# US 6,730,159 B1 · Clinker hydraulic binder, use and method for making same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,730,159 B1
- Document ID: US6730159B1
- Status: Granted
- Kind: B1
- Application number: 09/890,144
- Filed: 2001-11-13
- Granted: 2004-05-04
- Earliest claimed: 1999-01-26
- Assignees: Lafarge Aluminates
- Inventors: Jean-Pierre Falaschi; Hervé Fryda; Jean-Pierre Letourneux; Christopher Parr; Bruno Touzo; Michel Vialle
- Web page: https://patentgrep.com/patent/US6730159B1

## CPC

- C04B 35/6303: {Inorganic additives}
- C04B 7/32: Aluminous cements
- C04B 28/06: Aluminous cements (monolithic refractories or refractory mortars C04B35/66)
- C04B 35/66: Monolithic refractories or refractory mortars, including those whether or not containing clay {(making or repairing of linings F27D1/16)}
- C04B 2111/00879: {Non-ferrous metallurgy}
- C04B 2235/3206: Magnesium oxides or oxide-forming salts thereof
- C04B 2235/3217: Aluminum oxide or oxide forming salts thereof, e.g. bauxite, alpha-alumina
- C04B 2235/3222: Aluminates other than alumino-silicates, e.g. spinel (MgAl2O4)
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

A clinker-type hydraulic binder obtained by burning comprising a magnesia spinel mineralogical phase and at least a calcium aluminate mineralogical phase, with a lime content less than 15% of the binder by dry weight. The magnesia spinel represents between 68% and 81% by dry weight of the binder and preferably the calcium aluminates consist essentially of CA and CA2, with C═CaO and A═Al2O3. The invention also concerns the use of such a binder for making a refractory concrete and a method for making such a binder. The invention is useful for making steel ladles (1), preferably for their wear lining.

## Claims

### Claim 1

A hydraulic binder obtained through burning, said binder comprising:
a magnesium spinel mineralogical phase, and
at least a calcium aluminate mineralogical phase with a lime content of less than 15% of the binder by dry weight,
wherein the magnesium spinel comprises between 68% and 81% of the binder by dry weight, and the calcium aluminates are essentially made of CA and CA2, with C═CaO and A═Al2O3, and comprise between 19% and 32% of the binder by dry weight.

### Claim 2 (depends on 1)

The binder according to claim 1, comprising by dry weight of the binder, 71±2% of magnesium spinel, 18±2% Ca and 11±2% CA2.

### Claim 3 (depends on 1)

The binder according to claim 1, which is substantially free from free residual MgO, at least as can be observed upon X-ray diffraction spectrum for the binder.

### Claim 4 (depends on 1)

The binder according to claim 1, having the following chemical composition by dry weight of the binder:
lime CaO 4 to 12% magnesia MgO 19 to 23% alumina Al2O3 69 to 74%.

### Claim 5 (depends on 1)

The binder according to claim 1, having the following chemical composition by dry weight of the binder:
lime CaO 8.4% magnesia MgO 20.4% alumina Al2O3 71.2%.

### Claim 6 (depends on 1)

The binder according to claim 1, further comprising a SiO2 content of less than 0.5% of the binder by dry weight.

### Claim 7 (depends on 1)

The binder according to claim 1, having a Blaine area surface at least equal to 3000 cm2/g.

### Claim 8 (depends on 1)

A method of using a binder according to claim 1 for producing a refractory concrete.

### Claim 9 (depends on 8)

A method of using a binder according to claim 8, wherein said binder includes magnesium spinel in an amount between 20% and 30% of magnesium spinel by dry weight of the concrete.

### Claim 10 (depends on 8)

A method of using a binder according to claim 8, wherein the concrete is produced by mixing by dry weight of the binder:
between 16 and 27% of the binder,
between 2 and 13% of fine reactive alumina,
between 0 and 19% of magnesium spinel, and
between 52 and 71% of alumina granulates.

### Claim 11 (depends on 8)

A method of using a binder according to claim 8, wherein said binder is used in the manufacture of steel ladles for wear linings of such steel ladles.

### Claim 12 (depends on 1)

A process for producing a binder according to claim 1, wherein said binder is made through frittering by burning of a blend of raw materials comprising dolomite, alumina and magnesia.

### Claim 13 (depends on 12)

A process according to claim 12, wherein said dolomite is natural.

### Claim 14 (depends on 12)

A process according to claim 12, wherein said alumina is metallurgical.

### Claim 15 (depends on 12)

A process according to claim 12, wherein said magnesia is reactive and has a grain size less than 100 μm.

### Claim 16 (depends on 12)

A process according to claim 12, wherein the raw materials are, before burning, milled up to a grain size corresponding to a 2% maximum rejection on a sieve of 65 μm.

### Claim 17 (depends on 12)

A process according to claim 12, wherein said burning is carried out at a temperature comprised between 1400° C. and 1600° C.

### Claim 18 (depends on 12)

A process according to claim 12, wherein the degree of progression of said burning is evaluated by measuring the free magnesia content by dry weight of the mixture.