.7; and
said phase shift mask blank being capable of producing a photomask with substantially 180° phase shift and an optical transmission of at least 0.001% at a selected wavelength of <500 nm, wherein improved stability of said mask blank against irradiation of 157 nm photons is achieved.

### Claim 2 (depends on 1)

An attenuated phase shift mask blank according to claim 1, wherein the phase shifting layer comprises a silicon/titanium/nitrogen/oxygen composite.

### Claim 3 (depends on 2)

An attenuating phase shift mask blank according to claim 2, wherein said silicon/titanium/nitrogen/oxygen composite has structural formula SiwTixNyOz wherein w is about 0.1 to about 0.6, x is from about 0 to about 0.2, y is from about 0 to about 0.6, and z is from about 0 to about 0.7.

### Claim 4 (depends on 1)

An attenuating phase shift mask blank according to claim 1, wherein the phase shifting layer has a thickness of from about 400 Å to about 2000 Å.

### Claim 5 (depends on 1)

An attenuated phase shift mask blank according to claim 1, wherein the etch stop layer comprises a composite material where the composite material comprises a material selected from the group consisting of a metal, an element from Groups II, IV, and V, Nitrogen and Oxygen.

### Claim 6 (depends on 5)

An attenuated phase shift mask blank according to claim 5, wherein the etch stop layer comprises a material selected from the group consisting of titanium and tantalum.

### Claim 7 (depends on 5)

An attenuating phase shift mask blank according to claim 5, wherein the etch stop layer has a thickness of from about 50 Å to about 500 Å.

### Claim 8 (depends on 1)

An attenuating phase shift mask blank according to claim 1, wherein the phase shifting layer is SiTiO and the etch stop layer is Ta.

### Claim 9 (depends on 1)

An attenuating phase shift mask blank according to claim 1, wherein the phase shifting layer is SiTiO and the etch stop layer is Ti.

### Claim 10 (depends on 1)

An attenuating phase shift mask blank according to claim 1, wherein said etch selectivity is greater than 10:1 with substrates of quartz or fluorinated quartz and at the same time have stable optical transmission against chemical cleaning and irradiation of 157 nm photons.

### Claim 11

A method of fabricating an attenuating phase shift mask blank for use in lithography comprising:
providing a substrate comprising a quartz or fluorinated quartz material;
disposing a thin layer of etch stop layer on said substrate comprising a metal selected from groups II, IV, V, transition metals, lanthanides and actinides, said etch stop layer exhibiting improved etch selectivity;
disposing a layer of phase shifter layer on said etch stop layer, the phase shifting layer comprising a composite material of formula AwBxNyOz, where A is an element selected from the group consisting of Groups IVA, VA, or VIA; and B is selected from the group consisting of an element from Groups II, IV, V, the transition metals, the lanthanides and the actinides; wherein w is from about 0.1 to about 0.6, x is from about 0 to about 0.2, y is from about 0 to about 0.6, and z is from about 0 to about 0.7;
said blank is capable of producing a photomask with 180° phase shift and an optical transmission of at least 0.001% at a selected wavelength of <500 nm, wherein improved stability of said mask blank against irradiation of 157 nm photons is achieved.

### Claim 12 (depends on 11)

A method according to claim 11, wherein the phase shifting layer comprises a material selected from the group consisting of a silicon/titanium/nitrogen composite and a silicon/titanium/nitrogen/oxygen composite.

### Claim 13 (depends on 11)

A method according to claim 11, wherein said silicon/titanium/nitrogen/oxygen composite has structural formula SiwTixNyOz wherein w is from about 0.1 to about 0.6, x from about 0 to about 0.2, y is from about 0 to about 0.6, and z is from about 0 to about 0.7.

### Claim 14 (depends on 11)

A method according to claim 11, wherein the phase shifting film is formed by sputter deposition from two or more targets of different compositions using a technique selected from the group consisting of RF matching network, DC magnetron, AC magnetron, pulsed bipolar DC magnetron and RF diode.

### Claim 15 (depends on 14)

A method according to claim 14, wherein the phase shifting layer is formed by sputter deposition from a target of a composite material (Si1−xTix) wherein x is from about 0 to about 0.5 by a method selected from the group consisting of RF matching network, DC magnetron, AC magnetron, pulsed bipolar DC magnetron, Ion beam assisted deposition, Ion beam sputter deposition and RF diode.

### Claim 16 (depends on 14)

A method to claim 14, wherein the substrate is disposed in a holder which can be either planetary or stationary and/or rotating or non-rotating.

### Claim 17 (depends on 11)

A method according to claim 11, wherein the phase shifting film is formed by sputter deposition from two or more targets of different compositions using a technique selected from the group consisting of RF matching network, DC magnetron, AC magnetron, pulsed bipolar DC magnetron, Ion beam assisted deposition, Ion beam sputter deposition and RF diode.

### Claim 18 (depends on 17)

A method according to claim 17, wherein said two or more targets are selected from the group consisting of SiO2 targets and Ti targets, or (Si1−xTix) targets wherein x is from about 0 to about 0.5 and Ti targets.

### Claim 19 (depends on 17)

A method according to claim 17, wherein the substrate is disposed in a holder which can be either planetary or stationary and/or rotating or non-rotating.

### Claim 20 (depends on 11)

A method according to claim 11, wherein the substrate is annealed at elevated temperature in an atmosphere selected from the group consisting of air, oxygen, a vacuum and a mixture of gases selected from the group consisting of O2, N2, H2, Ar, Kr, Ne, He, O3 and H2O.

### Claim 21 (depends on 11)

A method according to claim 11, wherein said etch selectivity is greater than 10:1 with substrates of quartz or fluorinated quartz and at the same time have stable optical transmission against chemical cleaning and irradiation of 157 nm photons.