# US 6,730,429 B2 · Intermetallic negative electrodes for non-aqueous lithium cells and batteries

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,429 B2
- Document ID: US6730429B2
- Status: Granted
- Kind: B2
- Application number: 10/008,885
- Filed: 2001-11-08
- Published: 2002-05-30
- Granted: 2004-05-04
- Earliest claimed: 2000-11-10
- Assignees: The University of Chicago
- Inventors: Michael M. Thackeray; John T. Vaughey; Christopher S. Johnson; Linda M. L. Fransson; Ester Kristina Edstrom; Gary Henriksen
- Web page: https://patentgrep.com/patent/US6730429B2

## CPC

- H01M 4/40: Alloys based on alkali metals
- H01M 4/38: of elements or alloys
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 4/405: {Alloys based on lithium}
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 10/446: {Initial charging measures}
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method of operating an electrochemical cell is disclosed. The cell has an intermetallic negative electrode of Cu6-xMxSn5, wherein x is ≦3 and M is one or more metals including Si and a positive electrode containing Li in which Li is shuttled between the positive electrode and the negative electrode during charge and discharge to form a lithiated intermetallic negative electrode during charge. The voltage of the electrochemical cell is controlled during the charge portion of the charge-discharge cycles so that the potential of the lithiated intermetallic negative electrode in the fully charged electrochemical cell is less than 0.2 V but greater than 0 V versus metallic lithium.

## Claims

### Claim 1

A method of operating an electrochemical cell through a plurality of charge-discharge cycles, said electrochemical cell including an intermetallic negative electrode of Cu6-xMxSn5, wherein x is ≦3 and M is one or more metals including Si and a positive electrode containing Li in which said electrochemical cell Li is shuttled between the positive electrode and the negative electrode during charge and discharge to form a lithiated intermetallic negative electrode during charge comprising the step of controlling the voltage of the electrochemical cell during the charge portion of the charge-discharge cycles so that the potential of the lithiated intermetallic negative electrode in the fully charged electrochemical cell is less than 0.2 V but greater than 0 V versus metallic lithium.

### Claim 2 (depends on 1)

The method of claim 1, wherein x is ≦1.

### Claim 3 (depends on 1)

The method of claim 1, wherein M is one or more of a transition metal or Si or Li.

### Claim 4 (depends on 1)

The method of claim 1, wherein M is one or more of Mn, Fe, Zn and Ni.

### Claim 5 (depends on 1)

The method of claim 1, wherein the ratio of Cu and M atoms to Sn atoms in the negative electrode Cu6-xMxSn5 structure is between about 1.5:1 and 1.0:1 when the cell is fully charged.

### Claim 6 (depends on 1)

The method of claim 1, wherein the negative electrode contains greater than stoichiometric quantities of Cu and M.

### Claim 7 (depends on 6)

The method of claim 6, wherein either or both of Cu and M are present in amounts greater than stoichiometric up to about 10% by weight.

### Claim 8 (depends on 1)

The method of claim 1, wherein the negative electrode contains a grain growth inhibitor.

### Claim 9 (depends on 8)

The method of claim 8, wherein the grain growth inhibitor is carbon or graphite present as a powder.

### Claim 10 (depends on 1)

The method of claim 1, wherein the Cu and M atoms in the negative electrode are at least partially disordered.

### Claim 11 (depends on 1)

The method of claim 1, wherein the negative electrode includes a substrate of M as a current collector.

### Claim 12 (depends on 11)

The method of claim 11, wherein the substrate is laminated to the electrode.

### Claim 13 (depends on 11)

The method of claim 11, wherein the current collector is Cu or Ni.

### Claim 14 (depends on 1)

The method of claim 1, wherein the potential of the lithiated negative electrode is maintained above 0 V by controlling the installed capacity of the positive electrode.

### Claim 15 (depends on 1)

The method of claim 1, wherein a microprocessor is connected between the positive and negative electrodes to control the voltage of the cell.

### Claim 16

A method of operating an electrochemical cell through a plurality of charge-discharge cycles, said electrochemical cell including an intermetallic negative electrode of Cu6-xMxSn5, wherein x is ≦3 and M is one or more metals including Si and a non-aqueous electrolyte and a positive electrode containing Li from a source thereof from one or more of LiCoO2, LiNiO2, LiMnO2, LiMn2O4, LiFePO4 or derivatives thereof in which said electrochemical cell Li is shuttled between the positive electrode and the negative electrode during charge and discharge to form a lithiated intermetallic negative electrode during charge, comprising the step controlling the voltage of the electrochemical cell during the charge portion of the charge-discharge cycles so that the potential of the lithiated intermetallic negative electrode in the fully charged electrochemical cell is less than 0.2 V but greater than 0 V versus metallic lithium.

### Claim 17 (depends on 16)

The method of claim 16, wherein the potential of the negative electrode is maintained between about 1.5 V and 0.01 V vs. metallic lithium.

### Claim 18 (depends on 17)

The method of claim 17, wherein the potential of the negative electrode is maintained between about 1.2 V and 0.01 V vs. metallic lithium.

### Claim 19 (depends on 17)

The method of claim 17, wherein the negative electrode is made with up to about 10% by weight more than stoichiometric amounts of Cu and M present as powder.

### Claim 20 (depends on 19)

The method of claim 19, wherein the lithiated negative electrode has a disordered or partially disordered zinc-blende-type structure.