# US 6,730,160 B2 · Method of manufacture of structural insulating building materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,160 B2
- Document ID: US6730160B2
- Status: Granted
- Kind: B2
- Application number: 09/793,459
- Filed: 2001-02-26
- Published: 2002-08-29
- Granted: 2004-05-04
- Earliest claimed: 2001-02-26
- Inventors: Sergio Barbosa
- Web page: https://patentgrep.com/patent/US6730160B2

## CPC

- C04B 35/66: Monolithic refractories or refractory mortars, including those whether or not containing clay {(making or repairing of linings F27D1/16)}
- C04B 28/10: Lime cements or magnesium oxide cements
- C04B 30/02: containing fibrous materials
- C04B 2111/00482: {Coating or impregnation materials}
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A fire retardant building material composed of a mixture of water and cellulose fibers, both of which can be comprised of readily available materials at the job site, such as the available water supply or natural water and scrap shredded paper, including newspaper or other discarded paper or cardboard materials. The water and cellulose fiber is mixed to form a slurry and calcium hydroxide, alumina, salt and ammonia are added. Pigments and aggregates may be added for appearance.

## Claims

### Claim 1

A method of making a construction material comprising:
a. Mixing water and cellulose fibers to form a slurry;
b. Mixing salt into the slurry;
c. Mixing ammonia into the slurry;
d. Mixing calcium hydroxide into the slurry; and
e. Mixing alumina into the slurry,
wherein the ratio of calcium hydroxide to salt is approximately 25 to 1, by weight, and the ratio of calcium hydroxide to ammonia is approximately 25 to 1, by weight.

### Claim 2 (depends on 1)

The method of claim 1, wherein steps b, c, d and e may be performed in any order.

### Claim 3 (depends on 1)

The method of claim 1, including the step of pouring the combination created by steps a, b, c, d and e into a form and drying at ambient temperature.

### Claim 4 (depends on 1)

The method of claim 1, including the step of pouring the combination created by steps a, b, c, d and e into a mold and drying at ambient temperature.

### Claim 5 (depends on 1)

The method of claim 1, including the step of mixing an aggregate into the slurry.

### Claim 6 (depends on 1)

The method of claim 1, including the step of mixing a pigment into the slurry.

### Claim 7 (depends on 1)

The method of claim 1, wherein the ratio of calcium hydroxide to cellulose fiber is approximately 4 to 1, by weight.

### Claim 8 (depends on 1)

The method of claim 1, wherein there is included 6 kilograms of cellulose fibers for every 25 kilograms of calcium.

### Claim 9 (depends on 1)

The method of claim 1, wherein the ratio of calcium hydroxide to alumina is approximately 25 to 1, by weight.

### Claim 10 (depends on 1)

The method of claim 1, wherein there are approximately equal parts of salt, ammonia and alumina, by weight.

### Claim 11 (depends on 1)

The method of claim 1, wherein there are approximately equal parts of salt, ammonia and alumina by volume.

### Claim 12 (depends on 1)

The method of claim 1 wherein the various components comprise approximately the following formula:
6 kilogram of cellulose fibers;
1 liter of ammonia (NH4);
1 liter of alumina;
1 liter of salt (NaCl);
25 kilograms of calcium hydroxide (CaOH); and
180 liters of water.

### Claim 13 (depends on 1)

The method of claim 1, including the step of applying the combination created by steps a, b, c, d and e onto a surface to form a coating.

### Claim 14 (depends on 13)

The method of claim 13, wherein the coating is sprayed onto the surface.

### Claim 15 (depends on 13)

The method of claim 13, wherein the coating is spread by a trowel onto the surface.

### Claim 16 (depends on 13)

The method of claim 13, wherein the coating is rolled onto the surface.

### Claim 17

A method of making a construction material comprising:
a. Mixing water and cellulose fibers to form a slurry;
b. Mixing salt into the slurry;
c. Mixing ammonia into the slurry;
d. Mixing calcium hydroxide into the slurry; and
e. Mixing alumina into the slurry,
wherein the various components comprise approximately the following formula:
6 kilogram of cellulose fibers;
1 liter of ammonia (NH4);
1 liter of alumina;
1 liter of salt (NaCl);
25 kilograms of calcium hydroxide (CaOH); and
180 liters of water.