# US 6,730,381 B2 · Intumescent fire-protection strips jacketed on three sides and combined cold- and hot-gas seals

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,381 B2
- Document ID: US6730381B2
- Status: Granted
- Kind: B2
- Application number: 09/798,958
- Filed: 2001-03-06
- Published: 2003-02-20
- Granted: 2004-05-04
- Earliest claimed: 2000-03-07
- Assignees: Intumex Brandschutzprodukte AG
- Inventors: Heinrich Horacek
- Web page: https://patentgrep.com/patent/US6730381B2

## CPC

- C09K 21/14: Macromolecular materials
- Y10S 428/92: Fire or heat protection feature
- Y10S 428/921: Fire or flameproofing
- Y10T 428/1386: Natural or synthetic rubber or rubber-like compound containing
- Y10T 428/161: with frame, casing, or perimeter structure
- Y10T 428/24198: Channel-shaped edge component [e.g., binding, etc.]
- Y10T 428/25: Web or sheet containing structurally defined element or component and including a second component containing structurally defined particles
- Y10T 428/252: Glass or ceramic [i.e., fired or glazed clay, cement, etc.] [porcelain, quartz, etc.]
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Coextruded, intumescent fire-protection strips jacketed on three sides, obtained by coextruding an intumescent composition composed of a thermoplastic elastomer with a processing temperature of not more than 250° C. selected from the class consisting of block copolymers and uncrosslinked thermoplastic polyolefins, sulfuric-acid-treated graphite, flame retardant, and an inorganic additive which forms an enamel or forms a ceramic, and a three-sided jacket, where appropriate in association with a chambered profile, made from a thermoplastic elastomer with a processing temperature of not more than 250° C. selected from the class consisting of block copolymers and uncrosslinked thermoplastic polyolefins, flame retardant, and, where appropriate, a color pigment, where the fire-protection strips may be designed either as a hot-gas seal or else as a combined cold- and hot-gas seal with spatially separated functions.

## Claims

### Claim 1

A coextruded, intumescent fire-protection strip jacketed on three sides and composed of
a) an intumescent composition made from
a1) a thermoplastic elastomer with a processing temperature of not more than 250° C. selected from the group consisting of block copolymers and uncrosslinked thermoplastic polyolefins,
a2) sulfric-acid-treated graphite,
a3) flame retardant, and
a4) an inorganic additive which forms an enamel or forms a ceramic, and
b) a three-sided jacket, optionally in association with a chambered profile, made from
b1) a thermoplastic elastomer with a processing temperature of not more than 250° C. selected from the group consisting of block copolymers and uncrosslinked thermoplastic polyolefins,
b2) flame retardant, and, optionally,
b3) a color pigment,
and obtained by coextrusion of a) and b).

### Claim 2 (depends on 1)

The fire-protection strip as claimed in claim 1, wherein the thermoplastic elastomers a1) and b1) used comprise block copolymers selected from the group consisting of styrene-butadiene-styrene block copolymers, styrene-isoprene-styrene block copolymers and styrene-ethylene-co-butadiene-styrene block copolymers, polyether-polyamide block copolymers, polyurethane-polyether or -polyester block copolymers, polyether-polyester block copolymers, and uncrosslinked thermoplastic polyolefins.

### Claim 3 (depends on 1)

The fire-protection strip as claimed in claim 1, wherein additives selected from the group consisting of impact modifiers, coupling agents, and antioxidants are added to the thermoplastic elastomers.

### Claim 4 (depends on 1)

The fire-protection strip as claimed in claim 1, wherein the proportion of thermoplastic elastomers in the intumescent composition a) and in the jacket b) is from 20 to 80% by weight.

### Claim 5 (depends on 1)

The fire-protection strip as claimed in claim 1, wherein the amount of sulfuric-acid-treated graphite is from 10 to 50% by weight.

### Claim 6 (depends on 1)

The fire-protection strip as claimed in claim 1, wherein the flame retardants a3) and b2) used are nitrogen-phosphorus compounds selected from the group consisting of melamine phosphates, guanidine phosphates, ammonium hydrogenphosphates, ammonium polyphosphates, ammonium trihydrazinophosphates, or are ethylenediammonium phosphate, or are hydroxides, or are hydrates, where the proportion of a3) in the intumescent composition a) is from 1 to 10% by weight, and the proportion of b2) in the jacket is from 10 to 50% by weight.

### Claim 7 (depends on 1)

The fire-protection strip as claimed in claim 1, wherein the inorganic additive a4) which forms an enamel or forms a ceramic comprises neutral metal oxide compounds or neutral metal oxide mixtures selected from the group consisting of clay, kaolin, zinc borate, and calcium phosphate, or feldspar, or is a mixture made from acidic oxides selected from the group consisting of silicon dioxide, boron oxide, and phosphorus oxide with basic oxides selected from the group consisting of potassium oxide, sodium oxide, calcium oxide, aluminum oxide, zinc oxide, titanium oxide, and magnesium oxide, the proportion of a4) being from 5 to 30% by weight.

### Claim 8 (depends on 1)

The fire-protection strip as claimed in claim 1, designed as a combined cold- and hot-gas seal with spatially separated functions, where the three-sided jacket b) has been combined with a chambered profile which serves as cold-gas seal and has the same formulation as the jacket.

### Claim 9 (depends on 1)

The fire-protection strip as claimed in claim 1, which has an expansion factor of from 1:5 to 1:9 at 300° C.

### Claim 10 (depends on 6)

The fire-protection strip as claimed in claim 6, where the hydroxides are magnesium hydroxide or aluminum hydroxide and the hydrate is alumina trihydrate.

### Claim 11 (depends on 9)

The fire-protection strip as claimed in claim 9, having an expansion factor of above 1:5 and up to 1:9 at 300° C.

### Claim 12 (depends on 1)

A process for producing fire-protection strips as claimed in claim 1, which comprises extruding the jacket b) at a processing temperature of not more than 250° C. by way of a single-screw extruder and simultaneously extruding the intumescent composition a) at a processing temperature of not more than 250° C. into the cavity of the jacket by way of a twin-screw extruder, and then using a suitable coextrusion die, composed of a composite head with conically oriented slot dies of various widths, to obtain coextruded, intumescent fire-protection strips jacketed on three sides and having a width of from 10 to 60 mm and a thickness of from 1 to 5 mm, these being polished, where appropriate, by way of a roller take-off system and then wound up.