# US 6,730,248 B2 · Foamed article of thermoplastic resin composition and process for producing it

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,248 B2
- Document ID: US6730248B2
- Status: Granted
- Kind: B2
- Application number: 09/988,596
- Filed: 2001-11-20
- Published: 2003-01-23
- Granted: 2004-05-04
- Earliest claimed: 2001-07-05
- Assignees: Mitsui Chemicals, Inc.
- Inventors: Hideo Akimoto; Mitsuru Watari; Takashi Miyazaki; Tatsuji Kawamura
- Web page: https://patentgrep.com/patent/US6730248B2

## CPC

- B29C 44/086: {and feeding more material into the enlarged cavity}
- Y10T 428/249987: With nonvoid component of specified composition
- Y10T 428/249988: Of about the same composition as, and adjacent to, the void-containing component
- Y10T 428/249989: Integrally formed skin
- Y10T 428/249991: Synthetic resin or natural rubbers
- Y10T 428/249992: Linear or thermoplastic
- Y10T 428/249993: Hydrocarbon polymer
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A process is provided for producing a foamed article of a thermoplastic resin composition having a relatively thicker solid skin layer exhibiting better appearance without occurrence of a swirl mark and having a foam structure of relatively uniform foam cell size with better foam cell configuration, which is light-weighing and superior in stiffness, in an easy and efficient manner, by causing the resin composition to foam up in a cavity of a mold.

## Claims

### Claim 1

A process for producing a foamed article of a thermoplastic resin composition by causing the resin composition to foam up in a cavity of a mold, comprising
a primary injection step in which a part amount of the thermoplastic resin composition is injected into the mold cavity defined by a stationary mold element and a movable mold element settled at a position confining the mold cavity to a smaller volume than the total volume of the thermoplastic resin composition necessary for making up the complete foamed article, while imposing a clamping pressure on the movable mold element so as to settle it at the position,
a secondary injection step, subsequent to the primary injection step, in which the residual amount of the thermoplastic resin composition is further injected into the mold cavity, while drawing the movable mold element back from the position settled for the primary injection step so as to increase the cavity volume, and
a foaming step subsequent to the secondary injection step, in which injection of the thermoplastic resin composition is stopped and the movable mold element is further drawn back so as to permit the thermoplastic resin composition to foam up,
wherein the thickness L0 of the mold cavity at the start of the primary injection step is in the range from 1.0 to 1.5 mm, the injection time of the primary injection step is 1.5 seconds or less and the pressure imposed on the movable mold element in the primary injection step is in the range from 5 to 20 MPa with respect to the sectional area of the mold cavity in the projection onto the mold base plane and wherein
the ratio of the thickness L0 of the mold cavity at the start of the primary injection step relative to the thickness L1 at the end of the secondary injection step, namely, L0/L1, is in the range from 0.3 to 1.0.

### Claim 2 (depends on 1)

The process of claim 1, wherein the drawing back of the movable mold element during the foaming step begins within 5 seconds from the termination of the secondary injection step.

### Claim 3 (depends on 1)

The process of claim 1, further comprising compressing the foamed article by pressing the movable mold element onto the foamed article within 60 seconds from the termination of the foaming step.

### Claim 4 (depends on 2)

The process of claim 2, further comprising compressing the foamed article by pressing the movable mold element onto the foamed article within 60 seconds from the termination of the foaming step.

### Claim 5 (depends on 1)

The process of claim 1, wherein the thermoplastic resin composition comprises a polyolefin resin and a foaming agent.

### Claim 6 (depends on 4)

The process of claim 4, wherein the thermoplastic resin composition comprises a polyolefin resin and a foaming agent.

### Claim 7 (depends on 5)

The process of claim 5 wherein the polyolefin resin is a polypropylene resin.

### Claim 8 (depends on 6)

The process of claim 6 wherein the polyolefin resin is a polypropylene resin.

### Claim 9 (depends on 5)

The process of claim 5, wherein the polyolefin resin has a melt flow rate, determined according to ASTM D 1238 at 230° C. under a load of 2.16 kg, in the range of from 30 to 200 g/10 mm.

### Claim 10 (depends on 6)

The process of claim 6, wherein the polyolefin resin has a melt flow rate, determined according to ASTM D 1238 at 230° C. under a load of 2.16 kg, in the range of from 30 to 200 g/10 mm.