# US 6,730,365 B2 · Method of thin film deposition under reactive conditions with RF or pulsed DC plasma at the substrate holder

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,365 B2
- Document ID: US6730365B2
- Status: Granted
- Kind: B2
- Application number: 10/066,329
- Filed: 2002-01-31
- Published: 2002-08-08
- Granted: 2004-05-04
- Earliest claimed: 2001-02-06
- Inventors: Carlo Misiano; Hans K. Pulker
- Web page: https://patentgrep.com/patent/US6730365B2

## CPC

- C23C 14/0021: {Reactive sputtering or evaporation}
- C23C 14/32: by explosion; by evaporation and subsequent ionisation of the vapours {, e.g. ion-plating}(C23C14/34 - C23C14/48 take precedence)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

Method of thin film deposition especially in reactive conditions. Optical coatings with negligible optical absorption, of high quality and low cost even on unheated substrates are deposited using an RF/pulsed DC plasma RF/pulsed DC bias generates a plasma in front of the substrate. This plasma allows obtaining the right stoichiometry of the deposited film by increasing the reactivity of the reactive gas present in the plasma and, in addition, introduces an energetic ion bombardment of the substrate before and during the growth of the film which improves the adherence and the deposit compactness.

## Claims

### Claim 1

A method of applying a thin film coating to a substrate, comprising the steps of:
(a) mounting a substrate to be coated on a substrate holder in an evacuatable chamber and so that said substrate is spacedly juxtaposed with a crucible containing a component of a coating to be applied to said substrate;
(b) evacuating said chamber;
(c) positioning a shutter between said crucible and said substrate and heating said component in said crucible with a high energy electron beam;
(d) admitting a gas mixture to said chamber containing at least one gas reactive with said component to form said coating;
(e) connecting said substrate holder to a radio frequency or pulsed direct current source so that said substrate holder is poled cathodic and a plasma is formed at least around said substrate to create a self bias of several hundreds of volts on said substrate holder and a surface of said substrate is bombarded with particles from the plasma;
(f) withdrawing said shutter from its position between said crucible and said substrate, bombarding said component with low energy electrons from a low-energy electron source independent of said high energy electron beam to ionize said component at least in part and depositing a reaction product of said component and said at least one gas on said substrate; and
(g) controlling the ionization of said component so that said self bias is reduced by at least 50%.

### Claim 2 (depends on 1)

The method defined in claim 1 wherein said self bias and said plasma are produced by connecting said substrate holder to a radio frequency source.

### Claim 3 (depends on 2)

The method defined in claim 2 wherein the deposition of said coating is monitored and the coating is terminated when a predetermined thickness of the coating is reached.

### Claim 4 (depends on 1)

The method defined in claim 1 wherein said thin film coating is an optical coating.

### Claim 5 (depends on 1)

The method defined in claim 1, further comprising the step of depositing a reaction product of a component from another crucible and said at least one gas on said substrate following the deposition of said coating thereon.

### Claim 6 (depends on 1)

The method defined in claim 1, further comprising the step of directing another electron beam from an electron beam gun onto said component in said crucible.

### Claim 7

A method of applying a thin film coating to a substrate, comprising the steps of:
(a) mounting a substrate to be coated on a substrate holder in an evacuatable chamber and so that said substrate is spacedly juxtaposed with a crucible containing a component of a coating to be applied to said substrate;
(b) evacuating said chamber;
(c) positioning a shutter between said crucible and said substrate and heating said component in said crucible with a high energy electron beam;
(d) admitting a gas mixture to said chamber;
(e) connecting said substrate holder to a radio frequency or pulsed direct current source so that said substrate holder is poled cathodic and a plasma is formed at least around said substrate to create a self bias of several hundreds of volts on said substrate holder and a surface of said substrate is bombarded with particles from the plasma;
(f) withdrawing said shutter from its position between said crucible and said substrate, bombarding said component with low energy electrons to ionize said component at least in part and depositing said component and said at least one gas on said substrate; and