# US 6,730,364 B2 · Preparation of carbon molecular sieve membranes on porous substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,364 B2
- Document ID: US6730364B2
- Status: Granted
- Kind: B2
- Application number: 10/107,142
- Filed: 2002-03-28
- Published: 2003-10-02
- Granted: 2004-05-04
- Earliest claimed: 2002-03-28
- Assignees: National Science Council
- Inventors: Franklin Chau-Nan Hong; Liang-Chun Wang; Yoou-Bin Guo
- Web page: https://patentgrep.com/patent/US6730364B2

## CPC

- B01D 67/0072: {by deposition from the gaseous phase, e.g. sputtering, CVD, PVD}
- B01D 71/021: {Carbon}
- C23C 16/045: {Coating cavities or hollow spaces, e.g. interior of tubes; Infiltration of porous substrates}
- C23C 16/26: Deposition of carbon only
- C23C 16/56: After-treatment
- B01D 2323/08: Specific temperatures applied
- B01D 2323/12: Specific ratios of components used
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A method for preparing carbon molecular sieve membrane is invented. A thin carbon-containing film is first deposited on a porous substrate. The thin film is then bombarded by high energy ions for surface modification. The surface modified film is then baked or calcined at a high temperature. The carbon molecular sieve membrane prepared according to the present invention can be used for gas separation as well as liquid separation, ions or solvents, etc., exhibiting improved permeance and improved selectivity simultaneously in gas separation. The ion bombardment includes generating plasma and ions in a gas phase, and applying a negative bias voltage to the substrate.

## Claims

### Claim 1

A process for preparing a carbon molecular sieve membrane comprising the following steps:
(a) growing an amorphous carbon-based membrane on a porous substrate at a low temperature, where said membrane is able to be pyrolyzed or decomposed at a temperature higher than the growth temperature;
(b) performing a surface modification by bombarding said membrane with energized gaseous ions; and
(c) baking said surface-modified membrane at a temperature higher than the growth temperature in Step (a), so that a membrane having a gas separation effect is formed.

### Claim 2 (depends on 1)

The process according to claim 1, wherein said amorphous carbon-based membrane comprises carbon as a major portion thereof and, optionally, elements selected from the group consisting of Al, Si, O, N, P and F.

### Claim 3 (depends on 1)

The process according to claim 1, wherein said surface modification by bombarding the membrane with energized gaseous ions is carried out with a means selected from means for generating plasma, laser or ion beams, wherein a negative bias voltage is applied to said porous substrate, or an ion gun or an ion implantation device is used to accelerate ions.

### Claim 4 (depends on 3)

The process according to claim 3, wherein said surface modification is carried out by: bombarding said membrane with energized gaseous ions at a pressure less than 105 Pa and with an ion acceleration bias voltage less than 5000 volts.

### Claim 5 (depends on 1)

The process according to claim 1, wherein said baking is carried out at a pressure of 0.001 Pa-2×105 Pa, in an environment of vacuum, N2 or an inert gas, and for a period of time up to 100 hours.

### Claim 6 (depends on 1)

The process according to claim 1 further comprising repeating Steps (a), (b) and (c) one or more cycles, thereby further improving the separation effect of the membrane.

### Claim 7 (depends on 1)

The process according to claim 1, wherein said growth of said amorphous carbon-based membrane in Step (a) comprises using an inductively-coupled-plasma chemical vapor deposition (ICP CVD) to grow said membrane on said porous substrate under conditions comprising a gas phase pressure of 10−3-100 torr; a reaction gas mixture comprising 5-100 vol. % of a carbon-containing gas, and 95-0 vol. % of O2 or an oxygen-containing gas; a total flowrate of 0.5-10 sccm; RF high frequency power of 20-1000 W; and a processing time of 0.1-20 hours.

### Claim 8 (depends on 7)

The process according to claim 7, wherein said carbon-containing gas is hexamethyldisiloxane (HMDSO) or methane.

### Claim 9 (depends on 7)

The process according to claim 7, wherein said reaction gas mixture comprises 5-95 vol. % of said carbon-containing gas, and 95-5 vol. % of O2.

### Claim 10 (depends on 7)

The process according to claim 7, wherein said surface modification by bombarding said membrane with energized gaseous ions in Step (b) is carried out by means of an inductively-coupled-plasma chemical vapor deposition and applying a negative bias voltage to said porous substrate, wherein conditions of generating plasma comprise a gas pressure of 10−3-100 torr; a gas composition comprising 5-100 vol. % of a carbon-containing gas, 95-0 vol. % of O2 or an oxygen-containing gas, and 95-0 vol. % of an inert gas; a total gas flowrate of 0.5-10 sccm; RF high frequency power of 20-1000 W; and a processing time of 1-1000 second.

### Claim 11 (depends on 10)

The process according to claim 10, wherein said carbon-containing gas is hexamethyldisiloxane (HMDSO) or methane.

### Claim 12 (depends on 10)

The process according to claim 10, wherein said gas composition comprises 5-100 vol. % of said carbon-containing gas, and 95-0 vol. % of O2.

### Claim 13 (depends on 12)

The process according to claim 12, wherein said carbon-containing gas is hexamethyldisiloxane (HMDSO).

### Claim 14 (depends on 10)

The process according to claim 10, wherein said gas composition comprises 5-100 vol. % of said carbon-containing gas, and 95-0 vol. % of said inert gas.

### Claim 15 (depends on 14)

The process according to claim 14, wherein said carbon-containing gas is hexamethyldisiloxane (HMDSO).

### Claim 16 (depends on 10)

The process according to claim 10, wherein said processing time is of 3-30 seconds.

### Claim 17 (depends on 16)

The process according to claim 16, wherein said negative bias voltage is of 10-100 volts.

### Claim 18 (depends on 10)

The process according to claim 10, wherein said negative bias voltage is of 10-100 volts.

### Claim 19 (depends on 1)

The process according to claim 1, wherein said surface modification by bombarding said membrane with energized gaseous ions in Step (b) is carried out by means of an inductively-coupled-plasma chemical vapor deposition and applying a negative bias voltage to said porous substrate, wherein conditions of generating plasma comprise a gas pressure of 10−3-100 torr; a gas composition comprising 5-100 vol. % of a carbon-containing gas, 95-0 vol. % of O2 or an oxygen-containing gas, and 95-0 vol. % of an inert gas; a total gas flowrate of 0.5-10 sccm; RF high frequency power of 20-1000 W; and a processing time of 1-1000 second.

### Claim 20 (depends on 19)

The process according to claim 19, wherein said carbon-containing gas is hexamethyldisiloxane (HMDSO) or methane.

### Claim 21 (depends on 19)

The process according to claim 19, wherein said gas composition comprises 5-100 vol. % of said carbon-containing gas, and 95-0 vol. % of O2.

### Claim 22 (depends on 21)

The process according to claim 21, wherein said carbon-containing gas is hexamethyldisiloxane (HMDSO).

### Claim 23 (depends on 19)

The process according to claim 19, wherein said gas composition comprises 5-100 vol. % of said carbon-containing gas, and 95-0 vol. % of said inert gas.

### Claim 24 (depends on 23)

The process according to claim 23, wherein said carbon-containing gas is hexamethyldisiloxane (HMDSO).

### Claim 25 (depends on 19)

The process according to claim 19, wherein said processing time is of 3-30 seconds.

### Claim 26 (depends on 25)

The process according to claim 25, wherein said negative bias voltage is of 10-100 volts.

### Claim 27 (depends on 19)

The process according to claim 19, wherein said negative bias voltage is of 10-100 volts.