# US 6,730,368 B1 · Method of preparing a poly-crystalline silicon film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,368 B1
- Document ID: US6730368B1
- Status: Granted
- Kind: B1
- Application number: 09/468,217
- Filed: 1999-12-20
- Granted: 2004-05-04
- Earliest claimed: 1997-09-25
- Assignees: Kabushiki Kaisha Toshiba
- Inventors: Shinichi Kawamura
- Web page: https://patentgrep.com/patent/US6730368B1

## CPC

- H10P 14/24: using chemical vapour deposition [CVD]
- C23C 16/24: Deposition of silicon only
- C23C 16/56: After-treatment
- H10P 14/2922: {being non-crystalline insulating materials, e.g. glass or polymers}
- H10P 14/3238: {being insulating materials}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3816: {Pulsed laser beam}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A method of preparing a poly-crystalline silicon (p-Si) film is provided with efficient dehydrogenation treatment of an amorphous silicon (a-Si) film deposited by a plasma enhanced chemical deposition (PECVD) process. A substrate is received in a process chamber of a PECVD system. A plasma discharge takes place to deposit an a-Si film on the substrate in an atmosphere in which reactive and carrier passes are supplied to the chamber. The substrate is still left in the chamber to carry out dehydrogenation of the a-Si film after the same is deposited on the substrate. While the carrier gas is supplied to the chamber during the leaving period of time, the pressure of the chamber is set higher than during the leaving period of time. The pressure of the chamber is set higher than during the deposition the pressure of the chamber is set higher. After the dehydrogenation treatment, the substrate is taken out from the chamber. XeCl3 excimer laser beams are then used to irradiate the a-Si film to change it into a p-Si film.

## Claims

### Claim 1

A method of preparing a poly-crystalline silicon film comprising:
supplying reactive gases and carrier gases to a process chamber of a plasma chemical deposition system including a substrate;
depositing an amorphous silicon film on the substrate by plasma discharging at a temperature 400° C. or more;
after film deposition, transporting the substrate from the process chamber to a heating chamber attached to the plasma chemical deposition system without exposing the substrate to atmosphere external to the system and holding the substrate in the heating chamber to carry out dehydrogenation treatment of the amorphous silicon film;
removing the substrate from the heating chamber after the dehydrogenation treatment; and
irradiating the amorphous silicon film with a laser beam thereby changing the amorphous silicon film into a poly-crystalline silicon film.

### Claim 2 (depends on 1)

A method according to claim 1, wherein the temperature of the substrate in the heating chamber is higher than that in the process chamber.

### Claim 3 (depends on 1)

A method according to claim 1, wherein the plasma chemical deposition system is a cluster-type plasma chemical deposition system.

### Claim 4 (depends on 1)

A method according to claim 1, wherein the depositing step is carried out with reactive and carrier gases supplied to the process chamber and the dehydrogenation treatment is carried out with the carrier gas supplied to the heating chamber.

### Claim 5 (depends on 1)

A method according to claim 1, wherein the dehydrogenation treatment is carried out without a reactive gas.

### Claim 6 (depends on 1)

A method according to claim 1, wherein irradiating step comprises the step of irradiating with an excimer laser beam.

### Claim 7 (depends on 1)

A method according to claim 1, wherein the dehydrogenation treatment reduces the hydrogen content of the amorphous silicon film to less than 10%.

### Claim 8 (depends on 1)

A method according to claim 1, wherein a period of leaving time t (seconds) of the substrate in the heating chamber, a thickness d (angstroms) of the amorphous silicon film, and a temperature (° C.) of the heating chamber at the time when the substrate is left in the chamber satisfy the following equation (1):
t>d2/(A×exp B) (1)
where
A=6.0×1014,
B=−2.56×10−19/(k×(273+θ)),
and
k=1.38×10−23.

### Claim 9 (depends on 1)

A method according to claim 1, wherein the plasma chemical deposition system is a single substrate processing plasma chemical deposition system.

### Claim 10 (depends on 1)

A method according to claim 1, wherein transporting the substrate to the heating chamber is carried out through a path in a nitrogen or inactive gas atmosphere.

### Claim 11

A method of preparing a thin film transistor comprising:
supplying reactive gases and carrier gases to a process chamber of a plasma chemical deposition system including a substrate;
depositing an amorphous silicon film on the substrate by plasma discharging at a temperature 400° C. or more;
after film deposition, transporting the substrate from the process chamber to a heating chamber attached to the plasma chemical deposition system without exposing the substrate to atmosphere external to the system and holding the substrate in the heating chamber to carry out dehydrogenation treatment of the amorphous silicon film;
removing the substrate from the heating chamber after the dehydrogenation treatment;
irradiating the amorphous silicon film with a laser beam thereby changing the amorphous silicon film into a poly-crystalline silicon film; and
forming a thin film transistor including the poly-crystalline silicon as an active semiconductor layer.

### Claim 12

A method of preparing an active-matrix type liquid crystal display device comprising:
supplying reactive gases and carrier gases to a process chamber of a plasma chemical deposition system including a substrate;
depositing an amorphous silicon film on the substrate by plasma discharging at a temperature 400° C. or more;
after film deposition, transporting the substrate from the process chamber to a heating chamber attached to the plasma chemical deposition system without exposing the substrate to atmosphere external to the system and holding the substrate in the heating chamber to carry out dehydrogenation treatment of the amorphous silicon film;
removing the substrate from the heating chamber after the dehydrogenation treatment;
irradiating the amorphous silicon film with a laser beam thereby changing the amorphous silicon film into a poly-crystalline silicon film; and
forming an active-matrix type liquid crystal display device including a thin film transistor formed from the poly-crystalline silicon as an active semiconductor layer.