# US 6,730,243 B2 · Cesium halide storage phosphor with narrow emission spectrum upon UV-excitation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,243 B2
- Document ID: US6730243B2
- Status: Granted
- Kind: B2
- Application number: 09/995,561
- Filed: 2001-11-28
- Published: 2003-06-05
- Granted: 2004-05-04
- Earliest claimed: 2000-12-22
- Assignees: Afga-Gevaert Aktiengesellschaft
- Inventors: Paul Leblans; Luc Struye
- Web page: https://patentgrep.com/patent/US6730243B2

## CPC

- G21K 4/00: Conversion screens for the conversion of the spatial distribution of X-rays or particle radiation into visible images, e.g. fluoroscopic screens (photographic processes using X-ray intensifiers G03C5/17; discharge tubes comprising luminescent screens H01J1/62; cathode ray tubes for X-ray conversion with optical output H01J31/50)
- C09K 11/7733: {with alkali or alkaline earth metals}
- G21K: HANDLING OF PARTICLES OR IONISING RADIATION NOT OTHERWISE PROVIDED FOR; IRRADIATION DEVICES; GAMMA RAY OR X-RAY MICROSCOPES
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

A CsBr:Eu phosphor showing a narrow emission spectrum upon UV-excitation and panels including such a phosphor are disclosed. Also methods for preparing such a phosphor have been described.

## Claims

### Claim 1

A CsBr:Eu phosphor showing upon excitation with light of 370 nm at a wavelength of λmax a maximum emission intensity I0 and at λmax +30 nm an emission intensity I, such that I≦0.20 I0.

### Claim 2 (depends on 1)

A CsBr:Eu phosphor according to claim 1, wherein I≦0.15 I0.

### Claim 3 (depends on 1)

A CsBr:Eu phosphor according to claim 1, wherein Eu has been introduced using a europium compound containing an halogen atom.

### Claim 4 (depends on 1)

A CsBr:Eu phosphor according to claim 1, wherein during the preparation of said phosphor an “annealing step” is introduced.

### Claim 5

A method for preparing a CsBr:Eu phosphor comprising the steps of:
mixing or combining CsBr with between 10−3 mol % and 5 mol % of a europium compound wherein said europium compound is a member selected from the group consisting of EuX′2 EuX′3 and EuOX′, X′ being selected from the group consisting of F, Cl, Br, I and combinations thereof,
heating said mixture at a temperature above 450° C.;
cooling said mixture to room temperature,
bringing said mixture after cooling to a temperature between 80 and 220° C. and
maintaining said mixture at that temperature for a time between 10 minutes and 15 hours.

### Claim 6

A method for preparing a CsBr:Eu phosphor comprising the steps of:
mixing or combining CsBr with between 10−3 mol % and 5 mol % of a europium compound wherein said europium compound is a member selected from the group consisting of EuX′2 EuX′3 and EuOX′, X′ being selected from the group consisting of F, Cl, Br, I and combinations thereof,
heating said mixture at a temperature above 450° C.; cooling said mixture to a temperature between 80 and 220° C. maintaining said mixture at that temperature for between 10 minutes and 15 hours; and
cooling said mixture to room temperature.

### Claim 7

A method for producing a binderless CsBr:Eu phosphor screen comprising the steps of:
mixing or combining CsBr with between 10−3 mol % and 5 mol % of a europium compound wherein said europium compound is a member selected from the group consisting of EuX′2 EuX′3 and EuOX′, X′being selected from the group consisting of F, Cl, Br, I and combinations thereof,
vapour depositing that mixture onto a substrate, forming a binderless phosphor screen,
cooling said phosphor screen to room temperature,
bringing said phosphor screen to a temperature between 80 and 220° C. and
maintaining it at that temperature for between 10 minutes and 15 hours.

### Claim 8

A method for preparing a binderless CsBr:Eu phosphor screen comprising the steps of:
mixing or combining CsBr with between 10−3 mol% and 5 mol% of a europium compound wherein said europium compound is a member selected from the group selected from EuX′2, EuX′3 and EuOX′, X′ being selected from the group consisting of F, Cl, Br, I and combinations thereof,
vapor depositing that mixture onto a substrate, forming a binderless phosphor screen;
cooling said screen to a temperature between 80 and 220° C.;
maintaining it at that temperature for between 10 minutes and 15 hours; and
cooling said screen to room temperature.