# US 6,730,182 B2 · Method for vibrating, melting and bonding resin parts

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,182 B2
- Document ID: US6730182B2
- Status: Granted
- Kind: B2
- Application number: 10/056,134
- Filed: 2002-01-24
- Published: 2002-08-01
- Granted: 2004-05-04
- Earliest claimed: 2001-01-30
- Assignees: Denso Corporation
- Inventors: Yasuhiko Yamazaki; Takayuki Shibata; Syuuji Murata; Akihiro Yada; Ryouji Iwamatsu
- Web page: https://patentgrep.com/patent/US6730182B2

## CPC

- B29C 66/53461: {joining substantially flat covers and/or substantially flat bottoms to open ends of container bodies}
- B29C 65/06: using friction, e.g. spin welding {(non-plastics elements to plastic elements B29C65/645)}
- B29C 65/069: {the welding tool cooperating with specially formed features of at least one of the parts to be joined, e.g. cooperating with holes or ribs of at least one of the parts to be joined}
- B29C 66/112: {Single lapped joints}
- B29C 66/114: {Single butt joints}
- B29C 66/24244: {forming a rectangle}
- B29C 66/30223: {said melt initiators being rib-like}
- B29C 66/82261: {Wedges}
- B29C 66/8322: {Joining or pressing tools reciprocating along one axis}
- B29C 66/92443: {following a pressure-time profile}
- B29C 66/92615: {the gap being non-constant over time}
- B29C 66/92921: {in specific relation to time, e.g. pressure-time diagrams}
- B29C 66/93441: {the speed being non-constant over time}
- B29C 66/9512: {by controlling their vibration frequency}
- B29C 66/9516: {by controlling their vibration amplitude}
- B29C 66/954: {by measuring or controlling the thickness of the parts to be joined}
- B29C 66/961: {involving a feedback loop mechanism, e.g. comparison with a desired value}
- B29C 66/9231: {by measuring the displacement of the joining tools}
- B29C 66/949: {characterised by specific time values or ranges}
- B29C 66/9513: {characterised by specific vibration frequency values or ranges}
- B29C 66/9517: {characterised by specific vibration amplitude values or ranges}
- B29C 66/9592: {in explicit relation to another variable, e.g. X-Y diagrams}
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)

## Abstract

The present invention provides a method for vibrating, melting and creating well-bonded resin parts. Pressing the resin parts is started and then the pressing force is increased sharply to a predetermined value and the resin parts are vibrated to heat the resin part contact surfaces. After heat generation is started, the pressing force is increased gradually to a time, when the vibrating of the resin parts is finished, to push out the heated resin material from the contact surfaces. This exposes the new surface of the resin material which is heated at a low degree and thus can prevent the resin material at the contact surface from excessive heat and degradation. Thereafter, the vibration of the resin parts is stopped to solidify the resin material which is not degraded and is in a uniform, melted state throughout the contact surfaces.

## Claims

### Claim 1

A method for vibrating, melting and bonding at least two resin parts by making the at least two resin parts abut against each other and vibrating their contact surfaces while applying a pressing force to them,
wherein after initially applying the pressing force, the pressing force is sharply increased to a predetermined value and then is gradually increased.

### Claim 2 (depends on 1)

A method for vibrating, melting and bonding at least two resin parts according to claim 1, wherein the pressing force is continuously gradually increased until vibrating the contact surfaces is finished.

### Claim 3 (depends on 1)

A method for vibrating, melting and bonding at least two resin parts according to claim 1, wherein the pressing force is continuously gradually increased from a predetermined value in a range not exceeding a predetermined upper limit pressing force.

### Claim 4 (depends on 2)

A method for vibrating, melting and bonding at least two resin parts according to claim 2, wherein the pressing force is continuously gradually increased from the predetermined value in a range not exceeding a predetermined upper limit pressing force.

### Claim 5 (depends on 1)

A method for vibrating, melting and bonding at least two resin parts according to claim 1, wherein the pressing force is continuously gradually increased by a combination of a period in which the pressing force is held at a constant value and a period in which the pressing force is increased.

### Claim 6 (depends on 2)

A method for vibrating, melting and bonding at least two resin parts according to claim 2, wherein the pressing force is continuously gradually increased by a combination of a period in which the pressing force is held at a constant value and a period in which the pressing force is increased.

### Claim 7 (depends on 3)

A method for vibrating, melting and bonding at least two resin parts according to claim 3, wherein the pressing force is continuously gradually increased by a combination of a period in which the pressing force is held at a constant value and a period in which the pressing force is increased.

### Claim 8 (depends on 4)

A method for vibrating, melting and bonding at least two resin parts according to claim 4, wherein the pressing force is continuously gradually increased by a combination of a period in which the pressing force is held at a constant value and a period in which the pressing force is increased.

### Claim 9

A method for vibrating, melting and bonding at least two resin parts by making the at least two resin parts abut against each other and vibrating their contact surfaces while applying a pressing force to them,
wherein after the vibrating of the contact surfaces is started, a moving speed when the contact surfaces are vibrated is sharply increased to a predetermined upper limit and then the moving speed is gradually decreased.

### Claim 10

A method for vibrating, melting and bonding at least two resin parts by making the at least two resin parts abut against each other and vibrating their contact surfaces while applying a pressing force to them,
wherein the position of the first resin part of the two resin parts is measured by an amount of melting of the resin parts at the contact surfaces with reference to the second resin part of the two resin parts, a determination is made whether the amount of melting increases with a lapse of time or not, and on a basis of the determination result, a second determination is made whether a state of melting and bonding of the resin parts is good or not.

### Claim 11 (depends on 10)

A method for vibrating, melting and bonding at least two resin parts according to claim 10, wherein the determination result is obtained by determining whether or not the amount of melting is within a range determined by upper and lower limits both of which increase with the lapse of time.

### Claim 12 (depends on 10)

A method for vibrating, melting and bonding at least two resin parts according to claim 10, wherein the determination result is obtained by determining whether a target amount of melting is obtained within a predetermined time or not.

### Claim 13

A method for vibrating, melting and bonding at least two resin parts by making the at least two resin parts abut against each other and vibrating their contact surfaces while applying a pressing force to them,
wherein the contact surface is formed so as to make rigidity of a first resin part of the at least two resin parts nearly uniform at each portion of the contact surface.

### Claim 14

A method for vibrating, melting and bonding at least two resin parts by making the at least two resin parts abut against each other and vibrating their contact surfaces while applying a pressing force to them,
wherein a first resin part of the at least two resin parts has a projection on its outer peripheral surface, the first resin part being pressed into the holding portion of a vibrating jig to fix the vibrating jig, and the vibrating jig is vibrated in this state to vibrate the contact surfaces; and
wherein when the contact surface has a polygonal shape, a thickness of the resin part at a corner portion is made thinner than a thickness of the resin part at a straight portion to make rigidity of the resin part nearly uniform at each portion of the contact surface.

### Claim 15

A method for vibrating, melting and bonding at least two resin parts by making the at least two resin parts abut against each other and vibrating their contact surfaces while applying a pressing force to them,
wherein a first resin part of the at least two resin parts has a projection on its outer peripheral surface, the first resin part being pressed into the holding portion of a vibrating jig to fix the vibrating jig, and the vibrating jig is vibrated in this state to vibrate the contact surfaces; and
wherein in a state where the first resin part is fixed to a vibrating jig and the second resin part is fixed to a stationary jig, the vibrating jig is vibrated to vibrate the contact surfaces, the second resin part has a polygonal rib portion whose top surface is the contact surface, and a thickness of a rib portion at its corner portion is made thinner than a thickness of a rib portion at its corner portion is made thinner than a thickness of the rib portion at a straight portion to make rigidity of the second resin part nearly uniform at each portion of the contact surface.

### Claim 16

A method for vibrating, melting and bonding at least two resin parts by making the at least two resin parts abut against each other and vibrating their contact surfaces while applying a pressing force to them,
wherein the second resin part has a step at a contact surface and a portion, having a higher rigidity of the second resin part at the contact surface, is projected from a portion, having a lower rigidity of the second resin part at the contact surface.